Combined effect of surface anomalies and volumetric defects on fatigue assessment of AlSi7Mg fabricated via laser powder bed fusion
Source abstract
Abstract
Abstract In recent years, the fabrication of aluminum alloy parts via laser powder bed fusion has been extensively considered in the biomedical, aerospace, and other industrial sectors, as it provides advantages such as the ability to manufacture complex shapes with high performance associated with lightweight design. However, surface irregularities and sub-surface defects limit the full exploitation of such parts in fatigue-critical applications. Moreover, most of the commonly used metrological methods for surface characterization have proven to be unsuitable for determining important features such as undercuts and sub-surfaces pores. Hence, a comprehensive coupled investigation of metrological methods and cross-sectional analysis were performed in this study to evaluate the effects of surface features and volumetric defects typical of additively manufactured materials. Fatigue tests and fractographic analyses were conducted to support the finite element simulations and proposed fracture mechanics model. The results demonstrate that the standard metrological methods cannot provide all of the data needed to model the fatigue behaviors of additively manufactured materials robustly. Moreover, a statistical model describing the competition between volumetric defects and surface irregularities was developed and validated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (84)
Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Additive manufacturing of multi-material structures10.1016/j.mser.2018.04.001 ↗
4. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
5. On optimization of surface roughness of selective laser melted stainless steel parts: a statistical study10.1007/s11665-014-0993-9 ↗
6. Influences of processing parameters on surface roughness of Hastelloy X produced by selective laser melting
7. Influence of re-melting on surface roughness and porosity of AlSi10Mg parts fabricated by selective laser melting10.1016/j.jallcom.2019.04.017 ↗
8. The effect of post-processing operations on surface characteristics of 316L stainless steel produced by selective laser melting
9. Influence of process parameters on surface quality of CoCrMo produced by selective laser melting10.1007/s00170-015-7040-3 ↗
10. Finishing of internal and external surfaces produced by Powder Bed Fusion
11. Fatigue behavior of additively manufactured 17-4 PH stainless steel: synergistic effects of surface roughness and heat treatment10.1016/j.ijfatigue.2019.02.039 ↗
12. Effect of heat treatments on fatigue property of selective laser melting AlSi10Mg10.1016/j.ijfatigue.2018.07.016 ↗
13. Effect of heat treatment and laser surface remelting on AlSi10Mg alloy fabricated by selective laser melting10.1007/s00170-018-03272-y ↗
14. Effect of selective laser melting process parameters on the quality of al alloy parts: powder characterization, density, surface roughness, and dimensional accuracy10.3390/ma11122343 ↗
15. The influence of process parameters on vertical surface roughness of the AlSi10Mg parts fabricated by selective laser melting10.1016/j.jmatprotec.2018.10.015 ↗
16. Influence of shot peening on AlSi10Mg parts fabricated by additive manufacturing
17. On morphological surface features of the parts printed by selective laser melting (SLM)
18. Surface morphology in selective laser melting of metal powders10.1016/j.phpro.2011.03.034 ↗
19. Surface texture metrology for metal additive manufacturing: a review10.1016/j.precisioneng.2016.06.001 ↗
20. Physical processes linking input parameters and surface morphology in additive manufacturing
21. Experimental investigation on densification behavior and surface roughness of AlSi10Mg powders produced by selective laser melting10.1016/j.optlastec.2017.05.006 ↗
22. Top surface and side roughness of Inconel 625 parts processed using selective laser melting10.1108/13552540910943397 ↗
23. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
24. Effect of process parameters on the surface roughness of overhanging structures in laser powder bed fusion additive manufacturing10.1016/j.procir.2016.02.347 ↗
25. Machined surface integrity
26. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
27. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
28. A metrology horror story: the additive surface, in: ASPEN/ASPE Spring Top
29. Surface treatment of powder-bed fusion additive manufactured metals for improved fatigue life10.1007/s11665-018-3732-9 ↗
30. Top surface and side roughness of Inconel 625 parts processed using selective laser melting10.1108/13552540910943397 ↗
31. Surface texture measurement for additive manufacturing10.1088/2051-672X/3/2/024002 ↗
32. Application of laser Re-Melting on selective laser melting parts
33. Influence of process parameters on surface roughness of aluminum parts produced by DMLS10.1007/s00170-012-4688-9 ↗
34. Surface roughness visualisation for rapid prototyping models, CAD Comput10.1016/S0010-4485(01)00201-9 ↗
35. Analysis and optimisation of vertical surface roughness in micro selective laser melting10.1088/2051-672X/3/3/034007 ↗
36. Internal surface measurement of metal powder bed fusion parts
37. Characterization of typical surface effects in additive manufacturing with confocal microscopy10.1088/2051-672X/3/1/014001 ↗
38. Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)
