journal article·2020-12Open access

Continuous and pulsed selective laser melting of Ti6Al4V lattice structures: Effect of post-processing on microstructural anisotropy and fatigue behaviour

K. Karami, A. Blok, L. Weber, S.M. Ahmadi, R. Petrov, Ksenija Nikolic, E.V. Borisov, S. Leeflang, C. Ayas, A.A. Zadpoor, M. Mehdipour, E. Reinton, V.A. Popovich

Abstract

Additive manufacturing technologies in general and laser powder bed fusion (L-PBF) in particular have been on the rise in different applications, including biomedical implants. The effects of the various l-PBF process parameters on the microstructure and properties of Ti6Al4V lattice structures have been studied before. However, the relationship between the different modes of laser scanning and the resulting microstructure, internal imperfections, and surface morphology is still underexplored. In this study, the aforementioned parameters and their effect on the compressive mechanical properties and fatigue behaviour of lattice titanium have been studied for both continuous and pulsed laser scanning modes. Moreover, the influence of various combinations of post-processing treatments, such as hot isostatic pressing (HIP), sandblasting, and chemical etching, on the quasi-static mechanical properties and fatigue endurance of the resulting materials were investigated. It was found that continuous laser strategy results in fewer imperfections and higher fatigue resistance, while pulsed laser showed a more homogenous microstructure; likely leading to a more isotropic behaviour. Furthermore, the continuous mode showed larger prior β grains preferentially oriented in the building direction, while pulsed specimens exhibited finer equiaxed grains with no preferred orientations. The highest level of fatigue life was obtained by using an optimized combination of HIP, sandblasting, and chemical etching.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
2. R. Wauthle, Industrialization of selective laser melting for the production of porous titanium and tantalum implants, (2014).
3. ISO / ASTM52900-52915 · 2015
4. J.C. Chekotu, R. Groarke, K. O’Toole, D. Brabazon, Advances in Selective Laser Melting of Nitinol Shape Memory Alloy Part Production, 12(5) (2019) 809.10.3390/ma12050809 ↗
5. E. Hosseini, V.A. Popovich, A review of mechanical properties of additively manufactured Inconel 718, 30 (2019) 100877.10.1016/j.addma.2019.100877 ↗
6. A.R. Nassar, E. Reutzel, Additive manufacturing of Ti-6Al-4V using a pulsed laser beam, 46(6) (2015) 2781-2789.10.1007/s11661-015-2838-z ↗
7. Laser powder bed fusion of titanium-tantalum alloys: compositions and designs for biomedical applications10.1016/j.jmbbm.2020.103775 ↗
8. Effect of solution heat treatment on microstructure and mechanical properties of laser powder bed fusion produced cobalt-28chromium-6molybdenum10.1016/j.msea.2019.138511 ↗
9. J.-P. Kruth, P. Mercelis, J. Van Vaerenbergh, L. Froyen and M. Rombouts, Binding mechanisms in selective laser sintering and selective laser melting, 11(1) (2005) 26-36.10.1108/13552540510573365 ↗
10. L. Thijs, F. Verhaeghe, T. Craeghs, J. Van Humbeeck and J.-P. Kruth, A study of the microstructural evolution during selective laser melting of Ti–6Al–4V, 58(9) (2010) 3303-3312.10.1016/j.actamat.2010.02.004 ↗
11. R. Stamp, P. Fox, W. O’neill, E. Jones and C. Sutcliffe, The development of a scanning strategy for the manufacture of porous biomaterials by selective laser melting, 20(9) (2009) 1839.10.1007/s10856-009-3763-8 ↗
