journal article·2020-12

Pure tungsten and oxide dispersion strengthened tungsten manufactured by selective laser melting: Microstructure and cracking mechanism

Zhangping Hu, Yanan Zhao, Kai Guan, Zumin Wang, Zongqing Ma

Publisher page

Abstract

Abstract The microstructure and cracking behavior of pure tungsten and micron- and nanosized Y2O3 dispersion strengthened tungsten fabricated by selective laser melting are comparatively studied in this work. The pure tungsten with high density (98.3 ± 0.3 %) is successfully fabricated by optimizing processing parameters, but there are still a few microcracks. The cracking mechanism of pure tungsten is attributed to the segregation of tungsten oxide impurities at the grain boundaries and the formation of high-angle grain boundaries. The agglomeration of Y2O3 occurs only in the tungsten with the addition of micron-Y2O3 while not in the tungsten with the addition of nanosized Y2O3. The addition of Y2O3 can reduce cracks due to the formation of a large number of low-angle twisted tungsten grains. The cracking mechanism of pure tungsten and the inhibition of cracking by the addition of Y2O3 proposed in this work are of great significance for the SLM manufacture of high-performance and crack-free tungsten-based alloys. Our work may also provide relevant strategy for the suppression of crack in other alloys with high melting point by SLM.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Smart tungsten alloys as a material for the first wall of a future fusion power plant10.1088/1741-4326/aa6816 ↗
2. A full tungsten divertor for ITER: physics issues and design status10.1016/j.jnucmat.2013.01.008 ↗
3. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
4. Methods for improving ductility of tungsten - a review10.1016/j.ijrmhm.2018.04.012 ↗
5. Ductility enhancement of tungsten after plastic deformation10.1016/j.jallcom.2019.02.097 ↗
6. The role of tungsten phases formation during tungsten metal powder consolidation by FAST: implications for high-temperature applications10.1016/j.matchar.2018.02.022 ↗
7. Fabrication of tungsten & tungsten alloy and its high heat load testing for fusion applications10.1016/j.matpr.2016.09.020 ↗
8. Crack suppression via in-situ oxidation in additively manufactured W-Ta alloy
9. Suppressing pore-boundary separation during spark plasma sintering of tungsten10.1016/j.jnucmat.2013.03.042 ↗
10. A new fully automatic PIM tool to replicate two component tungsten DEMO divertor parts10.1016/j.fusengdes.2013.04.037 ↗
11. Formation of nanocrystalline tungsten by selective laser melting of tungsten powder10.1080/10426914.2012.663119 ↗
12. Controlling interdependent meso-nanosecond dynamics and defect generation in metal 3D printing10.1126/science.aay7830 ↗
13. Additive manufacturing (3D printing): a review of materials, methods, applications and challenges10.1016/j.compositesb.2018.02.012 ↗
14. Selective laser melting of tungsten carbide reinforced maraging steel composite
15. Laser direct manufacturing of tungsten nickel collimation component10.1016/j.jmatprotec.2003.12.009 ↗
16. Rapid additive manufacturing of MR compatible multipinhole collimators with selective laser melting of tungsten powder10.1118/1.4769122 ↗
17. Cracking in laser additively manufactured W: initiation mechanism and a suppression approach by alloying10.1016/j.matdes.2018.12.010 ↗
18. Crack suppression in additively manufactured tungsten by introducing secondary-phase nanoparticles into the matrix10.1016/j.ijrmhm.2018.11.013 ↗
19. Microstructural characteristics and crack formation in additively manufactured bimetal material of 316L stainless steel and Inconel 625
20. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
21. Methods for improving ductility of tungsten - A review10.1016/j.ijrmhm.2018.04.012 ↗
22. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
