journal article·2021-10Open access

Surface roughness parameter and modeling for fatigue behavior of additive manufactured parts: A non-destructive data-driven approach

Seungjong Lee, Behnam Rasoolian, Daniel F. Silva, Jonathan W. Pegues, Nima Shamsaei

Abstract

Abstract Metallic additive manufacturing produces undesired surface roughness due to the nature of the layer-by-layer fabrication process. As-built surface roughness can accelerate surface crack initiation and result in an early fatigue failure under cyclic loading. Therefore, the effect of surface roughness on the structural integrity of additive manufactured parts needs to be characterized before they can be used in fatigue-critical applications. In this study, the surface roughness of Ti-6Al-4V specimens fabricated by a laser beam powder bed fusion system is characterized, using a non-destructive data-driven approach, and correlated with their fatigue performance. Using a data-intensive surface topographical investigation, standard surface roughness parameters with statistical robustness are generated. The results confirm that conventional standard surface roughness parameters cannot appropriately represent the correlation between surface roughness and fatigue lives. Accordingly, a hybrid surface roughness parameter consisting of the maximum valley depth (Rv/Sv), the skewness (Rsk/Ssk), and the kurtosis (Rku/Sku) of the profiled lines/areas is suggested to explain the fatigue behavior. The proposed hybrid surface roughness parameter is validated by vertically fabricated flat specimens and diagonally built cylindrical dog-bone specimens to investigate the effect of design and build orientation. Moreover, a fatigue prediction model which considers the surface roughness as a micro-notch has been modified using the proposed hybrid surface roughness parameter and the part’s layer thickness and validated against experimental data.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
3. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
4. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
5. Laser and electron-beam powder-bed additive manufacturing of metallic implants: a review on processes, materials and designs10.1002/jor.23075 ↗
6. An overview of direct laser deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control
7. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
8. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
9. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
10. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
11. Biomedical applications of titanium and its alloys10.1007/s11837-008-0031-1 ↗
12. G. Lutjering, J.C. Williams, Titanium, second ed., 2007. https://doi.org/10.1007/978-3-540-73036-1.10.1007/978-3-540-73036-1 ↗
13. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
14. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
15. A review of powdered additive manufacturing techniques for Ti-6Al-4V biomedical applications
16. Additive manufacturing of titanium alloys by electron beam melting: a review
17. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
18. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock10.1007/s11837-015-1759-z ↗
19. Fatigue behaviour of additive manufactured materials: an overview of some recent experimental studies on Ti-6Al-4V considering various processing and loading direction effects10.1111/ffe.13000 ↗
20. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
21. Defects-dictated tensile properties of selective laser melted Ti-6Al-4V10.1016/j.matdes.2018.08.004 ↗
22. Fatigue of additive manufactured Ti-6Al-4V, Part II: the relationship between microstructure, material cyclic properties, and component performance10.1016/j.ijfatigue.2019.105363 ↗
23. Fatigue of additive manufactured Ti-6Al-4V, Part I: the effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects10.1016/j.ijfatigue.2019.105358 ↗
24. Stephens · 2000
25. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
26. Significance of hot isostatic pressing (HIP) on multiaxial deformation and fatigue behaviors of additive manufactured Ti-6Al-4V including build orientation and surface roughness effects10.1016/j.ijfatigue.2018.07.035 ↗
27. Fatigue behavior of additively manufactured 17-4 pHstainless steel: Synergistic effects of surface roughness and heat treatment10.1016/j.ijfatigue.2019.02.039 ↗
28. Surface texture metrology for metal additive manufacturing: a review10.1016/j.precisioneng.2016.06.001 ↗
