Demonstrating the roles of solute and nucleant in grain refinement of additively manufactured aluminium alloys
Source abstract
Abstract
Grain refinement is one of the most effective approaches to improving mechanical properties, reducing anisotropy and hot-cracking of additively manufactured alloys. Recent studies have shown that the extreme solidification conditions associated with additive manufacturing (AM), including large thermal gradient and high cooling rate, result in the difference in nucleation and grain growth mechanisms between AM and conventional casting. Thus, it is necessary to re-consider the grain refinement mechanisms, particularly the role of solute during AM. The present work investigates the grain refining efficiencies of different solute additives (Si, Cu and Ni) and their integration with nucleants (LaB nanoparticles) in additively manufactured pure Al. It was found that, despite the fast cooling during AM and nucleant inoculation, solute addition is essential for activating heterogeneous nucleation upon solidification to achieve high grain refining efficiency. However, the role of solute in grain refinement during AM cannot be readily interpreted by the classic grain growth restriction theory (Q value). This is attributed to the large thermal gradient in the melt pools during AM solidification, which significantly limits the development of constitutional supercooling. Alternatively, the role of solute can be better understood in terms of the lag in dendrite growth induced by solute rejection during solidification. This causes the difference between the actual dendrite growth and the theoretical pull rate, generating large thermal undercooling ahead of the solidification front to elicit heterogeneous nucleation. This work sheds new light on the factors affecting grain refinement under fast cooling.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (80)
Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Revealing the mechanisms of grain nucleation and formation during additive manufacturing10.1007/s11837-020-04019-5 ↗
3. Grain refinement of alloys in fusion-based additive manufacturing processes10.1007/s11661-020-05880-4 ↗
4. Micromechanical simulations of additively manufactured aluminum alloys10.1016/j.compstruc.2020.106412 ↗
5. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
6. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
7. Effect of processing parameters on microstructure and tensile properties of austenitic stainless steel 304L made by directed energy deposition additive manufacturing10.1016/j.actamat.2016.03.019 ↗
8. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
9. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
10. Nafisi · 2016
11. Grain refinement of aluminum alloys: Part I. the nucleant and solute paradigms—a review of the literature10.1007/s11661-999-0098-5 ↗
12. Giacovazzo · 2002
13. Nucleation catalysis10.1021/ie50510a031 ↗
14. Mechanism of grain refinement in aluminium10.1016/0956-7151(94)00405-7 ↗
15. Revisiting the role of peritectics in grain refinement of Al alloys10.1016/j.actamat.2012.09.075 ↗
16. Supercooling and dendritic freezing in alloys
17. A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles10.1016/S1359-6454(00)00368-2 ↗
18. Effects of solute content on grain refinement in an isothermal melt10.1016/j.actamat.2011.01.008 ↗
19. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
20. The effect of boron on the grain size and texture in additively manufactured β-Ti alloys10.1007/s10853-017-1371-4 ↗
21. Peritectic titanium alloys for 3D printing10.1038/s41467-018-05819-9 ↗
22. Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability10.1016/j.msea.2020.139079 ↗
23. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
24. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
25. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
26. Effect of nano-TiB2 particles on the anisotropy in an AlSi10Mg alloy processed by selective laser melting10.1016/j.jallcom.2019.05.279 ↗
27. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
28. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
29. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
30. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
31. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
32. Selective laser melting of a high strength AlMnSc alloy: Alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
33. Additive manufacturing of ultrafine-grained austenitic stainless steel matrix composite via vanadium carbide reinforcement addition and selective laser melting: Formation mechanism and strengthening effect10.1016/j.msea.2019.01.008 ↗
34. Selective laser melting of dispersed TiC particles strengthened 316L stainless steel10.1016/j.compositesb.2020.108291 ↗
35. The Interdependence Theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
36. Grain refinement of Al alloys: Mechanisms determining as-cast grain size in directional solidification10.1016/j.actamat.2005.06.018 ↗
