Quasi-static and fatigue properties of graded Ti–6Al–4V lattices produced by Laser Powder Bed Fusion (LPBF)
Source abstract
Abstract
The additive manufacturing of metallic lattices based on triply periodic minimal surfaces (TPMS) has recently received plenty of interest in the field of hard tissue engineering. Although these structures are deemed to present advantages over conventional designs in regard to their biological and compressive mechanical properties, their fatigue life has received little attention. In the following work, Ti–6Al–4V lattices based on gyroid, diamond and Schwartz primitive unit-cells were tested in quasi-static tension and tension-tension cyclic fatigue. Their resulting elastic and fatigue properties are reported and compared in the context of biomedical applications. Compared to the two others, the Schwartz lattices were found to have the lowest strength for a similar relative density. The Young's moduli of the three samples however, were of similar magnitude. Basquin's functions are presented to fit the fatigue S–N curves and these can assist with the fatigue design of lattices with identical unit-cells. Fractography analysis from scanning electron microscopy images revealed that the fatigue crack initiation always occurs at the surface, pointing out the importance of surface treatment in SLM-produced titanium lattices.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Bone Tissue Engineering Materials · Cellular and Composite Structures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Finite element analysis of porous commercially pure titanium for biomedical implant application10.1016/j.msea.2018.04.009 ↗
2. Additively manufactured metallic porous biomaterials based on minimal surfaces: a unique combination of topological, mechanical, and mass transport properties10.1016/j.actbio.2017.02.024 ↗
3. Investigation of the structure and mechanical properties of additively manufactured Ti-6Al-4V biomedical scaffolds designed with a Schwartz primitive unit-cell
4. Additive manufacturing and mechanical characterization of graded porosity scaffolds designed based on triply periodic minimal surface architectures10.1016/j.jmbbm.2016.05.027 ↗
5. Minimal surface scaffold designs for tissue engineering10.1016/j.biomaterials.2011.06.012 ↗
6. Additive manufacturing technology for porous metal implant applications and triple minimal surface structures: a review
7. Topology-mechanical property relationship of 3D printed strut, skeletal, and sheet based periodic metallic cellular materials
8. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
9. Ti–6Al–4V triply periodic minimal surface structures for bone implants fabricated via selective laser melting10.1016/j.jmbbm.2015.06.024 ↗
10. Gyroid porous titanium structures: a versatile solution to be used as scaffolds in bone defect reconstruction10.1016/j.matdes.2017.11.050 ↗
11. The very high cycle fatigue behaviour of Ti-6Al-4V alloy10.12693/APhysPolA.128.497 ↗
12. Fatigue properties of SLM-produced Ti6Al4V with various post-processing processes
13. Numerical modelling of surface roughness effect on the fatigue behavior of Ti-6Al-4V obtained by additive manufacturing10.1016/j.ijfatigue.2019.02.014 ↗
14. Surface roughness of Ti-6Al-4V parts obtained by SLM and EBM: effect on the high cycle fatigue life10.1016/j.proeng.2018.02.010 ↗
15. Fatigue life of additively manufactured Ti6Al4V scaffolds under tension-tension, tension-compression and compression-compression fatigue load10.1038/s41598-018-23414-2 ↗
16. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
17. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
18. Fatigue behavior of As-built selective laser melted titanium scaffolds with sheet-based gyroid microarchitecture for bone tissue engineering10.1016/j.actbio.2019.05.046 ↗
19. Relationship between unit cell type and porosity and the fatigue behavior of selective laser melted meta-biomaterials10.1016/j.jmbbm.2014.12.015 ↗
20. Fracture toughness and tensile strength of 316L stainless steel cellular lattice structures manufactured using the selective laser melting technique10.1016/j.msea.2016.05.075 ↗
