journal article·2020-12

Surface roughness in laser powder bed fusion – Interdependency of surface orientation and laser incidence

Sebastian Rott, Alexander Ladewig, Katrin Friedberger, Johannes Casper, Moritz Full, Johannes Henrich Schleifenbaum

Publisher page

Abstract

Abstract Additive Manufacturing (AM) offers the opportunity for the manufacture of innovative parts with complex geometries and new possibilities regarding complex part design. However, the relatively high surface roughness of as-built parts is a considerable limitation and one of the challenges in AM. Laser powder bed fusion (L-PBF) is one AM technique for the manufacture of metallic serial parts. Although the effect of various process parameters on the surface roughness in L-PBF has been studied, a prediction of surface roughness at the pre-processing stage has not been achieved yet. The interdependency of the surface orientation and the laser incidence, although it is mentioned in literature, is still not yet analyzed or quantified. Therefore, the novel parameter surface laser relation angle ζ is introduced to quantify this interdependency and act as a parameter to predict surface roughness. By using a constant laser relation angle ζ the range of roughness parameter R a on surfaces across the entire build platform can be decreased from 19 μm to 11 μm in comparison to the usage of a constant surface normal polar angle α . By this method the standard deviation is decreased from 5 μm to 2 μm as well with a constant arithmetic mean of 24 μm on both methods. Similar behavior can also be seen for the roughness parameter R z in this work. The results achieved so far lay the basis for a homogenization of the surface roughness across the entire build platform.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Gebhardt · 2019
2. Additive design and manufacturing of jet engine parts10.1016/J.ENG.2017.05.017 ↗
3. Understanding optimization and simulation of aero-structure design for next generation production with a metal additive manufacturing process
4. Selective laser melting (SLM) and topology optimization for lighter aerospace componentes
5. Effect of surface roughness on fatigue performance of additive manufactured Ti–6Al–4V10.1179/1743284715Y.0000000053 ↗
6. Influence of surface topography on fatigue behavior of Ti6Al4V alloy by laser powder bed fusion10.1016/j.procir.2018.08.028 ↗
7. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
8. On the effect of shot-peening on fatigue resistance of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting (AM-SLM)
9. Internal surface roughness enhancement of parts made by laser powder-bed fusion additive manufacturing
10. Modelling of laser powder bed fusion process and analysing the effective parameters on surface characteristics of Ti-6Al-4V
11. Manufacturing by combining selective laser melting and selective laser erosion/laser re-melting10.1016/j.cirp.2011.03.063 ↗
12. Layer-by-layer combination of laser powder bed fusion (LPBF) and femtosecond laser surface machining of fabricated stainless steel components10.1016/j.jmapro.2018.08.016 ↗
13. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
14. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
15. Tailoring surface quality through mass and momentum transfer modeling using a volume of fluid method in selective laser melting of TiC/AlSi10Mg powder10.1016/j.ijmachtools.2014.09.010 ↗
16. On the role of powder flow behavior in fluid thermodynamics and laser processability of Ni-based composites by selective laser melting10.1016/j.ijmachtools.2018.10.006 ↗
17. Main defects observed in aluminum alloy parts produced by SLM: from causes to consequences
18. On the measurement of relative powder-bed compaction density in powder-bed additive manufacturing processes10.1016/j.matdes.2018.06.030 ↗
19. Position dependent surface quality in selective laser melting
20. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
21. Effect of laser focus shift on surface quality and density of Inconel 718 parts produced via selective laser melting
22. Reliable beam positioning for metal-based additive manufacturing by means of focal shift reduction
23. Influences of processing parameters on surface roughness of Hastelloy HastelloyX produced by selective laser melting
24. Effect of process parameters on the surface roughness of overhanging structures in laser powder bed fusion additive manufacturing10.1016/j.procir.2016.02.347 ↗
25. Part geometry and conduction-based laser power control for powder bed fusion additive manufacturing
26. Characterization of typical surface effects in additive manufacturing with confocal microscopy10.1088/2051-672X/3/1/014001 ↗
27. Effect of process parameters on the generated surface roughness of down-facing surfaces in selective laser melting10.3390/app9061256 ↗
28. Influence of the particle size distribution on surface quality and mechanical properties in additive manufactured stainless steel parts10.1108/13552541111124770 ↗
29. Surface roughness of selective laser melted Ti-6Al-4V alloy components
30. The role of powder layer thickness on the quality of SLM printed parts10.1016/j.acme.2018.01.015 ↗
31. Non-destructive evaluation of AlSi10Mg prismatic samples generated by selective laser melting: Influence of manufacturing conditions
32. On the effect of spatter particles distribution on the quality of Hastelloy X parts made by laser powder-bed fusion additive manufacturing10.1016/j.jmapro.2018.11.012 ↗
33. Influence of the shielding gas flow on the removal of process
34. Effect of metal vaporization behavior on keyhole-mode surface morphology of selective laser melted composites using different protective atmospheres10.1016/j.apsusc.2015.07.044 ↗
35. Position dependency of surface roughness in parts from laser beam melting systems
36. Impact of build envelope on the properties of additive manufactured parts from AlSi10Mg10.1016/j.optlastec.2018.08.050 ↗
37. Oerlikon metco · 2017
38. Surface texture metrology for metal additive manufacturing: a review10.1016/j.precisioneng.2016.06.001 ↗
39. DIN · 2013
40. DIN · 2010
41. Verein Deutscher Ingenieure · 2015
42. Surface roughness optimisation for selective laser melting (SLM): accommodating relevant and irrelevant surfaces
43. Process monitoring dataset from the additive manufacturing metrology testbed (AMMT): “three-dimensional scan strategies
44. Papula · 2009
45. Numerical study of keyhole dynamics and keyhole-induced porosity formation in remote laser welding of Al alloys10.1016/j.ijheatmasstransfer.2016.12.019 ↗
46. R. A. Domröse, M. Frey, A. Schilling, A. Danzig, J. Hamann, T. Heß und M. Dimter, Verfahren, Vorrichtung zum Herstellen eines dreidimensionalen Objekts“. Deutschland Patent DE 10 2013 205 724 A1, 02 10 2014.
47. Microstructure and directional fatigue behavior of Inconel 718 produced by selective laser melting