Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys

Guichuan Li, Etienne Brodu, Jeroen Soete, Huiliang Wei, Tingting Liu, Tao Yang, Wenhe Liao, Kim Vanmeensel

Publisher page

Abstract

Abstract This work describes a systematic alloy design strategy resulting in the development of a high strength aluminum alloy adopted for L -PBF. First, based on the composition of a reference Al-Cu-Mg alloy, three Al-Cu-Mg-Mn-Zr-based alloys were investigated using computational thermodynamic tools. Subsequently, the L -PBF processing behavior, microstructure, and concomitant mechanical properties of the L -PBF-fabricated alloys were investigated. Alloys with different compositions showed substantial differences in microstructure: the alloy without Zr addition showed a coarse columnar microstructure and suffered from solidification cracking, alloys with low to mediate Zr additions (1–1.98 wt%) showed a mixed columnar and equiaxed microstructure, while alloys with high Zr addition (3.72 wt%) showed a fully equiaxed microstructure, accompanied by a grain size reduction down to 0.7 ± 0.3 µm. All alloys containing ≥ 1.98 wt% Zr were crack-free. The L -PBF-processed Al-4.40Cu-1.51Mg-1.15Mn-3.72Zr (wt%) alloy showed an extended Zr solid solubility in the Al matrix of ~ 1.3 ± 0.1 wt%. Coherent primary Al3Zr particles with a cubic L12 structure were formed in all the Zr-containing alloys. The mechanical properties of as-built alloys increased consistently with increasing Zr contents from 0 to 3.72 wt%. The designed Al-4.40Cu-1.51Mg-1.15Mn-3.72Zr (wt%) alloy combined a yield strength of 561 ± 24 MPa, an ultimate tensile strength of 580 ± 16 MPa, and an elongation at break of 6.0 ± 1.3%. The exceptionally high strength of this alloy is attributed to a combination of grain refinement, Orowan, solid solution, and dislocation strengthening. The current work shows the intrinsic potential of rapid solidification occurring during L -PBF for the fabrication of geometrically-complex, high-strength lightweight parts made of ultra-fine-grained hyper-peritectic aluminum alloys containing transition element additions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Increasing the productivity of laser powder bed fusion: influence of the hull-bulk strategy on part quality, microstructure and mechanical performance of Ti-6Al-4V
2. Multiprocess 3D printing for increasing component functionality
3. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
4. Effect of temperature on the microstructure and tensile properties of micro-crack free hastelloy X produced by selective laser melting
5. Surface modified copper alloy powder for reliable laser-based additive manufacturing
6. Metallurgy, mechanistic models and machine learning in metal printing10.1038/s41578-020-00236-1 ↗
7. Formation of metastable cellular microstructures in selective laser melted alloys10.1016/j.jallcom.2016.12.209 ↗
8. New aluminum alloys specifically designed for laser powder bed fusion: a review10.3390/ma12071007 ↗
9. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
10. A comparison of selective laser melting with bulk rapid solidification of AlSi10Mg alloy10.1016/j.jallcom.2018.01.309 ↗
11. Precipitation kinetics, microstructure evolution and mechanical behavior of a developed Al–Mn–Sc alloy fabricated by selective laser melting10.1016/j.actamat.2020.04.015 ↗
12. Interface velocity dependent solute trapping and phase selection during rapid solidification of laser melted hypo-eutectic Al-11at%Cu alloy10.1016/j.actamat.2020.04.006 ↗
13. Microstructure characterization of SLM-processed Al-Mg-Sc-Zr alloy in the heat treated and HIPed condition
14. Control of thermally stable core-shell nano-precipitates in additively manufactured Al-Sc-Zr alloys
15. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
16. Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion
17. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
18. Crystallographic study of Al3Zr and Al3Nb as grain refiners for Al alloys10.1016/S1003-6326(14)63309-4 ↗
19. Grain refinement mechanisms in additively manufactured nano-functionalized aluminum10.1016/j.actamat.2020.09.043 ↗
20. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
21. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
22. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
23. Scanning strategies for texture and anisotropy tailoring during selective laser melting of TiC/316L stainless steel nanocomposites10.1016/j.jallcom.2017.08.022 ↗
24. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
25. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
26. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
27. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
28. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
29. Crack mitigation in laser powder bed fusion processed hastelloy X using a combined numerical-experimental approach10.1016/j.jallcom.2021.158803 ↗
30. Evaluation of solidification cracking susceptibility during laser welding in advanced high strength automotive steels10.1016/j.matdes.2019.108104 ↗
31. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
32. On the hot cracking of HSLA steel welds: role of epitaxial growth and HAZ grain size10.1016/j.jmapro.2019.03.032 ↗
33. Additively manufactured novel Al-Cu-Sc-Zr alloy: microstructure and mechanical properties
