Effect of build height on the properties of large format stainless steel 316L fabricated via directed energy deposition
Source abstract
Abstract
Abstract Directed energy deposition (DED) is a promising technique for cladding and repair due to its ability to deposit molten metal onto existing surfaces. To date, much still needs to be understood regarding the microstructure evolution during DED. The work herein seeks to reveal the effect of build height on mechanical properties and corrosion for austenitic stainless steel 316L. A large 316L block was fabricated via DED and horizontal tensile specimens were taken from every 3 mm along the build height in order to assess the effect of build height on the mechanical response. Electron backscatter diffraction mapping was also conducted on sections taken from the bottom, middle and top heights of the build, to assess the microstructural evolution. Cyclic polarisation testing was performed on sections from the build to assess the pitting potential and re-passivation as a function of build height.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. State of the art in directed energy deposition: from additive manufacturing to materials design10.3390/coatings9070418 ↗
2. Additive manufacturing of biomaterials10.1016/j.pmatsci.2017.08.003 ↗
3. Application of directed energy deposition-based additive manufacturing in repair10.3390/app9163316 ↗
4. Developments in disk laser welding
5. An overview of Direct Laser Deposition for additive manufacturing; part II: mechanical behavior, process parameter optimization and control
6. Feasibility exploration of superalloys for AISI 4140 steel repairing using laser engineered net shaping10.1016/j.promfg.2017.07.080 ↗
7. Bonding mechanisms in cold spraying: the contributions of metallurgical and mechanical components10.1007/s11666-009-9298-1 ↗
8. Bonding mechanism in cold gas spraying10.1016/S1359-6454(03)00274-X ↗
9. An overview of Direct Laser Deposition for additive manufacturing; part I: transport phenomena, modeling and diagnostics
10. Effects of process variables and size-scale on solidification microstructure in beam-based fabrication of bulky 3D structures10.1016/j.msea.2009.02.019 ↗
11. Analysis of thermal phenomena in LENS™ deposition10.1016/j.msea.2006.07.087 ↗
12. Understanding thermal behavior in the LENS process10.1016/S0261-3069(99)00016-3 ↗
13. An investigation of the effect of laser deposition parameters on characteristics of multilayered 316 L deposits10.1007/s00170-014-5951-z ↗
14. Thermal behavior and geometry model of melt pool in laser material process10.1115/1.2005275 ↗
15. Additive manufacturing of a functionally graded material from Ti-6Al-4V to Invar: experimental characterization and thermodynamic calculations10.1016/j.actamat.2016.12.070 ↗
16. Thermal behavior and microstructural evolution during laser deposition with laser-engineered net shaping: part I. Numerical calculations10.1007/s11661-008-9557-7 ↗
17. The formation of the σ phase during long term high temperature creep of type 316 austenitic stainless steel10.1016/0025-5416(79)90091-0 ↗
18. Sigma phase embrittlement of a type 310 stainless steel10.1016/0921-5093(91)90695-J ↗
19. A comparison on metallurgical behaviors of 316L stainless steel by selective laser melting and laser cladding deposition10.1016/j.msea.2016.12.112 ↗
20. Microstructural control of additively manufactured metallic materials10.1146/annurev-matsci-070115-031816 ↗
21. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
22. Texture control during laser deposition of nickel-based superalloy10.1016/j.scriptamat.2012.06.014 ↗
23. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
24. Study on microstructure, mechanical properties and machinability of efficiently additive manufactured AISI 316L stainless steel by high-power direct laser deposition10.1016/j.jmatprotec.2016.09.005 ↗
25. Control of shape and performance for direct laser fabrication of precision large-scale metal parts with 316L Stainless Steel10.1016/j.optlastec.2012.07.002 ↗
26. Digital image correlation for microstructural analysis of deformation pattern in additively manufactured 316L thin walls
27. Dissimilar welding behavior of 22% Cr series stainless steel with 316L and its corrosion resistance in modified aggressive environment10.1016/j.jmapro.2016.07.001 ↗
28. Pitting corrosion of welded joints of austenitic stainless steels studied by using an electrochemical minicell10.1016/j.corsci.2007.11.028 ↗
29. Effect of heat treatment on microstructure, mechanical and corrosion properties of austenitic stainless steel 316L using arc additive manufacturing10.1016/j.msea.2017.10.002 ↗
30. The relationship between solidification and microstructure in austenitic and austenitic-ferritic stainless steel welds10.1007/BF02697081 ↗
31. Prediction of austenitic weld metal microstructure and properties
32. Technical Note: the Effect of Retained Ferrite on Localized Corrosion in Duplex 304L Stainless Steel
33. Mechanical behavior of selective laser melted 316L stainless steel10.1016/j.msea.2017.04.058 ↗
34. Effect of selective laser melting (SLM) process parameters on microstructure and mechanical properties of 316L austenitic stainless steel10.1016/j.jmatprotec.2017.05.042 ↗
35. On the corrosion and metastable pitting characteristics of 316L stainless steel produced by selective laser melting10.1149/2.0551706jes ↗
36. Inclusions in stainless steels — a review10.1002/srin.201700130 ↗
37. On the enhanced corrosion resistance of a selective laser melted austenitic stainless steel10.1016/j.scriptamat.2017.07.037 ↗
38. Microstructure and corrosion resistance of laser additively manufactured 316L stainless steel10.1007/s11837-016-1822-4 ↗
39. Studies on pitting corrosion and sensitization in laser rapid manufactured specimens of type 316L stainless steel10.1016/j.matdes.2012.03.011 ↗
40. Gray iron
41. Microstructure of 316L stainless steel components produced by direct laser deposition10.3103/S096709121612010X ↗
42. Epitaxial growth in 316L steel and CoCrFeMnNi high entropy alloy made by powder-bed laser melting10.1063/1.5035000 ↗
43. Additive manufacturing processes: selective laser melting, electron beam melting and binder jetting-selection guidelines10.3390/ma10060672 ↗
44. Quantitative examination of carbide and sulphide precipitates in chemically complex steels processed by direct strip casting10.1016/j.matchar.2015.12.028 ↗
45. Effect of residual stress on the corrosion behavior of austenitic stainless steel10.4236/aces.2015.51007 ↗
46. Effects of tensile and compressive stresses on the passive layers formed on a type 302 stainless steel in a normal sulphuric acid bath10.1007/BF00356115 ↗
47. Surface modifications induced in 316L steel by laser peening and shot-peening. Influence on pitting corrosion resistance10.1016/S0921-5093(99)00698-X ↗
48. The role of residual stress in neutral pH stress corrosion cracking of pipeline steels. Part I: pitting and cracking occurrence10.1016/j.actamat.2006.08.037 ↗
49. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
50. Corrosion of additively manufactured alloys: a review10.5006/2926 ↗