23. Oxide dispersion strengthened stainless steel 316L with superior strength and ductility by selective laser melting10.1016/j.jmst.2019.11.004 ↗
24. Selective laser melting of austenitic oxide dispersion strengthened steel: processing, microstructural evolution and strengthening mechanisms10.1016/j.msea.2020.139532 ↗
25. In-situ irradiation tolerance investigation of high strength ultrafine tungsten-titanium carbide alloy10.1016/j.actamat.2018.10.038 ↗
26. Microstructure and thermal properties of mechanically alloyed W-1%TiC powder consolidated via two-step HIPping10.1016/j.fusengdes.2017.11.010 ↗
27. Densification behavior, microstructural evolution, and mechanical properties of TiC/316L stainless steel nanocomposites fabricated by selective laser melting10.1016/j.matdes.2017.10.039 ↗
28. Microstructure, solidification behavior and mechanical properties of Al-Si-Mg-Ti/TiC fabricated by selective laser melting
29. Improvement of high temperature oxidation resistance of additively manufactured TiC/Inconel 625 nanocomposites by laser shock peening treatment
30. Preparation and characteristics of W–1 wt.% TiC alloy via a novel chemical method and spark plasma sintering10.1016/j.powtec.2014.12.033 ↗
31. Surface damages of polycrystalline W and La2O3-doped W induced by high-flux He plasma irradiation10.1016/j.jnucmat.2018.01.047 ↗
32. Microstructure and texture in W and W-1wt%La2O3 processed by high-pressure torsion10.1016/j.scriptamat.2017.06.008 ↗
33. Promoting the heterogeneous nucleation and the functional properties of directed energy deposited NiTi alloy by addition of La2O3
34. Controlled synthesis of high-quality W-Y2O3 composite powder precursor by ascertaining the synthesis mechanism behind the wet chemical method10.1016/j.jmst.2019.05.067 ↗
35. W–Y2O3 composite nanopowders prepared by hydrothermal synthesis method: co-deposition mechanism and low temperature sintering characteristics10.1016/j.jallcom.2019.153461 ↗
36. Synthesis of nanosized composite powders via a wet chemical process for sintering high performance W-Y2O3 alloy10.1016/j.ijrmhm.2017.09.001 ↗
37. Synthesis of W-Y2O3 alloys by freeze-drying and subsequent low temperature sintering: Microstructure refinement and second phase particles regulation10.1016/j.jmst.2019.08.010 ↗
38. Influence of yttrium addition on the reduction property of tungsten oxide prepared via wet chemical method10.1007/s40195-019-00975-3 ↗
39. Mechanical properties and microstructural change of W–Y2O3 alloy under helium irradiation10.1038/srep12755 ↗
40. The synthesis of composite powder precursors via chemical processes for the sintering of oxide dispersion-strengthened alloys10.1039/C9QM00422J ↗
41. Cohesion properties of W-ZrC interfaces from first principles calculation10.1016/j.jallcom.2018.07.238 ↗
42. Extraordinary high ductility/strength of the interface designed bulk W-ZrC alloy plate at relatively low temperature10.1038/srep16014 ↗
43. Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys10.1016/j.ijrmhm.2015.03.019 ↗
44. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
45. In-situ formation of novel TiC-particle-reinforced 316L stainless steel bulk-form composites by selective laser melting10.1016/j.jallcom.2017.01.149 ↗
46. Molybdenum and tungsten manufactured by selective laser melting: Analysis of defect structure and solidification mechanisms10.1016/j.ijrmhm.2019.104999 ↗
47. Influence of impurities on the fracture behaviour of tungsten10.1080/14786435.2011.558861 ↗
48. The influence of carbon and oxygen in the grain boundary on the brittle-ductile transition temperature of tungsten Bi-crystals10.1016/0036-9748(84)90318-1 ↗
49. Inherent strength of grain boundaries in tungsten10.1103/PhysRevB.83.134115 ↗
50. Effect of processing parameters on the densification, microstructure and crystallographic texture during the laser powder bed fusion of pure tungsten10.1016/j.ijrmhm.2018.10.004 ↗
51. Selective laser melting of tungsten and tungsten alloys10.1016/j.ijrmhm.2017.12.005 ↗