39. The influence of process parameters on the surface roughness of a 3D-Printed Co–Cr dental alloy produced via selective laser melting
40. Laser polishing
41. High-resolution microfocus X-ray computed tomography for 3d surface roughness measurements of additive manufactured porous materials10.1002/adem.201200156 ↗
42. Surface roughness and morphology customization of additive manufactured open porous Ti6Al4V structures10.3390/ma6104737 ↗
43. X-ray microcomputed tomography in additive manufacturing: a review of the current technology and applications, 3D print
44. Standardized X-ray tomography testing of additively manufactured parts: a round robin test
45. J.N. Domfang Ngnekou, Y. Nadot, G. Henaff, J. Nicolai, W.H. Kan, J.M. Cairney, L. Ridosz, fatigue properties of AlSi10Mg produced by additive layer manufacturing10.1016/j.ijfatigue.2018.09.029 ↗
46. Characterization of metal additive manufacturing surfaces using synchrotron X-ray CT and micromechanical modeling10.1007/s00466-017-1531-z ↗
47. Overview on microstructure- and defect-sensitive fatigue modeling of additively manufactured materials10.1007/s11837-018-2987-9 ↗
48. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
49. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
50. Fatigue properties of AlSi10Mg obtained by additive manufacturing: defect-based modelling and prediction of fatigue strength10.1016/j.engfracmech.2017.11.002 ↗
51. Murakami · 2002
52. Defect analysis and fatigue design basis for Ni-based superalloy 718 manufactured by selective laser melting10.1016/j.ijfatigue.2018.08.002 ↗
53. Effect of build orientation on the fatigue properties of as-built Electron beam Melted Ti-6Al-4V alloy10.1016/j.ijfatigue.2018.08.006 ↗
54. A new FE post-processor for probabilistic fatigue assessment in the presence of defects and its application to AM parts10.1016/j.ijfatigue.2019.04.008 ↗
55. LCF behaviour and a comprehensive life prediction model for AlSi10Mg obtained by SLM10.1016/j.ijfatigue.2018.07.030 ↗
56. Fatigue life prediction of additively manufactured material: effects of surface roughness, defect size, and shape, Fatigue Fract
57. Fatigue life estimation of additive manufactured parts in the as-built surface condition
58. High cycle fatigue life estimation of AlSi10Mg processed by laser powder bed fusion
59. Surface roughness of Ti-6Al-4V parts obtained by SLM and EBM: effect on the high cycle fatigue life10.1016/j.proeng.2018.02.010 ↗
60. Defect analysis and fatigue design basis for Ni-based superalloy 718 manufactured by additive manufacturing10.1016/j.ijfatigue.2018.08.002 ↗
61. Quality control of AlSi10Mg produced by SLM: metallography versus CT scans for critical defect size assessment
62. Expression of additive manufacturing surface irregularities through a flaw-based assessment
63. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
64. Effect of surface roughness on fatigue performance of additive manufactured Ti-6Al-4V10.1179/1743284715Y.0000000053 ↗
65. High cycle fatigue behavior and life prediction for additively manufactured 17-4 PH stainless steel: effect of sub-surface porosity and surface roughness
66. Qualification of AM parts: extreme value statistics applied to tomographic measurements10.1016/j.matdes.2017.05.091 ↗
67. ISO 4288:1996 Geometrical Product Specifications (GPS), Surface texture: Profile method-Rules and procedures for the assessment of surface texture (ISO 4288: 1996), in: Ger. Version EN ISO, 1997. doi:10.1186/s40557-016-0111-6.10.1186/s40557-016-0111-6 ↗
68. International Organization for Standardization, ISO 25178-2: Geometrical product specifications (GPS) - Surface texture: Areal Part 2: Terms, definitions and surface texture parameters, 2007.
69. Experimental and numerical investigation on compressive fatigue strength of lattice structures of AlSi7Mg manufactured by SLM10.1016/j.ijfatigue.2019.06.041 ↗
70. Aging response of an A357 Al alloy processed by selective laser melting
71. Energy input effect on morphology and microstructure of selective laser melting single track from metallic powder, J. Mater
72. Selective laser melting of aluminium components, J. Mater
73. Leach · Characterisation of areal surface texture · 201310.1007/978-3-642-36458-7 ↗
74. ASTM E2283 - 08(2014), Standard Practice for Extreme Value Analysis of Nonmetallic Inclusions in Steel and Other Microstructural Features, (2014). doi:10.1520/E2283-08R14.2.
75. Stress-intensity factor equations for cracks in Three-dimensional finite bodies subjected to tension and bending loads
76. Surface texture: two-dimensional
77. Improving the fatigue behaviour of a selectively laser melted aluminium alloy: influence of heat treatment and surface quality10.1016/j.matdes.2016.05.041 ↗
78. Consolidation phenomena in laser and powder-bed based layered manufacturing, CIRP Ann10.1016/j.cirp.2007.10.004 ↗
79. Effect of hardness and crack geometries on DKth of small cracks emanating from small defects
80. Quantitative evaluation of the effect of surface roughness10.1299/kikaia.63.1612 ↗
81. Übertragbarkeit von Werkstoffkennwerten am Beispiel eines betriebsfest auszulegenden geschmiedeten Nutzfahrzeug-Achsschenkels
82. Assessment of methods for prediction of notch and size effects at the fatigue limit based on test data by Böhm and Magin10.1016/j.ijfatigue.2010.03.011 ↗
83. A relation between theoretical stress concentration factor and fatigue notch factor deduced from the concept of highly stressed volume
84. Beretta · 2009