Microstructure and mechanical behavior of PH 13–8Mo martensitic stainless steel fabricated by wire arc additive manufacturing
Source abstract
Abstract
Abstract Wire arc additive manufacturing (WAAM) was applied to fabricate precipitation hardened (PH) 13–8Mo martensitic stainless steel parts for applications in injection molding equipment, aerospace components, and marine. The microstructural features, microhardness evaluation, and room temperature tensile properties of the as-printed parts have been comprehensively investigated at different locations and orientations. The experimental results showed that the predominant microstructure of the WAAM fabricated PH 13–8Mo stainless steel part mainly consists of vermicular and lathy remnant δ-ferrite embedded in a low-carbon fine martensitic matrix in addition to a small fraction of retained austenite. The content of both retained austenite and remnant δ-ferrite reduced through the building direction of the WAAM fabricated wall, causing a gradual increase of microhardness and ultimate tensile strength values from the bottom to the top of the component. Moreover, the measured tensile strength and ductility in horizontal and vertical directions of the wall revealed anisotropic mechanical properties associated with the columnar growth of primary δ-ferrite grains structure formed during the solidification of the material, creating a strong cubic texture along the building direction. The present study, for the first time, revealed successful implementation of WAAM technology to fabricate PH 13–8Mo stainless steel parts with comparable hardness and tensile strength with respect to other fabrication methods.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (76)
Show source-provided references
1. Wire + arc additive manufacture of 17-4 PH stainless steel: effect of different processing conditions on microstructure, hardness, and tensile strength10.1016/j.jmatprotec.2019.01.007 ↗
2. Effect of solidification defects and HAZ softening on the anisotropic mechanical properties of a wire arc additive-manufactured low-carbon low-alloy steel part10.1007/s11837-019-03773-5 ↗
3. J. Xiong, G. Zhang, W. Zhang, Forming appearance analysis in multi-layer single-pass GMAW-based additive manufacturing, 2015: 1767–1776. https://doi.org/10.1007/s00170–015-7112–4.10.1007/s00170-015-7112-4 ↗
4. A multi-bead overlapping model for robotic wire and arc additive manufacturing (WAAM)10.1016/j.rcim.2014.08.008 ↗
5. A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement10.1016/j.jmapro.2018.08.001 ↗
6. Microstructural evolution and mechanical properties of a low-carbon low-alloy steel produced by wire arc additive manufacturing10.1007/s00170-019-04393-8 ↗
7. Interfacial bonding between a wire arc additive manufactured 420 martensitic stainless steel part and its wrought base plate10.1016/j.matchemphys.2020.123199 ↗
8. Current status and perspectives on wire and arc additive manufacturing (WAAM)
9. Heat propagation of circular thin-walled parts fabricated in additive manufacturing using gas metal arc welding10.1016/j.jmatprotec.2017.08.007 ↗
10. On the Post-Printing Heat Treatment of a Wire Arc Additively Manufactured ER70S Part10.3390/ma13122795 ↗
11. Comparison of microstructural characteristics and mechanical properties of shipbuilding steel plates fabricated by conventional rolling versus wire arc additive manufacturing
12. Additive manufacturing of Ti-6Al-4V components by shaped metal deposition: microstructure and mechanical properties10.1016/j.matdes.2009.11.032 ↗
13. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
14. Microstructure and mechanical properties of 9Cr martensitic heat-resistant steel fabricated by wire and arc additive manufacture technology10.1166/mex.2019.1485 ↗
15. Wire and arc additive manufactured steel: Tensile and wear properties
16. Parameters effect on SS304 beads deposited by wire arc additive manufacturing10.1080/10426914.2020.1743852 ↗
17. Microstructure and mechanical properties of the austenitic stainless steel 316L fabricated by gas metal arc additive manufacturing10.1016/j.msea.2017.05.024 ↗
18. Correlation between arc mode, microstructure, and mechanical properties during wire arc additive manufacturing of 316L stainless steel10.1016/j.msea.2019.02.078 ↗
19. Microstructure characterization of SS308LSi components manufactured by GTAW-based additive manufacturing: shaped metal deposition using pulsed current arc10.1007/s00170-016-9053-y ↗
20. Wire-arc additive manufacturing of a duplex stainless steel: thermal cycle analysis and microstructure characterization10.1007/s40194-019-00735-y ↗
21. Thermal modeling and characterization of wire arc additive manufactured duplex stainless steel10.1016/j.jmatprotec.2019.05.003 ↗
22. Microstructure and mechanical properties of TOP-TIG-wire and arc additive manufactured super duplex stainless steel (ER2594)10.1016/j.msea.2019.138097 ↗
23. Characterization of wire arc additive manufacturing 2Cr13 part: process stability, microstructural evolution, and tensile properties10.1016/j.jallcom.2018.03.222 ↗
24. Microstructure and Mechanical Properties of AISI 420 Stainless Steel Produced by Wire Arc Additive Manufacturing, in: TMS 2020 149th Annu
25. Weld microstructure development and properties of precipitation-strengthened martensitic stainless steels
26. J.C. Lippold, D.J. Kotecki, Precipitation-hardening stainless steels, in: Weld. Metall. Weldability Stainl. Steels, New Jersey, 2005: pp. 264–286.