12. C. Zhang, H. Zhu, Z. Hu, L. Zhang, X. J. M. S. Zeng, A comparative study on single-laser and multi-laser selective laser melting AlSi10Mg: defects, microstructure and mechanical properties, 746 (2019) 416-423.10.1016/j.msea.2019.01.024 ↗
13. H. Shipley, D. McDonnell, M. Culleton, R. Coull, R. Lupoi, G. O’Donnell, D. Trimble, Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: A review, 128 (2018) 1-20.10.1016/j.ijmachtools.2018.01.003 ↗
14. Ding · 2016 · 10898
15. S. Ahmadi, R. Hedayati, R. A. K. Jain, Y. Li, S. Leeflang, A.A. Zadpoor, Effects of laser processing parameters on the mechanical properties, topology, and microstructure of additively manufactured porous metallic biomaterials: A vector-based approach, 134 (2017) 234-243.10.1016/j.matdes.2017.08.046 ↗
16. E. Brandl, F. Palm, V. Michailov, B. Viehweger, C. Leyens, Mechanical properties of additive manufactured titanium (Ti–6Al–4V) blocks deposited by a solid-state laser and wire, 32(10) (2011) 4665-4675.10.1016/j.matdes.2011.06.062 ↗
17. S. Kuriakose and M. Shunmugam, Characteristics of wire-electro discharge machined Ti6Al4V surface, 58(17-18) (2004) 2231-2237.10.1016/j.matlet.2004.01.037 ↗
18. Antonysamy · 2012
19. Bundy · 2008 · 56
20. C. Elias, J. Lima, R. Valiev and M. Meyers, Biomedical applications of titanium and its alloys, 60(3) (2008) 46-49.10.1007/s11837-008-0031-1 ↗
21. Pederson · 2002
22. L. Yuan, S. Ding and C. Wen, Additive manufacturing technology for porous metal implant applications and triple minimal surface structures: A review. 4(1) (2019) 56-70.10.1016/j.bioactmat.2018.12.003 ↗
23. B. Levine, A new era in porous metals: applications in orthopaedics. 10(9) (2008) 788-792.10.1002/adem.200800215 ↗
24. X. Li, C. Wang, W. Zhang and Y. Li, Fabrication and compressive properties of Ti6Al4V implant with honeycomb-like structure for biomedical applications. 16(1) (2010) 44-49.10.1108/13552541011011703 ↗
25. Meta-biomaterials10.1039/C9BM01247H ↗
26. J. H. Lee, J. P. Singer and E. Thomas, Micro‐/nanostructured mechanical metamaterials, 24(36) (2012) 4782-4810.10.1002/adma.201201644 ↗
27. S. Ahmadi, R. Hedayati, Y. Li, K. Lietaert, N. Tümer, A. Fatemi, C.D. Rans, B. Pouran, H. Weinans, A.A. Zadpoor, Fatigue performance of additively manufactured meta-biomaterials: The effects of topology and material type, 65 (2018) 292-304.10.1016/j.actbio.2017.11.014 ↗
28. B. Van Hooreweder, Y. Apers, K. Lietaert and J.-P. Kruth, Improving the fatigue performance of porous metallic biomaterials produced by Selective Laser Melting, 47 (2017) 93-202.10.1016/j.actbio.2016.10.005 ↗
29. S. A. Yavari, S. Ahmadi, R. Wauthle, B. Pouran, J. Schrooten, H. Weinans, A.A. Zadpoor, Relationship between unit cell type and porosity and the fatigue behavior of selective laser melted meta-biomaterials, 43 (2015) 91-100.10.1016/j.jmbbm.2014.12.015 ↗
30. S. A. Yavari, R. Wauthlé, J. van der Stok, A. Riemslag, M. Janssen, M. Mulier, A.A. Zadpoor, Fatigue behavior of porous biomaterials manufactured using selective laser melting, 33(8) (2013) 4849-4858.10.1016/j.msec.2013.08.006 ↗
31. S. M. Ahmadi, R. Kumar, E.V. Borisov, R. Petrov, S. Leeflang, Y. Li, N. Tümer, R. Huizenga, C. Ayas, A.A. Zadpoor, V.A. Popovich, From microstructural design to surface engineering: A tailored approach for improving fatigue life of additively manufactured meta-biomaterials, 83 (2019) 153-166.10.1016/j.actbio.2018.10.043 ↗
32. N. Loh and K. Sia, An overview of hot isostatic pressing, 30(1) (1992) 45-65.10.1016/0924-0136(92)90038-T ↗