29. Effects of defects in laser additive manufactured Ti-6Al-4V on fatigue properties10.1016/j.phpro.2014.08.120 ↗
30. Effect of surface roughness on fatigue performance of additive manufactured Ti–6Al–4V10.1179/1743284715Y.0000000053 ↗
31. Fatigue performance evaluation of selective laser melted Ti-6Al-4V10.1016/j.msea.2014.01.041 ↗
32. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
33. Fatigue behavior of additive manufactured 316L stainless steel parts: Effects of layer orientation and surface roughness
34. Post processing methods used to improve surface finish of products which are manufactured by additive manufacturing technologies: a review10.1007/s40032-016-0340-z ↗
35. Laser peening: a tool for additive manufacturing post-processing
36. Laser polishing for improving fatigue performance of additive manufactured Ti-6Al-4V parts10.1016/j.optlastec.2020.106639 ↗
37. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
38. Surface post-treatments for metal additive manufacturing: progress, challenges, and opportunities
39. Standard method for microCT-based additive manufacturing quality control 3: surface roughness10.1016/j.mex.2018.09.004 ↗
40. International Organization for Standardization, ISO 4287:1997. Geometrical product specifications (GPS). Surface texture: profile method. Terms, definitions and surface texture parameters, Geneva, 1997.
41. Study of tool wear and surface roughness in machining of homogenised SiC-p reinforced aluminium metal matrix composite10.1016/j.jmatprotec.2005.02.109 ↗
42. Effect of process parameters on the surface roughness of overhanging structures in laser powder bed fusion additive manufacturing10.1016/j.procir.2016.02.347 ↗
43. The influence of additive manufacturing processing parameters on surface roughness and fatigue life10.1016/j.ijfatigue.2019.03.025 ↗
44. H. Neuber, Theory of notch stresses: principles for exact calculation of strength with reference to structural form and material, 1958.
45. Estimating the fatigue stress concentration factor of machined surfaces10.1016/S0142-1123(02)00012-9 ↗
46. Fatigue life estimation of additive manufactured parts in the as‐built surface condition
47. Fatigue behavior and modeling for additive manufactured 304l stainless steel: the effect of surface roughness10.1016/j.ijfatigue.2020.105856 ↗
48. ASTM International, ASTM E466 Standard Practice for Conducting Force Controlled Constant Amplitude Axial Fatigue Tests of Metallic Materials, West Conshohocken, PA, 2002, pp. 1–6. https://doi.org/10.1520/E0466-07.2.
49. ASTM International, Standard specification for additive manufacturing titanium-6 aluminum-4 vanadium with powder bed fusion, ASTM International, 2012, pp. 1–8. https://doi.org/10.1520/F2924-14.2.
50. Torsional fatigue behavior of wrought and additive manufactured Ti-6Al-4V by powder bed fusion including surface finish effect10.1016/j.ijfatigue.2017.03.002 ↗
51. ASTM International, ASTM E606 Standard Test Method for Strain-Controlled Fatigue Testing, West Conshohocken, PA, 2008, pp. 1–16. https://doi.org/10.1520/mnl10913m.10.1520/MNL10913M ↗
52. Combined effect of surface anomalies and volumetric defects on fatigue assessment of AlSi7Mg fabricated via laser powder bed fusion
53. Small fatigue crack growth under multiaxial stresses10.1016/j.ijfatigue.2013.02.002 ↗
54. Shamsaei · 2010
55. The effect of machined topography and integrity on fatigue life10.1016/j.ijmachtools.2003.10.018 ↗
56. Griffiths · 2001
57. Stout · 2000
58. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
59. An examination of the effects from surface texture on the strength of fiber reinforced plastics10.1177/002199839903300201 ↗
60. Powder recycling effects on the tensile and fatigue behavior of additively manufactured Ti-6Al-4V parts10.1007/s11837-018-3248-7 ↗
61. Investigation of the accuracy and roughness in the laser powder bed fusion process10.1080/17452759.2018.1426368 ↗
62. The effect of slip length and slip character on the properties of titanium alloys
63. R.W. Karry, T.J. Dolan, Influence of grain size on fatigue notch-sensitivity, University of Illinois at Urbana, Engineering Experiment Station, 1953.
64. J. Ruppen, P. Bhowal, D. Eylon, A.J. McEvily, On the process of subsurface fatigue crack initiation in Ti-6Al-4V. ASTM Special Technical Publication, 1979. https://doi.org/10.1520/stp35884s.10.1520/STP35884S ↗
65. Internal fatigue origins in α-β titanium allols10.1016/0001-6160(76)90147-4 ↗