journal article·2018-12

Standardized X-ray tomography testing of additively manufactured parts: A round robin test

Anton du Plessis, Stephan G. le Roux

Publisher page

Abstract

Abstract Micro computed tomography (microCT) allows non-destructive insights into the quality of additively manufactured parts and the processes that produce them. MicroCT has been used widely in this industry but the use of this technique is often time consuming and costly which reduces its potential impact and the benefits associated with its use. By using standardized test procedures, the analysis time and cost can be minimized and confidence in obtained results increased. A round robin test was conducted as follows: a series of standard test procedures (part sizes and shapes and test protocols) were applied – using one microCT system – to identical parts produced on a variety of metal additive manufacturing systems (specifically laser powder bed fusion systems). These are simple parts: a 10 mm cube, a 15 mm diameter vertical-built cylinder and a basic topology optimized example part – a bracket. The 15 mm diameter cylinder acts as witness specimen for the build of the complex part. All these were produced in Ti6Al4V, and in some cases parts were provided with variations in process parameters or manufacturing conditions which led to different types of intentional manufacturing flaws or defects. Various intentional and unintentional flaws were identified and quantified. The major result shown is that the analysis of a simple 10 mm cube clearly identifies incorrect process parameters even for very low levels of porosity, with unique porosity distributions and characteristics. It is found that generally this porosity extends to larger, more complex parts. The witness specimen (15 mm cylinder) allows clear identification of layered stop-start flaws, at a resolution better than a complex part built alongside it, allowing to identify defective builds. The results indicate a successful first step at standardized microCT analysis procedures for improvement of processes and quality control in additive manufacturing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Advanced X-ray and CT Imaging · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Laser based additive manufacturing in industry and academia10.1016/j.cirp.2017.05.011 ↗
2. Additive manufacturing of metallic components—process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. Qualification of Ti6Al4V ELI alloy produced by laser powder bed fusion for biomedical applications10.1007/s11837-017-2655-5 ↗
4. Additive manufacturing and postprocessing of Ti-6Al-4V for superior mechanical properties10.1557/mrs.2016.215 ↗
5. Overview of materials qualification needs for metal additive manufacturing10.1007/s11837-015-1810-0 ↗
6. Progress towards metal additive manufacturing standardization to support qualification and certification10.1007/s11837-017-2265-2 ↗
7. Applications of non-destructive testing techniques for post-process control of additively manufactured parts10.1080/17452759.2017.1357319 ↗
8. Porosity measurements and analysis for metal additive manufacturing process control10.6028/jres.119.019 ↗
9. X-ray microcomputed tomography in additive manufacturing: a review of the current technology and applications
10. X-ray computed tomography of consumer-grade 3D-printed parts10.1089/3dp.2015.0015 ↗
11. Quality investigation of 3D printer filament using laboratory X-ray tomography10.1089/3dp.2016.0011 ↗
12. Characterization of mechanical properties and fracture mode of additively manufactured carbon fiber and glass fiber reinforced thermoplastics10.1016/j.matdes.2017.10.021 ↗
13. Development of bendable strain sensor with embedded microchannels using 3D printing10.1016/j.sna.2017.07.025 ↗
14. Quality control of a laser additive manufactured medical implant by X-Ray tomography10.1089/3dp.2016.0012 ↗
15. ASTM E1570-11 · 2011
16. ASTM WK56649 · 2018
17. ASTM WK47031 · 2018
18. du Plessis · 2018
19. du Plessis · 2018
20. du Plessis · 2018
21. du Plessis · 2018
22. du Plessis · 2018
23. Surface roughness and morphology customization of additive manufactured open porous Ti6Al4V structures10.3390/ma6104737 ↗
24. High-resolution microfocus X-ray computed tomography for 3D surface roughness measurements of additive manufactured porous materials10.1002/adem.201200156 ↗
25. Topography of selectively laser melted surfaces: a comparison of different measurement methods10.1016/j.cirp.2017.04.075 ↗
26. Internal surface measurement of metal powder bed fusion parts
27. High resolution pore size analysis in metallic powders by X-ray tomography10.1016/j.csndt.2016.09.002 ↗
28. Size and shape determination of sub-millimeter sized abrasive particles with X-ray computed tomography
29. Additive manufacturing powder feedstock characterization using X-ray tomography10.1016/j.mprp.2018.01.002 ↗
30. Laboratory x-ray micro-computed tomography: a user guideline for biological samples10.1093/gigascience/gix027 ↗
31. The CT scanner facility at Stellenbosch University: an open access X-ray computed tomography laboratory10.1016/j.nimb.2016.08.005 ↗
32. An interlaboratory comparison of X-ray computed tomography measurement for texture and dimensional characterisation of additively manufactured parts
33. A. Thompson, S. Tammas-williams, N. Senin, I. Todd, M.M. Team, Correlating Volume and Surface Features in Additively Manufactured Metal Parts 1 Manufacturing Metrology Team, Faculty of Engineering, 2 Manufacture using Advanced Powder Processes (MAPP), ePrints Nottingham (2018) 1–5.