journal article·2021-01

Additive manufacturing of a martensitic Co–Cr–Mo alloy: Towards circumventing the strength–ductility trade-off

Z. Wang, S.Y. Tang, S. Scudino, Yu.P. Ivanov, R.T. Qu, D. Wang, C. Yang, W.W. Zhang, A.L. Greer, J. Eckert, K.G. Prashanth

Publisher page

Abstract

Abstract A Co–Cr–Mo alloy with predominantly martensitic structure was prepared by selective laser melting (SLM), where the amount of martensite formed in the SLM specimens is much larger than in the cast samples which can be ascribed to the high density of internal defects such as dislocations and SFs. We observe a hierarchical microstructure spanning over different length scales, consisting of remelted zones and track core regions at the macro-scale, regions with elongated columnar grains and equiaxed grains at the micro-scale, martensitic laths at the submicron-scale, and a high density of dislocations and stacking faults at the nano- and atomic scale. The hierarchical microstructure leads to the outstanding tensile properties of the as-prepared SLM and SLM annealed samples (with yield strength, ultimate tensile strength and fracture strain of ~ 735 MPa, ~ 1211 MPa and ~ 12.8%, and ~ 893 MPa, ~ 1214 MPa and ~ 13.8%, respectively). The mechanisms determining the strength and ductility are discussed in terms of the hierarchical microstructure and internal defects. The cellular structure with a high density of dislocations along their boundaries and the martensitic structure are the reasons for strengthening, while the hierarchical microstructure helps to obtain appropriate ductility. Furthermore, martensitic transformation induced plastic bending of the residual FCC plates was confirmed, which is helpful to maintain the different plastic strain between the heterogeneous structure. The development of the martensitic structure in this Co–Cr–Mo alloy by SLM and its characteristic hierarchical microstructure are promising features for material design and application of high-strength materials with improved strength‒ductility tradeoff.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. https://doi.org/10.1520/stp1365-ebJ.A. Disegi, R.L. Kennedy, R. Pilliar, Cobalt-Base Alloys for Biomedical Applications, 1999. 〈〉.
2. Fatigue improvement of electron beam melting-fabricated biomedical Co–Cr–Mo alloy by accessible heat treatment10.1080/21663831.2017.1396506 ↗
3. Selective laser melting technique of Co-Cr dental alloys: a review of structure and properties and comparative analysis with other available techniques10.1111/jopr.12268 ↗
4. Developing high strength and ductility in biomedical Co-Cr cast alloys by simultaneous doping with nitrogen and carbon10.1016/j.actbio.2015.12.011 ↗
5. Osseointegration enhancement by Zr doping of Co-Cr-Mo implants fabricated by electron beam melting
6. Porter · 2009
7. Strain-induced martensitic transformation near twin boundaries in a biomedical Co-Cr-Mo alloy with negative stacking fault energy10.1016/j.actamat.2012.11.041 ↗
8. Microstructures and mechanical properties of Co-29Cr-6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗
9. Effect of cold rolling on phase decomposition in biomedical Co-29Cr-6Mo-0.2N alloy during isothermal heat treatment at 1073 K10.1016/j.jallcom.2014.05.175 ↗
10. Microscopic mechanism of plastic deformation in a polycrystalline Co-Cr-Mo alloy with a single hcp phase10.1016/j.actamat.2013.11.005 ↗
11. Development of athermal and isothermal ε-martensite in atomized Co-Cr-Mo-C implant alloy powders10.1007/BF02586154 ↗
12. Effect of solution treatments on the FCC/HCP isothermal martensitic transformation in Co-27Cr-5Mo-0.05C aged at 800 °C10.1016/S1359-6462(98)00489-8 ↗
13. Tribological behaviour of cast and wrought Co-Cr-Mo implant alloys10.1179/026708399101505284 ↗
14. Martensitic transformation in a cast Co-Cr-Mo-C alloy10.1007/s11661-007-9370-8 ↗
15. Nanoarchitectured Co-Cr-Mo orthopedic implant alloys: nitrogen-enhanced nanostructural evolution and its effect on phase stability10.1016/j.actbio.2012.12.013 ↗
16. Heterogeneous microstructures and corrosion resistance of biomedical Co-Cr-Mo alloy fabricated by electron beam melting (EBM)
17. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
18. Microstructure and mechanical properties of Al-12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
19. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
20. Anisotropy in local microstructure – does it affect the tensile properties of the SLM samples?10.1016/j.mfglet.2018.02.012 ↗
21. Development of strong and ductile metastable face-centered cubic single-phase high-entropy alloys10.1016/j.actamat.2019.09.050 ↗
22. On microstructural homogenization and mechanical properties optimization of biomedical Co-Cr-Mo alloy additively manufactured by using electron beam melting
23. Molten pool behavior and effect of fluid flow on solidification conditions in selective electron beam melting (SEBM) of a biomedical Co-Cr-Mo alloy
24. Carbide precipitation characteristics in additive manufacturing of Co-Cr-Mo alloy via selective election beam melting10.1016/j.scriptamat.2017.09.022 ↗