33. Effects of heat treatment on microstructure and mechanical behaviour of additive manufactured porous Ti6Al4V10.1088/1757-899X/293/1/012009 ↗
34. R. Hedayati, S. Ahmadi, K. Lietaert, B. Pouran, Y. Li, H. Weinans, A.A. Zadpoor, Isolated and modulated effects of topology and material type on the mechanical properties of additively manufactured porous biomaterials. 79 (2018) 254-263.10.1016/j.jmbbm.2017.12.029 ↗
35. Leyens · 2003
36. M. Niinomi, Mechanical properties of biomedical titanium alloys, 243 (1-2) (1998) 231-236.10.1016/S0921-5093(97)00806-X ↗
37. S. Li, H. Xiao, K. Liu, W. Xiao, Y. Li, X. Han, J. Mazumder, L. Song, Melt-pool motion, temperature variation and dendritic morphology of Inconel 718 during pulsed-and continuous-wave laser additive manufacturing: A comparative study, 119 (2017) 351-360.10.1016/j.matdes.2017.01.065 ↗
38. G. Ravi, C. Qiu and M. Attallah, Microstructural control in a Ti-based alloy by changing laser processing mode and power during direct laser deposition, 179 (2016) 104-108.10.1016/j.matlet.2016.05.038 ↗
39. S. Ghouse, S. Babu, R. J. Van Arkel, K. Nai, P. A. Hooper, J. Jeffers, et al., The influence of laser parameters and scanning strategies on the mechanical properties of a stochastic porous material, 131 (2017) 498-508.10.1016/j.matdes.2017.06.041 ↗
40. C. Biffi, J. Fiocchi, P. Bassani and A. Tuissi, Continuous wave vs pulsed wave laser emission in selective laser melting of AlSi10Mg parts with industrial optimized process parameters: microstructure and mechanical behaviour, 24 (2018) 639-646.10.1016/j.addma.2018.10.021 ↗
41. Caprio · 2017 · 1304
42. J. Kim, S. Ji, Y.-S. Yun, J. Yeo, A Review: Melt Pool Analysis for Selective Laser Melting with Continuous Wave and Pulse Width Modulated Lasers, 27(6) (2018) 113-119.10.5757/ASCT.2018.27.6.113 ↗
43. A. G. Demir, P. Colombo and B. Previtali, From pulsed to continuous wave emission in SLM with contemporary fiber laser sources: effect of temporal and spatial pulse overlap in part quality, 91(5-8) (2017) 2701-2714.10.1007/s00170-016-9948-7 ↗
44. C. Qiu, C. Panwisawas, M. Ward, H. C. Basoalto, J. W. Brooks and M. Attallah, On the role of melt flow into the surface structure and porosity development during selective laser melting, 96 (2015) 72-79.10.1016/j.actamat.2015.06.004 ↗
45. S. Ahmadi, G. Campoli, S. A. Yavari, B. Sajadi, R. Wauthlé, J. Schrooten, A.A. Zadpoor, Mechanical behavior of regular open-cell porous biomaterials made of diamond lattice unit cells, 34 (2014) 106-115.10.1016/j.jmbbm.2014.02.003 ↗
46. C. Cayron, ARPGE: a computer program to automatically reconstruct the parent grains from electron backscatter diffraction data, 40(6) (2007) 1183-1188.10.1107/S0021889807048777 ↗
47. ISO 13314 · 2011 · 1
48. Deviant · 2011
49. Gibson · 1999
50. A. Zargarian, M. Esfahanian, J. Kadkhodapour, S. Ziaei-Rad,, Numerical simulation of the fatigue behavior of additive manufactured titanium porous lattice structures, 60 (2016), 339-347.10.1016/j.msec.2015.11.054 ↗
51. P. Collins, D. Brice, P. Samimi, I. Ghamarian and H. Fraser, Microstructural control of additively manufactured metallic materials, 46 (2016) 63-91.10.1146/annurev-matsci-070115-031816 ↗
52. A. Basak and S. Das, Epitaxy and microstructure evolution in metal additive manufacturing. 46 (2016) 125-149.10.1146/annurev-matsci-070115-031728 ↗
53. E. Onal, A. Medvedev, M. Leeflang, A. Molotnikov and A.A. Zadpoor, Novel microstructural features of selective laser melted lattice struts fabricated with single point exposure scanning. 29 (2019) 100785.10.1016/j.addma.2019.100785 ↗