27. Laser powder bed fusion of precipitation-hardened martensitic stainless steels: a review10.3390/met10020255 ↗
28. Metallurgical and hydrogen effects on the small punch tested mechanical properties of PH-13-8Mo stainless steel10.3390/ma11101966 ↗
29. Microstructural evolution and mechanical properties of simulated heat-affected zones in cast precipitation-hardened stainless steels 17-4 and 13-8+Mo10.1007/s11661-016-3851-6 ↗
30. Microstructural evolution in 13Cr-8Ni-2.5Mo-2Al martensitic precipitation-hardened stainless steel10.1016/j.msea.2004.12.002 ↗
31. Singh · 2016
32. Metallography and microstructures of stainless steels and maraging steels
33. Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel10.1016/j.msea.2018.10.086 ↗
34. R.J. Hamlin, Microstructural Evolution and Mechanical Properties of Simulated Microstructural Evolution and Mechanical Properties of Simulated Heat Affected Zones in Cast Precipitation Hardened Stainless Heat Affected Zones in Cast Precipitation Hardened Stainless Ste, (2015: 〈https://preserve.lehigh.edu/etd/2625〉.
35. Effect of aging treatment on hydrogen embrittlement of PH 13-8 Mo martensite stainless steel10.1016/j.msea.2015.09.116 ↗
36. Tandem metal inert gas process for high productivity wire arc additive manufacturing in stainless steel
37. Experimental investigation on selective laser melting of 17-4PH stainless steel10.1016/j.optlastec.2016.07.012 ↗
38. Experimental design approach to optimize selective laser melting of martensitic 17-4 PH powder: Part i − single laser tracks and first layer10.1108/13552541211193476 ↗
39. Microstructure, post thermal treatment response, and tribological properties of 3D printed 17-4 PH stainless steel
40. Microstructures and properties of 17-4 PH stainless steel fabricated by selective laser melting10.1016/S2238-7854(12)70029-7 ↗
41. The effects of fabrication atmosphere condition on the microstructural and mechanical properties of laser direct manufactured stainless steel 17-4 PH10.1016/j.jmst.2019.03.009 ↗
42. Additive manufacturing of 17-4 PH stainless steel: post-processing heat treatment to achieve uniform reproducible microstructure10.1007/s11837-015-1754-4 ↗
43. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
44. Fatigue behavior of additively manufactured 17-4 PH stainless steel: synergistic effects of surface roughness and heat treatment10.1016/j.ijfatigue.2019.02.039 ↗
45. Effect of retained austenite on subsequent thermal processing and resultant mechanical properties of selective laser melted 17–4 PH stainless steel10.1016/j.matdes.2015.05.026 ↗
46. Effect of heat treatments on microstructural evolution of additively manufactured and wrought 17-4PH stainless steel10.1016/j.matdes.2018.07.015 ↗
47. Effects of heat treatment and build orientations on the fatigue life of selective laser melted 15-5 PH stainless steel10.1016/j.msea.2019.04.003 ↗
48. Improving the surface quality and mechanical properties by shot-peening of 17-4 stainless steel fabricated by additive manufacturing10.1016/j.matdes.2016.08.037 ↗
49. Integration of heat treatment with shot peening of 17-4 stainless steel fabricated by direct metal laser sintering10.1007/s11837-017-2538-9 ↗
50. Microstructure and mechanical properties of stainless steel CX manufactured by Direct Metal Laser Sintering10.1016/j.msea.2017.10.045 ↗
51. Study of mechanical properties of AISI 316 stainless steel processed by “selective laser melting”, following different manufacturing strategies10.1007/s00170-010-2631-5 ↗
52. Microstructure and corrosion behavior of a novel additively manufactured maraging stainless steel10.1016/j.electacta.2020.135925 ↗
53. Wire-feed additive manufacturing of metal components: technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
54. U.S. Welding Corporation, Technical Data Sheets & Safety Data Sheets – Iron Base Alloys, n.d.: 〈https://www.usweldingcorp.net/technical-data/tds-sds-iron-base-alloys/〉 (accessed 1 September 2020).
