journal article·2019-08Open access

Biodegradation-affected fatigue behavior of additively manufactured porous magnesium

Y. Li, H. Jahr, X-Y. Zhang, M.A. Leeflang, W. Li, B. Pouran, F.D. Tichelaar, H. Weinans, J. Zhou, A.A. Zadpoor

Abstract

Abstract Additively manufactured (AM) biodegradable metals with topologically ordered porous structures hold unprecedented promise as potential bone substitutes. The first reports on this type of biomaterials have just recently appeared in the literature. There is, however, no information available in the literature regarding their mechanical performance under cyclic loading or the interactions between biodegradation and cyclic loading. We therefore used selective laser melting (SLM) to fabricate porous magnesium alloy (WE43) scaffolds based on diamond unit cells. The microstructure of the resulting material was examined using electron back-scattered diffraction, scanning transmission electron microscopy, and X-ray diffraction. The fatigue behaviors of the material in air and in revised simulated body fluid (r-SBF) were evaluated and compared. Biodegradation decreased the fatigue strength of the porous material from 30% to 20% of its yield strength. Moreover, cyclic loading significantly increased its biodegradation rate. The mechanistic aspects of how biodegradation and cyclic loading interacted with each other on different scales were revealed as well. On the micro-scale, cracks initiated at biodegradation pits and propagated transgranularly. In addition, dislocations became more tangled after the fatigue tests. On the macro-scale, cracks preferred initiating at the strut junctions where tensile stress concentrations were present, as revealed by the finite element analysis of the porous material under compressive loading. Most of the cracks initiated in the struts were positioned on the periphery of the specimens. Furthermore, the biodegradation pattern was found to be location-dependent with more localized biodegradation occurring in the center of the specimens. Further improvements in the biodegradation-affected fatigue performance of the AM porous Mg alloy may therefore be realized by optimizing both the topological design of the porous structure and the laser-processing parameters that determine the microstructure of the SLM porous material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
2. Corrosion fatigue fracture of magnesium alloys in bioimplant applications: a review10.1016/j.engfracmech.2014.08.009 ↗
3. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
4. Biodegradable behaviors of AZ31 magnesium alloy in simulated body fluid10.1016/j.msec.2008.08.026 ↗
5. Additively manufactured biodegradable porous iron10.1016/j.actbio.2018.07.011 ↗
6. Laser additive manufacturing of Zn porous scaffolds: shielding gas flow, surface quality and densification
7. Additively manufactured biodegradable porous magnesium10.1016/j.actbio.2017.12.008 ↗
8. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
9. Calcium phosphate coatings on magnesium alloys for biomedical applications: a review10.1016/j.actbio.2011.10.016 ↗
10. Design of magnesium alloys with controllable degradation for biomedical implants: from bulk to surface10.1016/j.actbio.2016.09.005 ↗
11. Corrosion behaviour of AZ31 magnesium alloy with different grain sizes in simulated biological fluids10.1016/j.actbio.2009.04.041 ↗
12. Influence of fine-grain and solid-solution strengthening on mechanical properties and in vitro degradation of WE43 alloy
13. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
14. Corrosion of, and cellular responses to Mg-Zn-Ca bulk metallic glasses10.1016/j.biomaterials.2009.11.015 ↗
15. Ductile biodegradable Mg-Based metallic glasses with excellent biocompatibility10.1002/adfm.201203738 ↗
16. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
17. Current status on clinical applications of magnesium-based orthopaedic implants: a review from clinical translational perspective10.1016/j.biomaterials.2016.10.017 ↗
18. Revival of pure titanium for dynamically loaded porous implants using additive manufacturing10.1016/j.msec.2015.05.001 ↗
19. Relationship between unit cell type and porosity and the fatigue behavior of selective laser melted meta-10.1016/j.jmbbm.2014.12.015 ↗
20. Additively manufactured metallic porous biomaterials based on minimal surfaces: a unique combination of topological, mechanical, and mass transport properties10.1016/j.actbio.2017.02.024 ↗
21. Compression fatigue behavior of Ti–6Al–4V mesh arrays fabricated by electron beam melting10.1016/j.actamat.2011.10.051 ↗