54. X. Ding, L. Wang and S. Wang, Comparison study of numerical analysis for heat transfer and fluid flow under two different laser scan pattern during selective laser melting, 127(22) (2016) 10898-10907.10.1016/j.ijleo.2016.08.123 ↗
55. S. Malinov, Z. Guo, W. Sha, A. Wilson, Differential scanning calorimetry study and computer modeling of β⇒ α phase transformation in a Ti-6Al-4V alloy, 32(4) (2001) 879-887.10.1007/s11661-001-0345-x ↗
56. G. Kasperovich and J. Hausmann, Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting, 220 (2015) 202-214.10.1016/j.jmatprotec.2015.01.025 ↗
57. R. Wauthle, B. Vrancken, B. Beynaerts, K. Jorissen, J. Schrooten, J.-P. Kruth, Effects of build orientation and heat treatment on the microstructure and mechanical properties of selective laser melted Ti6Al4V lattice structures, 5 (2015) 77-84.10.1016/j.addma.2014.12.008 ↗
58. B. Baufeld, E. Brandl and O. Van der Biest, Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti–6Al–4V components fabricated by laser-beam deposition and shaped metal deposition, 211(6) (2011) 1146-1158.10.1016/j.jmatprotec.2011.01.018 ↗
59. R. Nalla, J. Campbell, R. J. F. Ritchie, Effects of microstructure on mixed‐mode, high‐cycle fatigue crack‐growth thresholds in Ti‐6Al‐4V alloy, 25(6) (2002) 587-606.10.1046/j.1460-2695.2002.00522.x ↗
60. Y. Zhai, D. A. Lados, E. J. Brown and G. Vigilante, Fatigue crack growth behavior and microstructural mechanisms in Ti-6Al-4V manufactured by laser engineered net shaping, 93 (2016) 51-63.10.1016/j.ijfatigue.2016.08.009 ↗
61. T. Vilaro, C. Colin, J. Bartout, As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting, 42(10) (2011) 3190-3199.10.1007/s11661-011-0731-y ↗
62. C. Chen, Y. Xie, X. Yan, S. Yin, H. Fukanuma, R. Huang, Effect of hot isostatic pressing (HIP) on microstructure and mechanical properties of Ti6Al4V alloy fabricated by cold spray additive manufacturing, 27 (2019) 595-605.10.1016/j.addma.2019.03.028 ↗
63. B. Vrancken, L. Thijs, J.-P. Kruth, J. Van Humbeeck, Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties. 541 (2012) 177-185.10.1016/j.jallcom.2012.07.022 ↗
64. S. L. Sing, F. E. Wiria, W. Yeong, Selective laser melting of lattice structures: A statistical approach to manufacturability and mechanical behavior, 49 (2018) 170-180.10.1016/j.rcim.2017.06.006 ↗
65. N. T. Aboulkhair, N. M. Everitt, I. Ashcroft and C. Tuck, Reducing porosity in AlSi10Mg parts processed by selective laser melting, 1 (2014) 77-86.10.1016/j.addma.2014.08.001 ↗
66. Z. Dong, Y. Liu, W. Li and J. Liang, Orientation dependency for microstructure, geometric accuracy and mechanical properties of selective laser melting AlSi10Mg lattices, 791 (2019) 490-500.10.1016/j.jallcom.2019.03.344 ↗
67. M. Smith, Z. Guan and W. Cantwell, Finite element modelling of the compressive response of lattice structures manufactured using the selective laser melting technique, 67 (2013) 28-41.10.1016/j.ijmecsci.2012.12.004 ↗
68. Gibson · 1997
69. Influence of re-melting on surface roughness and porosity of AlSi10Mg parts fabricated by selective laser melting10.1016/j.jallcom.2019.04.017 ↗
70. Microstructural evolution and EBSD analysis of AlSi10Mg alloy fabricated by selective laser remelting10.1016/j.matchar.2019.110079 ↗
71. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V10.1016/j.matdes.2011.09.051 ↗
72. Additive manufacturing of Al-12Si alloy via pulsed selective laser melting10.1007/s11837-014-1272-9 ↗