55. Effects of post-printing heat treatment on the microstructure and mechanical properties of a wire arc additive manufactured 420 martensitic stainless steel part10.1016/j.msea.2021.141167 ↗
56. A. American Society for Testing and Materials, E8M Standard Test Methods for Tension Testing of Metallic Materials, ASTM International, West Conshohocken, PA, 2008: https://doi.org/10.1520/E0008_E0008M-13A.10.1520/E0008_E0008M-13A ↗
57. Welding and weldability of the ‘super-austenitic’ and ‘super-martensitic’ stainless steels10.1533/wint.2003.3149 ↗
58. Forming process, microstructure, and mechanical properties of thin-walled 316L stainless steel using speed-cold-welding additive manufacturing10.3390/met9010109 ↗
59. S. Kou, Welding metallurgy, second ed., Wiley-Interscience, New Jersey, 2003.10.1002/0471434027 ↗
60. Evaluation of microstructure and texture across the welded interface of super duplex stainless steel and high strength low alloy steel10.1016/j.surfcoat.2014.12.060 ↗
61. An investigation of the high-temperature and solidification microstructures of PH 13-8 Mo stainless steel10.1007/BF02646991 ↗
62. Microstructure of welded joints of X5CrNiCuNb 16-4 (17-4 PH) martensitic stainlees steel after heat treatment10.2478/amm-2014-0162 ↗
63. Influence of Creq/Nieq ratio on solidification structures and tensile properties of strip cast austenitic stainless steels10.1080/13640461.1996.11819658 ↗
64. Orientational dependence of lathy ferrite in Fe-Cr-Ni alloy during directional solidification10.1016/j.matlet.2012.04.149 ↗
65. Effect of weld cooling rate on delta-ferrite content of austenitic weld metals10.1007/BF00721800 ↗
66. Study on microstructure and tensile properties of high nitrogen Cr-Mn steel processed by CMT wire and arc additive manufacturing10.1016/j.matdes.2019.107611 ↗
67. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels10.1016/j.matdes.2015.08.045 ↗
68. Hot-cracking mechanism in Co//2 laser beam welds of dissimilar metals involving Ph martensitic stainless steels
69. Revisiting the structure of martensite in iron-carbon steels10.2320/matertrans.MRA2007338 ↗
70. The effects of heat-treatment parameters on corrosion resistance and phase transformations of 14Cr-3Mo martensitic stainless steel10.1016/j.msea.2006.03.134 ↗
71. Effect of retained austenite stabilized via quench and partitioning on the strain hardening of martensitic steels10.1007/s11661-008-9609-z ↗
72. Effect of interpass temperature on the formation of retained austenite in a wire arc additive manufactured ER420 martensitic stainless steel10.1016/j.matchemphys.2021.124555 ↗
73. Additive manufacturing of an Fe–Cr–Ni–Al maraging stainless steel: microstructure evolution, heat treatment, and strengthening mechanisms10.1016/j.msea.2020.139470 ↗
74. Effect of delta ferrite on impact properties of low carbon 13Cr–4Ni martensitic stainless steel10.1016/j.msea.2010.01.085 ↗
75. Effect of trace lanthanum hexaboride and boron additions on microstructure, tensile properties and anisotropy of Ti-6Al-4V produced by additive manufacturing10.1016/j.msea.2018.02.012 ↗
76. Trace carbon addition to refine microstructure and enhance properties of additive-manufactured Ti-6Al-4V10.1007/s11837-018-2994-x ↗