22. Compressive and fatigue behavior of beta-type titanium porous structures fabricated by electron beam melting10.1016/j.actamat.2016.12.052 ↗
23. Fatigue performance of additively manufactured meta-biomaterials: the effects of topology and material type10.1016/j.actbio.2017.11.014 ↗
24. CoCr F75 scaffolds produced by additive manufacturing: influence of chemical etching on powder removal and mechanical performance10.1016/j.jmbbm.2017.03.017 ↗
25. Additively manufactured porous tantalum implants10.1016/j.actbio.2014.12.003 ↗
26. Fatigue behaviors of HP-Mg, Mg–Ca and Mg–Zn–Ca biodegradable metals in air and simulated body fluid10.1016/j.actbio.2016.05.031 ↗
27. Stress corrosion cracking and corrosion fatigue characterisation of MgZn1Ca0.3 (ZX10) in a simulated physiological environment10.1016/j.jmbbm.2016.09.033 ↗
28. Corrosion fatigue behaviors of two biomedical Mg alloys – AZ91D and WE43 – in simulated body fluid10.1016/j.actbio.2010.07.026 ↗
29. Biodegradable magnesium-based screw clinically equivalent to titanium screw in hallux valgus surgery: short term results of the first prospective, randomized, controlled clinical pilot study10.1186/1475-925X-12-62 ↗
30. Preparation and assessment of revised simulated body fluids10.1002/jbm.a.10482 ↗
31. Effect of loading frequency on cyclic fatigue lifetime of a standard-diameter implant with an internal abutment connection10.1016/j.dental.2018.09.001 ↗
32. Montreal (Canada)Microstructure and Properties of WE43 Manufactured via SLM. Symposium on Biodegradable Metals for Biomedical Applications. 14 May 2016 - 17 May 20162016
33. Microstructure and mechanical properties of selective laser melted magnesium10.1016/j.apsusc.2011.03.004 ↗
34. Dupont · 2019 · 700
35. Selective laser melting of magnesium and magnesium alloy powders: a review10.3390/met7010002 ↗
36. Grain structure control of additively manufactured metallic materials10.3390/ma10111260 ↗
37. Characterization of microstructure and mechanical properties of laser melting deposited Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.matdes.2013.11.044 ↗
38. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
39. Fatigue and tensile behavior of cast, hot-rolled, and severely plastically deformed AZ31 magnesium alloy10.1007/s11661-007-9109-6 ↗
40. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
41. Effects of grain size on the corrosion resistance of wrought magnesium alloys containing neodymium10.1016/j.corsci.2012.01.021 ↗
42. The effects of heat treatment on very high cycle fatigue behavior in hot-rolled WE43 magnesium10.1016/j.ijfatigue.2016.05.033 ↗
43. Effect of aging treatment on fatigue behaviour in extruded AZ61 and AZ80 magnesium alloys10.1016/j.msea.2009.03.066 ↗
44. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
45. AC impedance spectroscopy in characterizing time-dependent corrosion of AZ91 and AM50 magnesium alloys characterization with respect to their microstructures10.1149/1.1415722 ↗
46. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
47. Grain size distribution effects on the corrosion behaviour of materials10.1016/j.corsci.2012.04.040 ↗
48. Fatigue failure of an open cell and a closed cell aluminium alloy foam10.1016/S1359-6454(99)00097-X ↗
49. The stress–life fatigue behaviour of aluminium alloy foams10.1046/j.1460-2695.2000.00261.x ↗
50. Compression–compression fatigue of open cell aluminum foams: macro-/micro- mechanisms and the effects of heat treatment10.1016/j.msea.2003.08.009 ↗
51. Corrosion fatigue behavior of extruded magnesium alloy AZ80-T5 in a 5% NaCl environment10.1016/j.engfracmech.2010.03.032 ↗
52. Corrosion fatigue of a magnesium alloy in modified simulated body fluid10.1016/j.engfracmech.2014.07.007 ↗
53. Effects of humidity and temperature on the fatigue behaviour of an extruded AZ61 magnesium alloy10.1111/j.1460-2695.2005.00775.x ↗
54. The role of twinning–detwinning on fatigue fracture morphology of Mg–3%Al–1%Zn alloy10.1016/j.msea.2008.04.056 ↗
55. High cycle fatigue of a die cast AZ91E-T4 magnesium alloy10.1016/j.actamat.2003.11.018 ↗
56. Influence of shot peening on high cycle fatigue properties of the high-strength wrought magnesium alloy AZ8010.1016/j.scriptamat.2004.11.003 ↗
57. Low-cycle fatigue characteristics of rolled Mg–3Al–1Zn alloy10.1016/j.ijfatigue.2010.05.002 ↗
58. Low cycle fatigue of a rare-earth containing extruded magnesium alloy10.1016/j.msea.2013.03.041 ↗
59. Fatigue behavior of porous biomaterials manufactured using selective laser melting10.1016/j.msec.2013.08.006 ↗
60. Additively manufactured biodegradable porous iron