Abstract
Abstract Porosity in additively manufactured metals can reduce material strength and is generally undesirable. Although studies have shown relationships between process parameters and porosity, monitoring strategies for defect detection and pore formation are still needed. In this paper, instantaneous anomalous conditions are detected in-situ via pyrometry during laser powder bed fusion additive manufacturing and correlated with voids observed using post-build micro-computed tomography. Large two-color pyrometry data sets were used to estimate instantaneous temperatures, melt pool orientations and aspect ratios. Machine learning algorithms were then applied to processed pyrometry data to detect outlier images and conditions. It is shown that melt pool outliers are good predictors of voids observed post-build. With this approach, real time process monitoring can be incorporated into systems to detect defect and void formation. Alternatively, using the methodology presented here, pyrometry data can be post processed for porosity assessment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Characterization of the effects of internal pores on tensile properties of additively manufactured austenitic stainless steel 316l
2. Influence of energy density on porosity and microstrucutre of selective laser melted 17-4PH stainless steel
3. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
4. Prediction of lack-of-fusion porosity for powder bed fusion
5. Review of in-situ process monitoring and in-situ metrology for metal additive manufacturing10.1016/j.matdes.2016.01.099 ↗
6. In-process sensing in selective laser melting (slm) additive manufacturing10.1186/s40192-016-0045-4 ↗
7. Melt pool temperature and cooling rates in laser powder bed fusion
8. Advancing quantitative description of porosity in autogenous laser-welds of 304L stainless steel
9. Formation and influence mechanism of keyhole-induced porosity in deep-penetration laser welding based on 3D transient modeling10.1016/j.ijheatmasstransfer.2015.07.041 ↗
10. 3D transient multiphase model for keyhole, vapor plume, and weld pool dynamics in laser welding including the ambient pressure effect10.1016/j.optlaseng.2015.05.003 ↗
11. The effect of reduced pressure on laser keyhole weld porosity and weld geometry in commercially pure titanium and nickel
12. Extreme-value statistics reveal rare failure-critical defects in additive manufacturing10.1002/adem.201700102 ↗
13. High-throughput stochastic tensile performance of additively manufactured stainless steel10.1016/j.jmatprotec.2016.10.023 ↗
14. Effect of hot isostatic pressing and powder feedstock on porosity, microstructure, and mechanical properties of selective laser melted AlSi10Mg
15. Computed tomography characterisation of additive manufacturing materials10.1016/j.medengphy.2010.12.015 ↗
16. Corroborating tomographic defect metrics with mechanical response in an additively manufactured precipitation-hardened stainless steel
17. Structural imperfections in additive manufacturing perceived from the X-ray micro-tomography perspective10.1016/j.jmatprotec.2016.03.019 ↗
18. X-ray computed tomography for additive manufacturing: a review10.1088/0957-0233/27/7/072001 ↗
19. X-ray microcomputed tomography in additive manufacturing: a review of the current technology and applications10.1089/3dp.2018.0060 ↗
20. X-ray computed tomography for additive manufacturing: a review
21. Segmentation of four-dimensional, X-ray computed tomography data
22. 3-D growth of a short fatigue crack within a polycrystalline microstructure studied using combined diffraction and phase-contrast X-ray tomography10.1016/j.actamat.2010.09.063 ↗
23. High resolution X-ray tomography of micromechanisms of fatigue crack closure10.1016/j.scriptamat.2006.01.016 ↗
24. In situ and real-time 3-D microtomography investigation of dendritic solidification in an Al-10 wt.% Cu alloy10.1016/j.actamat.2009.01.035 ↗
25. X-ray computed tomography vs. metallography for pore sizing and fatigue of cast Al-alloys10.1016/j.proeng.2010.03.059 ↗
26. Fast in situ X-ray microtomography observations of solidification and semisolid deformation of Al-Cu alloys10.1007/s11837-011-0219-7 ↗
27. Standardized X-ray tomography testing of additively manufactured parts: a round robin test
28. Process-defect-structure-property correlations during laser powder bed fusion of alloy 718: role of in situ and ex situ characterizations10.1007/s11661-018-4870-2 ↗
29. Thermography for monitoring the selective laser melting process
30. In situ quality control of the selective laser melting process using a high-speed, real-time melt pool monitoring system10.1007/s00170-014-6214-8 ↗
31. Stainless steel 304l lens am process monitoring using in-situ pyrometer data10.1007/s11837-018-3033-7 ↗
32. Porosity prediction: Supervised-learning of thermal history for direct laser deposition10.1016/j.jmsy.2018.04.001 ↗
33. Vollmer · 2017
34. Dagel · 2016 · 986103
35. Wikipedia contributors · 2018
36. Emissivity and temperature determination on steel above the melting point10.1007/s40194-013-0054-2 ↗
37. Direct least squares fitting of ellipses10.1109/ICPR.1996.546029 ↗
38. Application of joint histogram and mutual information to registration and data fusion problems in serial sectioning microstructure studies10.1016/j.scriptamat.2008.11.004 ↗
39. Certain topics in telegraph transmission theory
40. Communication in the presence of noise
41. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