Effect of crack-like defects on the fracture behaviour of Wire + Arc Additively Manufactured nickel-base Alloy 718
Source abstract
Abstract
The fabrication of large components using a high deposition rate, near-net shape process like Wire + Arc Additive Manufacturing (WAAM) is a promising option for many industries, due to the potential for reduction in material wastage and shorter lead times in comparison to conventional methods. Specialist materials like nickel-base superalloys, which are typically used in high temperature and corrosive environments, are particularly attractive options due to their high raw material costs. Although nickel-base Alloy 718 seems well suited to the process due to its good weldability, process-induced defects can arise from unfavourable deposition conditions and elimination of these defects may not always be possible. In WAAM Alloy 718 deposited under such conditions, crack-like defects with planar morphology and hot cracking characteristics were observed. These defects were observable using conventional non-destructive testing techniques and displayed directionality relating to the deposition path. The fracture behaviour of WAAM Alloy 718 containing these defects was “semi-stable” – a mixture of fracture instability and stable crack extension. The apparent fracture toughness of WAAM Alloy 718 containing these defects was found to be anisotropic, which can be attributed to the interaction of the notched crack with pre-existing defects. WAAM Alloy 718 displayed an apparent fracture toughness comparable to that of wrought Alloy 718 when notched perpendicular to the defects; but only half that of wrought when notched parallel to the defects. Therefore, careful consideration of defect orientation and their effects on mechanical properties is important in assessing the fitness-for-service of WAAM Alloy 718.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
2. Wire and arc additive manufactured steel: Tensile and wear properties
3. Tandem metal inert gas process for high productivity wire arc additive manufacturing in stainless steel
4. Microstructural evolution and mechanical properties of maraging steel produced by wire + arc additive manufacture process10.1016/j.matchar.2017.12.002 ↗
5. Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy10.1007/s00170-014-6346-x ↗
6. Additive manufacturing using WAAM with AA5183 wire10.1016/j.jmatprotec.2018.04.014 ↗
7. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components10.1016/j.scriptamat.2016.10.031 ↗
8. Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
9. Morphology investigation on direct current pulsed gas tungsten arc welded additive layer manufactured Ti6Al4V alloy10.1007/s00170-011-3299-1 ↗
10. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1007/s11661-012-1444-6 ↗
11. Investigation of the benefits of plasma deposition for the additive layer manufacture of Ti-6Al-4V10.1016/j.jmatprotec.2012.02.002 ↗
12. Manufacturing of Ti-6Al-4V components by shaped metal deposition: Microstructure and mechanical properties
13. Shaped metal deposition of a nickel alloy for aero engine applications10.1016/j.jmatprotec.2007.10.051 ↗
14. Microstructural characterization of a polycrystalline nickel-based superalloy processed via tungsten-inert-gas-shaped metal deposition10.1007/s11663-010-9410-4 ↗
15. Mechanical properties of INCONEL 718 parts manufactured by shaped metal deposition (SMD)10.1007/s11665-011-0009-y ↗
16. Microstructural Analyses of ATI 718Plus® Produced by Wire-ARC Additive Manufacturing Process10.1007/s11661-017-4162-2 ↗
17. Investigation of process factors affecting mechanical properties of INCONEL 718 superalloy in wire + arc additive manufacture process10.1016/j.jmatprotec.2018.10.023 ↗
18. Precipitation-Strengthened Ni-base Alloys
19. Donachie · 2002
20. Wire + Arc Additively Manufactured Inconel 718: Effect of post-deposition heat treatments on microstructure and tensile properties10.1016/j.matdes.2019.108157 ↗
21. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
22. A review of mechanical properties of additively manufactured Inconel 71810.1016/j.addma.2019.100877 ↗
23. The influence of pulsed laser powder bed fusion process parameters on Inconel 718 material properties10.1016/j.msea.2019.138527 ↗
24. Microstructure and mechanical properties of nickel based superalloy IN718 produced by rapid prototyping with electron beam melting (EBM)10.1179/026708309X12468927349451 ↗
25. Metal Additive Manufacturing: A Review of Mechanical Properties10.1146/annurev-matsci-070115-032024 ↗
26. Fracture toughness and fatigue crack growth rate properties in wire + arc additive manufactured Ti-6Al-4V10.1111/ffe.12547 ↗
27. Analysis of fracture toughness properties of wire + arc additive manufactured high strength low alloy structural steel components
28. On the toughness scatter in low alloy C-Mn steel samples fabricated using wire arc additive manufacturing10.1016/j.msea.2017.11.101 ↗
29. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy10.1016/j.jallcom.2014.06.172 ↗
30. Effects of HIP on microstructural heterogeneity, defect distribution and mechanical properties of additively manufactured EBM Ti-48Al-2Cr-2Nb10.1016/j.jallcom.2017.09.163 ↗
31. Enhancing mechanical properties of wire + arc additively manufactured INCONEL 718 superalloy through in-process thermomechanical processing10.1016/j.matdes.2018.10.038 ↗
32. SAE International · 2018
33. SAE International · 2016
34. Post-processing of the full matrix of ultrasonic transmit-receive array data for non-destructive evaluation10.1016/j.ndteint.2005.04.002 ↗
35. ASTM International · 2018
36. ISO · 2016
37. NACE International · 2015
38. Specific aspects on crack advance during J-test method for structural materials at cryogenic temperatures10.1111/j.1460-2695.2006.00963.x ↗
39. Evaluation and interpretation of ductile crack extension in SENT specimens using unloading compliance technique10.1016/j.engfracmech.2013.11.004 ↗
40. JIc Data Analysis Methods with a ‘Negative Crack Growth’ Correction Procedure10.1520/JTE12488J ↗
41. Solidification cracking of superalloy single- and bi-crystals10.1016/j.actamat.2004.03.047 ↗
42. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
43. Launey · 1999
44. The conflicts between strength and toughness10.1038/nmat3115 ↗
45. Mechanisms of fatigue crack propagation in metals, ceramics and composites: Role of crack tip shielding10.1016/0025-5416(88)90547-2 ↗
46. Verification and validation of a rapid heat transfer calculation methodology for transient melt pool solidification conditions in powder bed metal additive manufacturing
47. Development of residual stress in parts fabricated via selective laser melting (SLM) technique under different scanning strategies10.2514/6.2018-0090 ↗
48. The relationship between carbon content, microstructure, and intergranular liquation cracking in cast nickel alloy 718,” Metall
49. Microstructural Evolution in the HAZ of Inconel 718 and Correlation with the Hot Ductility Test
50. Non-destructive testing application of radiography and ultrasound for wire and arc additive manufacturing
51. Controlling hot cracking in Ni-based Inconel-718 superalloy cast sheets during tungsten inert gas welding10.1016/j.jmatprotec.2015.03.031 ↗
52. Influence of Interpass Temperature on Wire Arc Additive Manufacturing (WAAM) of Aluminium Alloy Components10.1051/matecconf/201926905001 ↗
53. Invited review article: Strategies and processes for high quality wire arc additive manufacturing10.1016/j.addma.2018.06.020 ↗
54. Revisiting fundamental welding concepts to improve additive manufacturing: From theory to practice10.1016/j.pmatsci.2019.100590 ↗
55. Microstructural evolution and mechanical properties of Ti-6Al-4V wall deposited by pulsed plasma arc additive manufacturing10.1016/j.matdes.2016.04.018 ↗
56. Reducing arc heat input and obtaining equiaxed grains by hot-wire method during arc additive manufacturing titanium alloy10.1016/j.msea.2018.11.022 ↗
57. Heat accumulation prevention in Wire-Arc-Additive-Manufacturing using air jet impingement10.1016/j.mfglet.2018.06.004 ↗
58. Van Der Aa · 2007
59. Open-source wire and arc additive manufacturing system: formability, microstructures, and mechanical properties10.1007/s00170-017-0636-z ↗
60. Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling10.1016/j.jallcom.2016.01.250 ↗
61. The effects of forced interpass cooling on the material properties of wire arc additively manufactured Ti6Al4V alloy10.1016/j.jmatprotec.2018.03.024 ↗
62. Mitigation of thermal distortion in wire arc additively manufactured Ti6Al4V part using active interpass cooling10.1080/13621718.2019.1580439 ↗
63. Mitigation of hot cracking in Inconel 718 superalloy by ultrasonic vibration during gas tungsten arc welding10.1016/j.jallcom.2017.12.295 ↗
64. Reduction of ductility-dip cracking susceptibility by ultrasonic-assisted GTAW10.1016/j.jmatprotec.2016.08.018 ↗
65. Influence of Mechanical Arc Oscillation on the Microstructural and Mechanical Properties of Inconel 718 Welds10.1007/s12666-019-01710-3 ↗
66. Reducing hot cracking tendency of dissimilar weld overlay by magnetic arc oscillation10.1179/1743284713Y.0000000358 ↗
67. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling10.1016/j.jmatprotec.2013.04.012 ↗
68. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
69. Investigations into effect of weld-deposition pattern on residual stress evolution for metallic additive manufacturing10.1007/s00170-016-9510-7 ↗
70. Optimization of WAAM Deposition Patterns for T-crossing Features10.1016/j.procir.2016.08.043 ↗
71. A modular path planning solution for Wire + Arc Additive Manufacturing10.1016/j.rcim.2019.05.009 ↗
72. Design for wire + Arc additive manufacture: Design rules and build orientation selection10.1080/09544828.2017.1365826 ↗
73. Thermal analysis for single-pass multi-layer GMAW based additive manufacturing using infrared thermography10.1016/j.jmatprotec.2017.01.024 ↗