journal article·2018-03

Achieving low surface roughness AlSi10Mg_200C parts using direct metal laser sintering

Mohsen Mohammadi, Hamed Asgari

Publisher page

Abstract

Abstract Laser sintered aluminum alloys produced by metal 3D printers can replace cast aluminum alloys in aerospace, defense, and marine industries by offering better mechanical properties, less porosity, and competitive fatigue characteristics. One of the major issues currently is the considerable surface roughness of additively manufactured aluminum alloys demanding post-processing procedures such as bead blasting or machining. In the current study, the process parameters such as laser power, scan speed, and hatch spacing were altered such that better surface roughness could be achieved for AlSi10Mg_200C using a Direct Metal Laser Sintering (DMLS) system. The process parameters were chosen such that three samples with the same core properties but different upskin characteristics were produced. The achieved surface roughness of the additively manufactured aluminum samples were almost as low as one fifth of the regular samples manufactured using standard process parameters. The microstructure and the porosity level of the samples printed by different process parameters were studied to reveal the causality of the low surface roughness for the proposed process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Manufacturing Process and Optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
2. Gibson · 2015
3. EOS Electro Optical Systems GmbH. (2017) [Online]. www.eos.info.
4. Direct metal laser sintering for rapid tooling: processing and characterisation of EOS parts10.1016/S0924-0136(01)00584-2 ↗
5. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
6. Case study: additive manufacturing of aerospace brackets
7. Multiple material additive manufacturing, Part1: a review10.1080/17452759.2013.778175 ↗
8. Design guidelines for laser additive manufacturing of lightweight structures in TiAl6V410.2351/1.4885235 ↗
9. Progress in additive manufacturing
10. Wohlers report—3D printing and additive manufacturing state of the industry
11. Selective laser melting (SLM) and topology optimization for lighter aerospace componentes10.1016/j.prostr.2016.02.039 ↗
12. Material and design considerations for rapid manufacturing10.1080/00207840410001733940 ↗
13. On the formation of AlSi10Mg single tracks and layers in selective laser melting: microstructure and nano-mechanical properties10.1016/j.jmatprotec.2015.11.016 ↗
14. Effect of Ce on solidification and mechanical properties of A360 alloy10.1016/j.jallcom.2011.04.059 ↗
15. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
16. On microstructure and mechanical properties of additively manufactured AlSi10Mg_200C using recycled powder10.1016/j.msea.2017.09.041 ↗
17. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
18. Selective laser melting of AlSi10Mg: effects of scan direction, part placement and inert gas flow velocity on tensile strength10.1016/j.jmatprotec.2016.10.015 ↗
19. On the selective laser melting (SLM) of the AlSi10Mg alloy: process, microstructure, and mechanical properties10.3390/ma10010076 ↗
20. On the effect of process parameters on properties of AlSi10Mg parts produced by DMLS10.1108/RPJ-03-2013-0028 ↗
21. Processing AlSi10Mg by selective laser melting: parameter optimization and material characterization10.1179/1743284714Y.0000000702 ↗
22. Selective laser melting of AlSi10Mg alloy: process optimization and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
23. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
24. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
25. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
26. Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by selective laser melting10.1016/j.msea.2016.11.070 ↗
27. On dynamic mechanical behavior of additively manufactured AlSi10Mg_200C10.1016/j.matlet.2017.10.001 ↗
28. Improved tensile properties of a new aluminum alloy for high pressure die casting10.1016/j.msea.2015.10.127 ↗
29. Additive manufactured AlSi10Mg samples using selective laser melting (SLM): microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
30. A.S.M., Handbook · 1990 · vol. 2
31. Oxides, porosity and fatigue performance of AlSi10Mg parts produced by selective laser melting10.1016/j.ijfatigue.2016.06.002 ↗
32. Reducing porosity in AlSi10Mg parts processed by selective laser melting
33. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
34. Measurement and analysis of porosity in Al-10Si-1Mg components additively manufactured by selective laser melting10.1520/MPC20160037 ↗
35. Surface roughness and morphology customization of additive manufactured open porous Ti6Al4 V structures10.3390/ma6104737 ↗
36. Influence of process parameters on surface roughness of aluminum parts produced by DMLS10.1007/s00170-012-4688-9 ↗
37. Impact of chemical finishing on laser-sintered nylon 12 materials
38. Influences of processing parameters on surface roughness of Hastelloy X produced by selective laser melting
39. On the surface quality of additive manufactured parts10.1007/s00170-016-9215-y ↗
40. Surface roughness and bone healing: a systematic review10.1177/154405910608500603 ↗
41. Corrosion behavior of AlSi10Mg alloy produced by additive manufacturing (AM) vs. its counterpart gravity cast alloy10.3390/met6070148 ↗
42. The numerical modeling of fatigue properties of a bio-compatible dental implant produced by electron beam melting (EBM)
43. Stephens · 2000
44. The intergranular corrosion behavior of 6000-series alloys with different Mg/Si and Cu content10.1016/j.apsusc.2017.02.045 ↗
45. Characterization of atmospheric corrosion of 2A12 aluminum alloy in tropical marine environment10.1007/s11665-009-9506-7 ↗
46. Molland · 2017
47. The effect of defects on the mechanical response of Ti-6Al-4 V cubic lattice structures fabricated by electron beam melting10.1016/j.actamat.2016.02.029 ↗
48. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
49. Microstructure and mechanical properties of aluminium alloy cellular lattice structures manufactured by direct metal laser sintering10.1016/j.msea.2015.01.063 ↗
50. From powders to dense metal parts: characterization of a commercial AlSiMg alloy processed through direct metal laser sintering10.3390/ma6030856 ↗
51. Microstructural evolution during annealing of a rapidly solidified Al–12Si alloy10.1016/j.jallcom.2006.08.068 ↗
52. Dental implant surface enhancement and osseointegration
53. Fatigue behavior and failure mechanisms of direct laser deposited Ti-6Al-4 V10.1016/j.msea.2015.12.026 ↗
54. Corrosion behavior and microstructure of direct metal laser sintered AlSi10Mg_200C alloy versus aluminum A360.1 die casting
55. Multiaxial fatigue behavior of wrought and additive manufactured Ti-6Al-4 V including surface finish effect10.1016/j.ijfatigue.2017.03.044 ↗
56. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by selective laser melting (SLM)10.1016/j.matchar.2017.06.029 ↗
57. Binding mechanisms in selective laser sintering and selective laser melting10.1108/13552540510573365 ↗
58. Selective laser sintering of gas atomized M2 high speed steel powder10.1023/A:1004720011671 ↗
59. On optimization of surface roughness of selective laser melted stainless steel parts: a statistical study10.1007/s11665-014-0993-9 ↗
60. Statistical modelling and optimization of surface roughness in the selective laser sintering process10.1243/09544054JEM670 ↗