Evolution of crystallographic orientation, columnar to equiaxed transformation and mechanical properties realized by adding TiCps in wire and arc additive manufacturing 2219 aluminum alloy
Source abstract
Abstract
Abstract 2219Al/TiCps composites were deposited by the wire and arc additive manufacturing method. The effects of TiCps content on the phase transformation, average grain size, crystal orientation, and mechanical properties of the deposited 2219 aluminium alloys were investigated as the variation of TiCps fraction is from 0.5 wt% to 2.0 wt%. The results show that the addition of 5 µm TiCps can effectively reduce the nucleation free energy of the system, which provided an opportunity for nuclei to grow on the surface of TiCps. The average grain size first decreased, then increased with the increase of TiCps weight fraction. Also, the EBSD testing results show the texture intensity both the Al-matrix and the θ-CuAl2 phase gradually decreased with increasing TiCps fraction. TiCps played an important role in generating nucleation undercooling (ΔTnu, 0.38 °C), which could be used to counteract the constitutional supercooling (ΔTcs) caused by solute segregation, and further promoted the transformation of granular θ-CuAl2 phase to a fine spot-like one within the grains. The fine spot-like phase possessed a strong interfacial bonding with the Al-matrix, thereby the mechanical properties of the deposited 2219 aluminium alloy were strengthened. Eventually, the deposited alloy exhibited a tensile strength around 405 MPa, and the elongation was up to 15.6%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Heat treatments for improved quality binder jetted molds for casting aluminum alloys
2. Comparative study on the microstructures and properties of wire+arc additively manufactured 5356 aluminium alloy with argon and nitrogen as the shielding gas
3. Composition and automated crystal orientation mapping of rapid solidification products in hypoeutectic Al-4 at% Cu alloys10.1016/j.actamat.2017.11.040 ↗
4. Recent development in aluminium alloys for aerospace applications10.1016/S0921-5093(99)00674-7 ↗
5. Three-dimensional analysis of grain structure and texture of additively manufactured 316L austenitic stainless steel
6. Deformations of Ti-6Al-4V additive-manufacturing-induced isotropic and anisotropic columnar structures: Insitu measurements and underlying mechanisms
7. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
8. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
9. Mechanical properties of 2219-Al components produced by additive manufacturing with TIG10.1007/s00170-015-8168-x ↗
10. A comparative study of additively manufactured thin wall and block structure with Al-6.3% Cu alloy using cold metal transfer process [J]10.3390/app7030275 ↗
11. Influence of travel speed on microstructure and mechanical properties of wire + arc additively manufactured 2219 aluminum alloy10.1016/j.jmst.2019.06.016 ↗
12. Microstructure and mechanical properties of 2219 aluminum alloy fabricated by double-electrode gas metal arc additive manufacturing
13. Microstructure evolution of wire-arc additively manufactured 2319 aluminum alloy with interlayer hammering
14. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy10.1016/j.msea.2015.10.101 ↗
15. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
16. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
17. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
18. Processing and properties of magnesium containing a dense uniform dispersion of nanoparticles10.1038/nature16445 ↗
19. Laser solid forming additive manufacturing TiB2 reinforced 2024Al composite: Microstructure and mechanical properties10.1016/j.msea.2018.12.072 ↗
20. Real-time observation of grain nucleation and growth during solidification of aluminium alloys10.1016/j.actamat.2005.02.045 ↗
21. Wetting of liquid copper on TC4 titanium alloy and 304 stainless steel at 1273–1433 K10.1016/j.matdes.2019.107667 ↗
22. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
23. Grain refinement of aluminium alloys by inoculation
24. Gale · 1998
25. Wetting of TiC by molten Al at 1123–1323 K10.1016/j.actamat.2010.11.055 ↗
26. Behavior of ceramic particles at the solid- liquid metal interface in metal matrix composites10.1007/BF02645819 ↗
27. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface10.1007/BF02801184 ↗
28. An analytical solution of the critical interface velocity for the encapturing of insoluble particles by a moving solid/liquid interface10.1007/s11661-998-0186-y ↗
29. Solid–liquid interface dynamics during solidification of Al 7075-Al2O3np based metal matrix composites10.1016/j.matdes.2016.01.042 ↗
30. Effect of clustering on particle pushing and solidification behaviour in TiB2 reinforced aluminium PMMCs10.1016/j.compositesa.2004.10.027 ↗
31. Thermal conductivity of TiC10.1111/j.1151-2916.1963.tb19782.x ↗
32. Formation conditions of presolar TiC core-graphite mantle spherules in the murchison meteorite10.1086/306628 ↗
33. The interdependence theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
34. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
35. On the strength of discontinuous silicon carbide rein-forced aluminum composites10.1016/0036-9748(86)90210-3 ↗