journal article·2023-04

Superior strength of laser-arc hybrid additive manufactured Al-Zn-Mg-Cu alloy enabled by a tunable microstructure

Dehua Liu, Dongjiang Wu, Changrong Ge, Haifei Lu, Zhuo Chen, Miaoran Liu, Yunsong Wang, Fangyong Niu, Guangyi Ma, Kaiyu Luo, Jinzhong Lu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (82)

Show source-provided references
1. Nanoparticle-enabled phase control for arc welding of unweldable aluminum alloy 707510.1038/s41467-018-07989-y ↗
2. Development of ultrafine grained high strength age hardenable Al 7075 alloy by cryorolling10.1016/j.matdes.2011.02.051 ↗
3. Microstructure tuning enables synergistic improvements in strength and ductility of wire-arc additive manufactured commercia Al-Zn-Mg-Cu alloys10.1080/17452759.2022.2048236 ↗
4. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
5. Progress and perspectives in laser additive manufacturing of key aeroengine materials10.1016/j.ijmachtools.2021.103804 ↗
6. Comparative study of microstructure evaluation and mechanical properties of 4043 aluminum alloy fabricated by wire-based additive manufacturing10.1016/j.matdes.2019.108205 ↗
7. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗
8. Laser powder bed fusion of AA7075 alloy: influence of process parameters on porosity and hot cracking
9. Selective laser melting of Al7050 powder: melting mode transition and comparison of the characteristics between the keyhole and conduction mode10.1016/j.matdes.2017.09.014 ↗
10. Assessment of AlZnMgCu alloy powder modification for crack-free laser powder bed fusion by differential fast scanning calorimetry10.1016/j.matdes.2021.109677 ↗
11. Influence of erbium addition on the defects of selective laser-melted 7075 aluminium alloy10.1080/17452759.2021.1990358 ↗
12. Complete columnar-to-equiaxed transition and significant grain refinement in an aluminium alloy by adding Nb particles through laser powder bed fusion
13. Microstructures and tensile properties of a selective laser melted Al-Zn-Mg-Cu (Al7075) alloy by Si and Zr microalloying10.1016/j.msea.2020.139492 ↗
14. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
15. Enhanced strength and ductility in Al-Zn-Mg-Cu alloys fabricated by laser powder bed fusion using a synergistic grain-refining strategy10.1016/j.jmst.2021.12.078 ↗
16. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
17. Wire and arc additive manufacturing: opportunities and challenges to control the quality and accuracy of manufactured parts10.1016/j.matdes.2021.109471 ↗
18. Invited review article: strategies and processes for high quality wire arc additive manufacturing
19. Microstructure and properties research of Al-Zn-Mg-Cu alloy with high strength and high elongation fabricated by wire arc additive manufacturing10.1016/j.jmatprotec.2022.117665 ↗
20. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
21. Wire and arc additive manufacturing of high-strength Al-Zn-Mg aluminum alloy10.3389/fmats.2021.656429 ↗
22. Achieving high strength-ductility of Al-Zn-Mg-Cu alloys via hot-wire arc additive manufacturing enabled by strengthening precipitates
23. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
24. Ultrasonic effects on gas tungsten arc based wire additive manufacturing of aluminum matrix nanocomposite10.1016/j.matdes.2022.110393 ↗
25. Measuring the effects of a laser beam on melt pool fluctuation in arc additive manufacturing10.1108/RPJ-01-2018-0033 ↗
26. Laser-arc hybrid additive manufacturing of stainless steel with beam oscillation
27. Effects of laser power on texture evolution and mechanical properties of laser-arc hybrid additive manufacturing
28. Multi-energy source (MES) configuration for bead shape control in wire-based directed energy deposition (w-DED
29. Segregation assisted grain boundary precipitation in a model Al-Zn-Mg-Cu alloy10.1016/j.actamat.2018.07.003 ↗
30. Fusion zone geometries, cooling rates and solidification parameters during wire arc additive manufacturing10.1016/j.ijheatmasstransfer.2018.08.111 ↗
31. Multi-layer deposition mechanism in ultra high-frequency pulsed wire arc additive manufacturing (WAAM) of NiTi shape memory alloys
32. Comprehensive modeling of transport phenomena in laser hot-wire deposition process10.1016/j.ijheatmasstransfer.2018.04.164 ↗
33. Modeling of temperature field and pool formation during linear laser welding of DP1000 steel10.1016/j.jmatprotec.2014.03.030 ↗
34. An adaptive heat source model for finite-element analysis of keyhole plasma arc welding10.1016/j.commatsci.2009.02.018 ↗
35. Experimental and numerical investigation of hybrid laser arc welding process and the influence of welding sequence on the manufacture of stiffened flat panels10.1016/j.jmapro.2020.11.040 ↗
36. Revisiting fundamental welding concepts to improve additive manufacturing: from theory to practice10.1016/j.pmatsci.2019.100590 ↗
37. Formation mechanism of Al-Zn-Mg-Cu alloy fabricated by laser-arc hybrid additive manufacturing: microstructure evaluation and mechanical properties
38. Microstructure and mechanical properties of Ti-6Al-4V by electron beam rapid manufacturing10.1016/S1875-5372(14)60083-7 ↗