25. Mechanical behavior of porous commercially pure Ti and Ti-TiB composite materials manufactured by selective laser melting10.1016/j.msea.2014.12.036 ↗
26. Comparison of wear properties of commercially pure titanium prepared by selective laser melting and casting processes10.1016/j.matlet.2014.11.156 ↗
27. Novel Co-rich high entropy alloys with superior tensile properties10.1080/21663831.2018.1553803 ↗
28. Is the energy density a reliable parameter for materials synthesis by selective laser melting?10.1080/21663831.2017.1299808 ↗
29. Production of high strength Al85Nd8Ni5Co2 alloy by selective laser melting
30. Selective laser melting of Ti-45Nb alloy10.3390/met5020686 ↗
31. Cellular lattices of biomedical Co-Cr-Mo-alloy fabricated by electron beam melting with the aid of shape optimization
32. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
33. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
34. Formation of metastable cellular microstructures in selective laser melted alloys10.1016/j.jallcom.2016.12.209 ↗
35. Méthode d"analyse quantitative des variétés allotropiques du cobalt par les rayons X10.1051/metal/195047020139 ↗
36. Athermal ε-martensite transformation in a Co-20Cr alloy: effect of rapid solidification on plate nucleation10.1016/j.actamat.2016.03.047 ↗
37. Mechanism-based strain gradient plasticity – I. Theory10.1016/S0022-5096(98)00103-3 ↗
38. About quantitative EBSD analysis of deformation and recovery substructures in pure Tantalum10.1088/1757-899X/89/1/012038 ↗
39. In vitro biocompatibility of CoCrMo dental alloys fabricated by selective laser melting10.1016/j.dental.2014.02.008 ↗
40. Hybrid nanostructured aluminum alloy with super-high strength10.1038/am.2015.129 ↗
41. Shaping of metallic glasses by stress-annealing without thermal embrittlement10.1016/j.actamat.2011.02.039 ↗
42. Simultaneously enhanced strength and ductility for 3D-printed stainless steel 316L by selective laser melting10.1038/s41427-018-0018-5 ↗
43. Microstructure and phase formation in Al-20Si-5Fe-3Cu-1Mg synthesized by selective laser melting10.1016/j.jallcom.2015.10.119 ↗
44. Fabrication of Fe-based bulk metallic glass by selective laser melting: a parameter study10.1016/j.matdes.2015.07.145 ↗
45. Effect of heat-treatment temperature on microstructures and mechanical properties of Co–Cr–Mo alloys fabricated by selective laser melting10.1016/j.msea.2018.04.048 ↗
46. Effect of the heat treatment on corrosion and mechanical properties of CoCrMo alloys manufactured by selective laser melting10.1108/RPJ-10-2017-0215 ↗
47. Build direction dependence of microstructure and high-temperature tensile property of Co-Cr-Mo alloy fabricated by electron beam melting10.1016/j.actamat.2013.10.017 ↗
48. Ductility and structure of some cobalt-base dental casting alloys10.1016/0142-9612(84)90016-4 ↗
49. Static mechanical properties of cast and sinter-annealed cobalt-chromium surgical implants10.1007/BF00553274 ↗
50. The effect of HIPing on the fatigue and tensile strength of a cast, porous-coated Co-Cr-Mo alloy10.1002/jbm.820200812 ↗
51. Effect of heat treatment on the properties of CoCrMo alloy manufactured by selective laser melting10.1007/s11665-018-3351-5 ↗
52. Effect of alloy preheating on the mechanical properties of as-cast Co-Cr-Mo-C alloys10.1007/s11661-999-0052-6 ↗
53. Effects of chromium and nitrogen content on the microstructures and mechanical properties of as-cast Co-Cr-Mo alloys for dental applications10.1016/j.actbio.2012.03.024 ↗
54. Effect of cobalt-aluminate addition on microstructure and mechanical property of Co-Cr-Mo alloy10.1179/1432891715Z.0000000001370 ↗
55. Effect of carbon addition on microstructure and mechanical properties of a wrought Co-Cr-Mo implant alloy10.2320/matertrans.47.287 ↗
56. Mechanical and phase transformation behaviour of biomedical Co-Cr-Mo alloy fabricated by direct metal laser sintering10.1016/j.msea.2017.12.087 ↗
57. A model for the microstructure behaviour and strength evolution in lath martensite10.1016/j.actamat.2015.07.018 ↗
58. Exploring the relationship between the microstructure and strength of fresh and tempered martensite in a maraging stainless steel Fe–15Cr–5Ni10.1016/j.msea.2018.12.126 ↗
59. Premature failure of an additively manufactured material10.1038/s41427-020-0212-0 ↗
60. Size effects and Hall–Petch relation in polycrystalline cobalt10.1080/09500839.2015.1020351 ↗
61. Chapter 7 – Strengthening mechanisms and super-strength of severely deformed titanium
62. A deformation map for cobalt10.1016/0036-9748(83)90390-3 ↗
63. https://doi.org/10.1007/s11665-018-3840-6Z. Zhang, Z.F. Hu, P.M. Singh, X. Li, S. Xiong, X.X. Fang, Microstructure Evolution and Stress Corrosion Cracking Susceptibility of 12Cr Martensitic Steel Upon Long-Term Service in Power Plants, 28, 2019, pp. 995–1006. 〈〉.10.1007/s11665-018-3840-6 ↗
64. Deformation induced FCC to HCP transformation in a Co-27Cr-5Mo-0.05C alloy10.1016/j.msea.2010.12.024 ↗
65. Precipitation hardening in metals10.1179/026708399773002782 ↗
66. A low-alloy high-carbon martensite steel with 2.6 GPa tensile strength and good ductility10.1016/j.actamat.2018.07.060 ↗
67. Theory of the tensile test10.1016/0001-6160(67)90211-8 ↗