34. Effect of energy density on formability, microstructure and micro-hardness of selective laser melted Sc- and Zr- modified 7075 aluminum alloy10.1016/j.powtec.2019.08.082 ↗
35. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
36. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
37. Grain structure evolution of Al–Cu alloys in powder bed fusion with laser beam for excellent mechanical properties10.3390/ma13010082 ↗
38. Laser powder bed fusion of AlSi10Mg: influence of energy intensities on spatter and porosity evolution, microstructure and mechanical properties10.1016/j.jallcom.2020.156300 ↗
39. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
40. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by laser-based powder bed fusion10.1007/s11661-020-06073-9 ↗
41. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
42. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
43. Design approaches for printability-performance synergy in Al alloys for laser-powder bed additive manufacturing10.1016/j.matdes.2021.109640 ↗
44. Dendritic and seaweed growth of proeutectic scandium tri-aluminide in hypereutectic Al-Sc undercooled melt10.1016/j.actamat.2020.08.078 ↗
45. The origin of high-density dislocations in additively manufactured metals10.1080/21663831.2020.1751739 ↗
46. First-principles calculation of structural energetics of Al-TM (TM = Ti, Zr, Hf) intermetallics10.1016/j.actamat.2005.03.028 ↗
47. Modelling of inoculation of metallic melts: application to grain refinement of aluminium by Al-Ti-B10.1016/S1359-6454(00)00094-X ↗
48. Grain refinement limit and mechanical properties of 6063 alloy inoculated by Al–Ti–C (B) master alloys10.1016/j.jallcom.2014.01.145 ↗
49. The Portevin-Le Chatelier (PLC) effect and shear band formation in an AA5754 alloy10.1016/j.actamat.2007.03.007 ↗
50. K. Anderson, J. Weritz, J.G. Kaufman, 2024 and Alclad 2024, in: Prop. Sel. Alum. Alloy 2019 ASM International, 298 303 doi: 10.31399/asm.hb.v02b.a0006598.10.31399/asm.hb.v02b.a0006598 ↗
51. Development of a high strength Al–Zn–Si–Mg–Cu alloy for selective laser melting10.1016/j.jallcom.2019.06.123 ↗
52. Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability10.1016/j.msea.2020.139079 ↗
53. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
54. Metals Handbook · 1990
55. Study of size effect on microstructure and mechanical properties of AlSi10Mg samples made by selective laser melting10.3390/ma11122463 ↗
56. Characterisation of structural properties for AlSi10Mg alloys fabricated by selective laser melting10.1080/02670836.2017.1398513 ↗
57. Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing
58. Electronic cigarette use among patients with cancer: characteristics of electronic cigarette users and their smoking cessation outcomes10.1002/cncr.29118 ↗
59. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
60. Laser powder bed fusion of AA7075 alloy: Influence of process parameters on porosity and hot cracking
61. Prediction of solidification cracking in pulsed laser welding of 2024 aluminum alloy10.1016/j.actamat.2014.09.002 ↗
62. Cracking criterion for high strength Al–Cu alloys fabricated by selective laser melting
63. Kurz · 1998 · 316
64. Metastable phase and grain refinement in rapidly solidified Al-Zr alloys10.2464/jilm.31.793 ↗
65. Grain refinement of commercially pure aluminum with addition of Ti and Zr elements based on crystallography orientation
66. Metastable phases in the Al3X (X = Ti, Zr, and Hf) intermetallic system10.1016/0956-716X(91)90059-A ↗
67. The solid solution strengthening in Al-Zr nanocrystalline alloy films10.1016/j.surfcoat.2017.04.048 ↗
68. Simultaneous enhancement of strength, ductility, and hardness of TiN/AlSi10Mg nanocomposites via selective laser melting
69. Tracking the path of dislocations across ordered Al3Zr nano-precipitates in three dimensions10.1016/j.scriptamat.2013.09.014 ↗
70. Study of Lüders phenomena in reactor pressure vessel steels10.1016/j.msea.2013.05.021 ↗
71. On the role of Zr content into Portevin-Le Chatelier (PLC) effect of selective laser melted high strength Al-Cu-Mg-Mn alloy10.1016/j.matlet.2019.03.112 ↗
72. On the nature of the yield point phenomenon10.1016/j.actamat.2012.12.003 ↗
73. Strength and ductility of ultrafine grained aluminum and iron produced by ARB and annealing10.1016/S1359-6462(02)00282-8 ↗
74. On the microstructure and solidification behavior of new generation additively manufactured Al-Cu-Mg-Ag-Ti-B alloys
75. Underlying material response for Lüders-like instabilities10.1016/j.ijplas.2012.12.002 ↗
76. Laser powder bed fusion of high-strength Sc/Zr-modified Al–Mg alloy: phase selection, microstructural/mechanical heterogeneity, and tensile deformation behavior10.1016/j.jmst.2021.03.069 ↗
77. The influence of microstructural characteristics on yield point elongation phenomenon in Fe-0.2C–11Mn-2Al steel10.1016/j.msea.2018.09.114 ↗
78. Mechanical behaviors of ultrafine-grained 301 austenitic stainless steel produced by equal-channel angular pressing10.1007/s11661-010-0575-x ↗
79. Effect of defocusing distance on laser powder bed fusion of high strength Al–Cu–Mg–Mn alloy10.1080/17452759.2020.1760895 ↗
80. Optimizing the strength and ductility of fine structured 2024 Al alloy by nano-precipitation10.1016/j.actamat.2007.06.043 ↗