39. Superior mechanical properties of a selective-laser-melted AlZnMgCuScZr alloy enabled by a tunable hierarchical microstructure and dual-nanoprecipitation10.1016/j.mattod.2021.11.019 ↗
40. Dislocation models of crystal grain boundary10.1103/PhysRev.78.275 ↗
41. Grain refinement and property improvements of Al-Zn-Mg-Cu alloy by heterogeneous particle addition during wire and arc additive manufacturing10.1016/j.jmrt.2021.12.049 ↗
42. Overlapping rate effect on laser shock processing of 1045 steel by small spots with Nd:YAG pulsed laser10.1016/j.surfcoat.2007.07.008 ↗
43. The microstructural evolution of an Al-Zn-Mg-Cu alloy during homogenization10.1016/j.matlet.2005.11.049 ↗
44. Use of ultrasound irradiation during acid etching of the 2024 aluminum alloy: effect on corrosion resistance after anodization10.1016/j.ultsonch.2019.104879 ↗
45. Al-Cu alloy fabricated by novel laser-tungsten inert gas hybrid additive manufacturing
46. Coherent to incoherent transition in mismatched interfaces10.1016/S1359-6462(97)00570-8 ↗
47. An atomic scale structural investigation of nanometre-sized η precipitates in the 7050 aluminium alloy10.1016/j.actamat.2019.05.041 ↗
48. Liquid phase bonding of aluminium and aluminium/nicalon composite using copper interlayers10.1179/mst.1993.9.5.417 ↗
49. Characterisation and modelling of precipitate evolution in an Al-Zn-Mg alloy during non-isothermal heat treatments10.1016/S1359-6454(03)00429-4 ↗
50. Influence of predeformation on ageing in an Al-Zn-Mg alloy–I. Microstructure evolution and mechanical properties10.1016/S1359-6454(98)00293-6 ↗
51. Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
52. In situ transmission electron microscopy investigation of nucleation of GP zones under natural aging in Al-Zn-Mg alloy10.1016/j.scriptamat.2021.114319 ↗
53. Secondary ageing in an aluminium alloy 705010.1016/j.msea.2008.02.039 ↗
54. Microstructure and mechanical properties of ultra-high strength Al-Zn-Mg-Cu-Sc aluminum alloy fabricated by wire + arc additive manufacturing10.1016/j.jmapro.2022.05.009 ↗
55. Additive manufacturing using WAAM with AA5183 wire10.1016/j.jmatprotec.2018.04.014 ↗
56. Effect of heat input on microstructure and mechanical properties of Al-Mg alloys fabricated by WAAM10.1016/j.apsusc.2019.04.255 ↗
57. The effects of ultrasonic frequency pulsed arc on wire + arc additively manufactured high strength aluminum alloys
58. Evolution of crystallographic orientation, columnar to equiaxed transformation and mechanical properties realized by adding TiCps in wire and arc additive manufacturing 2219 aluminum alloy
59. The heterogeneous band microstructure and mechanical performance in a wire + arc additively manufactured 2219 Al alloy
60. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
61. The origins for tensile properties of selective laser melted aluminium alloy A357
62. SLM-processed Sc-and Zr-modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
63. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
64. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
65. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
66. Deformation-based additive manufacturing of 7075 aluminum with wrought-like mechanical properties10.1016/j.matdes.2020.109288 ↗
67. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: a state of the art review10.1016/j.pmatsci.2019.04.006 ↗
68. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
69. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
70. Laser-arc hybrid additive manufactured Al-Cu alloy for T-shaped structure: microstructure evaluation and molten pool behavior10.1016/j.jmapro.2022.04.042 ↗
71. TiCp reinforced Ti6Al4V of follow-up synchronous electromagnetic induction-laser hybrid directed energy deposition: microstructure evolution and mechanical properties
72. Physical processes in fusion welding10.1103/RevModPhys.67.85 ↗
73. Numerical analysis of heat transfer during multi-layer selective laser melting of AlSi10Mg10.1016/j.ijleo.2016.06.115 ↗
74. Numerical simulation of keyhole behaviors and fluid dynamics in laser-gas metal arc hybrid welding of ferrite stainless steel plates10.1016/j.jmapro.2016.11.009 ↗
75. Development of a high strength Zr/Sc/Hf-modified Al-Mn-Mg alloy using laser powder bed fusion: design of a heterogeneous microstructure incorporating synergistic multiple strengthening mechanisms
76. Effect of post-deposition heat treatment on laser-TIG hybrid additive manufactured Al-Cu alloy10.1080/17452759.2020.1818021 ↗
77. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
78. Structure-property correlations in Al 7050 and Al 7055 high-strength aluminum alloys10.1016/j.msea.2007.05.116 ↗
79. Coarsening resistance at 400 °C of precipitation-strengthened Al-Zr-Sc-Er alloys10.1016/j.actamat.2011.07.057 ↗
80. Layer control method and mechanical anisotropy of titanium alloy based on double-hot-wire arc additive manufacturing10.1016/j.jmapro.2022.08.019 ↗
81. Micropore evolution in additively manufactured aluminum alloys under heat treatment and inter-layer rolling10.1016/j.matdes.2019.108288 ↗
82. Microstructure and mechanical properties of wire + arc additively manufactured 2024 aluminum alloy components: As-deposited and post heat-treated10.1016/j.jmapro.2019.03.003 ↗