21. Mechanical properties and in vitro behavior of additively manufactured and functionally graded Ti6Al4V porous scaffolds10.3390/met8040200 ↗
22. Mechanical and in vitro study of an isotropic Ti6Al4V lattice structure fabricated using selective laser melting10.1016/j.jallcom.2018.12.220 ↗
23. Selective laser melting of lattice structures: a statistical approach to manufacturability and mechanical behavior10.1016/j.rcim.2017.06.006 ↗
24. Young’s modulus of trabecular and cortical bone material: ultrasonic and microtensile measurements10.1016/0021-9290(93)90042-D ↗
25. Mathematically defined tissue engineering scaffold architectures prepared by stereolithography10.1016/j.biomaterials.2010.05.068 ↗
26. Lamit · 2015
27. Investigation of accuracy and dimensional limits of part produced in aluminum alloy by selective laser melting10.1007/s00170-016-8788-9 ↗
28. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
29. Surface and morphological modification of selectively laser melted titanium lattices using a chemical post treatment10.1016/j.surfcoat.2020.125794 ↗
30. Effect of large hydrostatic pressures on the torsional fatigue strength of two steels10.1243/JMES_JOUR_1964_006_042_02 ↗
31. Recent research and development in titanium alloys for biomedical applications and healthcare goods10.1016/j.stam.2003.09.002 ↗
32. Insights into the mechanical properties of several triply periodic minimal surface lattice structures made by polymer additive manufacturing10.1016/j.polymer.2017.11.049 ↗
33. Influence of hydrogen content on tensile and compressive properties of Ti–6Al–4V alloy at room temperature10.1016/j.msea.2010.03.052 ↗
34. PM versus IM Ti-5Al-5V–5Mo-3Cr alloy in mechanical properties and fracture behaviour10.1590/1980-5373-mr-2018-0739 ↗
35. In-situ investigation of stress-induced martensitic transformation in Ti–Nb binary alloys with low Young’s modulus10.1016/j.msea.2015.11.005 ↗
36. The rate dependent response of a titanium alloy subjected to quasi-static loading in ambient environment10.1023/A:1021085026220 ↗
37. M.M. Rahman, L.A. Hof, B. Johnston, S.A. Khanoki, D. Pasini, R. Wüthrich, Electro-polishing of additive manufactured porous titanium for medical implants, in: Meeting Abstracts, 2015, pp. 1247–1247.10.1149/MA2015-01/17/1247 ↗
38. Improved fatigue endurance ratio of additive manufactured Ti-6Al-4V lattice by hot isostatic pressing10.1016/j.matdes.2017.08.048 ↗
39. Ellyin · 2012
40. H.A. Stoffregen, K. Butterweck, E. Abele, Fatigue analysis in selective laser melting: review and investigation of thin-walled actuator housings, in: Proceedings of the 25th Solid Freeform Fabrication Symposium, 2014, pp. 635–650.
41. A comparison of Ti-6Al-4V in-situ alloying in Selective Laser Melting using simply-mixed and satellited powder blend feedstocks10.1016/j.matchar.2018.05.039 ↗
42. Mapping the tray of electron beam melting of Ti-6Al-4V: properties and microstructure10.3390/ma12091470 ↗
43. Fatigue and biological properties of Ti-6Al-4V ELI cellular structures with variously arranged cubic cells made by selective laser melting10.1016/j.jmbbm.2017.11.044 ↗
44. The anisotropic elastic behavior of the widely-used triply-periodic minimal surface based scaffolds10.1016/j.jmbbm.2019.07.012 ↗
45. Determination of the effective elastic properties of titanium lattice structures
46. Fatigue performance of selective laser melted Ti6Al4V components: state of the art10.1088/2053-1591/aae10e ↗
47. Analysis of fracture toughness and crack propagation of Ti6Al4V produced by selective laser melting10.1002/adem.201100233 ↗
48. Fatigue design with additive manufactured metals: issues to consider and perspective for future research10.1016/j.proeng.2018.02.002 ↗
49. On the effect of geometrical imperfections and defects on the fatigue strength of cellular lattice structures additively manufactured via Selective Laser Melting10.1016/j.ijfatigue.2019.03.019 ↗
50. Advanced fatigue analysis of metal lattice structures produced by Selective Laser Melting10.1016/j.cirp.2017.04.130 ↗
51. Fatigue performances of chemically etched thin struts built by selective electron beam melting: experiments and predictions10.1016/j.mtla.2020.100589 ↗