37. A quantitative study of solute diffusion field effects on heterogeneous nucleation and the grain size of alloys10.1016/j.actamat.2010.12.014 ↗
38. Heterogeneous nucleation and grain growth of inoculated aluminium alloys: an integrated study by in-situ X-radiography and numerical modelling10.1016/j.actamat.2017.08.053 ↗
39. Revealing the heterogeneous nucleation behavior of equiaxed grains of inoculated Al alloys during directional solidification10.1016/j.actamat.2018.02.058 ↗
40. Understanding the refinement of grains in laser surface remelted Al–Cu alloys10.1016/j.scriptamat.2019.12.020 ↗
41. Modelling of inoculation of metallic melts: application to grain refinement of aluminium by Al–Ti–B10.1016/S1359-6454(00)00094-X ↗
42. Towards understanding grain nucleation under Additive Manufacturing solidification conditions10.1016/j.actamat.2020.05.012 ↗
43. Microstructure formation in rapidly solidified alloys
44. Model for solute redistribution during rapid solidification10.1063/1.329867 ↗
45. Solute trapping in aluminum alloys10.1016/0956-7151(94)90483-9 ↗
46. Kurz · 1992
47. Nucleation potency prediction of LaB6 with E2EM model and its influence on microstructure and tensile properties of Al-7Si-0.3Mg alloy10.1016/S1003-6326(18)64812-5 ↗
48. Enhanced grain refinement of in situ CeB6/Al composite inoculant on pure aluminum by microstructure control10.1016/j.jallcom.2017.01.188 ↗
49. Laser powder bed fusion of nano-CaB6 decorated 2024 aluminum alloy10.1016/j.jallcom.2021.158714 ↗
50. Uncovering the role of LaB6-nanoparticle content on the microstructure and mechanical properties of AlSi10Mg alloy fabricated by selective laser melting
51. Crystallographic features of phase transformations in solids10.1016/j.pmatsci.2009.06.001 ↗
52. Polmear · 1995
53. Grain refining efficiency and the role of alloying elements in determining the nucleation potency of LaB6 in aluminum alloys10.1007/s11837-019-03970-2 ↗
54. A study of the microstructure and the mechanical properties of an AlSiNi alloy produced via selective laser melting10.1016/j.jallcom.2016.10.285 ↗
55. Texture control during laser deposition of nickel-based superalloy10.1016/j.scriptamat.2012.06.014 ↗
56. Texture control of 316L parts by modulation of the melt pool morphology in selective laser melting10.1016/j.jmatprotec.2018.08.049 ↗
57. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
58. Quantification of microsegregation during rapid solidification of Al-Cu powders10.1007/s11661-006-0102-2 ↗
59. Selective laser melting of high strength Al–Cu–Mg alloys: Processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
60. Grain boundary nucleation kinetics10.1016/0001-6160(69)90057-1 ↗
61. Influence of Cr on the nucleation of primary Al and formation of twinned dendrites in Al-Zn-Cr alloys: Can icosahedral solid clusters play a role?10.1016/j.actamat.2013.07.056 ↗
62. Icosahedral quasicrystal-enhanced nucleation of the fcc phase in liquid gold alloys10.1016/j.actamat.2014.02.037 ↗
63. New insights into the origin of fine equiaxed microstructures in additively manufactured Inconel 71810.1016/j.scriptamat.2021.113740 ↗
64. Icosahedral quasicrystal-enhanced nucleation in Al alloys fabricated by selective laser melting
65. Multi-scale microstuctural investigation of a new Al-Mn-Ni-Cu-Zr aluminium alloy processed by laser powder bed fusion10.1016/j.mtla.2021.101160 ↗
66. Homogeneous nucleation and growth of droplets in vapours10.1080/00018736600101264 ↗
67. Prediction of phase selection in rapid solidification using time dependent nucleation theory10.1016/0956-7151(94)90391-3 ↗
68. Wetting of ceramics by liquid aluminum10.1111/j.1151-2916.1970.tb12138.x ↗
69. The influence of nickel coating on the wettability of aluminum on ceramics10.1016/S1359-835X(02)00161-6 ↗
70. Formation of metastable crystalline phases in light-metal systems by rapid solidification10.1080/13642819008219289 ↗
71. Diffusion coefficients of some solutes in fcc and liquid Al: critical evaluation and correlation10.1016/S0921-5093(03)00624-5 ↗
72. Kargl · J. Phys.: Conf. Ser. · 2012 · 340
73. Nanoparticle-inhibited growth of primary aluminum in Al–10Si alloys10.1016/j.actamat.2015.10.005 ↗
74. Effect of cooling rate on grain refinement of cast aluminium alloys10.1016/j.mtla.2018.08.008 ↗
75. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles10.1007/s11661-005-0054-y ↗
76. An analytical model for constitutional supercooling-driven grain formation and grain size prediction10.1016/j.actamat.2010.01.052 ↗
77. Effect of Grain Refinement on Tensile Properties of Cast Zinc Alloys10.1007/s11661-015-3229-1 ↗
78. Effects of boron on microstructure in cast titanium alloys10.1016/j.scriptamat.2008.05.002 ↗
79. A. Prasad, Microsegregation studies of rapidly solidified binary aluminum-copper alloys (Diss.), University of Alberta, 2006.
80. No more tears for metal 3D printing10.1038/549342a ↗