Wire arc additive manufacturing of titanium aluminide alloys using two-wire TOP-TIG welding: Processing, microstructures, and mechanical properties
Source abstract
Abstract
Abstract Titanium aluminide (TiAl) alloys are promising high-temperature structural materials in the aerospace field. Additive manufacturing is a desirable process for fabricating TiAl alloys. In the process of wire arc additive manufacturing of TiAl alloys, Al-based and Ti-based wires were used as the feedstocks. However, it is hard to ensure the two different wires melt synchronously under the heat of one single arc, so the desired microstructures with γ (TiAl) phase and α2 (Ti3Al) phase are hard to obtain. A two-wire TOP-TIG-based additive manufacturing process for TiAl alloys is proposed in this paper. The Ti6Al4V wire and pure Al wire are used as the feedstocks. The Al wire is fed in TOP-TIG mode behind the molten pool, while the Ti6Al4V wire is fed in conventional TIG mode in front of the molten pool. The two wires melt synchronously in a broad range of parameters. The compositions of the component can be controlled by adjusting the two-wire feeding speeds. The main microstructures of the as-fabricated component contain α2/γ lamellae colonies, equiaxed γ grains, and α2 grains. In the top and middle regions, when the Al content is 45 at.%, the structures are full α2/γ lamellae; as the Al content increases to 50 at.%, some equiaxed γ grains distribute at the grain boundaries; the component with 55 at.% Al content exhibits the structures consists of equiaxed γ grains with snowflake-shaped α2/γ lamellae colonies. In the bottom region, all components exhibit the coarse equiaxed α2 grains with γ laths. As the Al content increases, the α2 phase decreases, but the γ phase increases, and from the top region to the bottom region, the volume fraction of the α2 increases by about 19.4 %. The hardness value of the top and bottom regions is higher, and the middle region exhibits the lowest hardness. As the Al content increases, the hardness decreases. The component with 50 at.% Al exhibits the highest compressive strength with 1762 MPa and the largest compressive ratio with 26.1%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Intermetallic alloys based on gamma titanium aluminide10.1007/BF03220267 ↗
2. Electrochemical corrosion and tribological evaluation of TiAl alloy for marine application10.1016/j.triboint.2017.06.027 ↗
3. Modern refractory alloys based on titanium gamma-aluminide: prospects of development and application10.1007/s11041-014-9763-4 ↗
4. Interfacial strengthening by soft phase in lamellar microstructure of TiAl alloys10.1063/1.2733600 ↗
5. Advances in gamma titanium aluminides and their manufacturing techniques10.1016/j.paerosci.2012.04.001 ↗
6. Review of alloy and process development of TiAl alloys10.1016/j.intermet.2005.10.019 ↗
7. Fabrication of NiTi through additive manufacturing: a review10.1016/j.pmatsci.2016.08.001 ↗
8. Effect of building direction on the microstructure and tensile properties of Ti-48Al-2Cr-2Nb alloy additively manufactured by electron beam melting
9. Additive manufacturing of γ-TiAl: processing, microstructure, and properties10.1002/adem.201500588 ↗
10. The optimisation of processing parameters and characterisation of microstructure of direct laser fabricated TiAl alloy components10.1016/S0261-3069(99)00091-6 ↗
11. The effect of process parameters and heat treatment on the microstructure of direct laser fabricated TiAl alloy samples10.1016/S0966-9795(01)00063-2 ↗
12. Effect of energy input on microstructure and mechanical properties of titanium aluminide alloy fabricated by the additive manufacturing process of electron beam melting10.3390/ma10020211 ↗
13. Electron beam melting of Ti-48Al-2Cr-2Nb alloy: Microstructure and mechanical properties investigation10.1016/j.intermet.2010.11.017 ↗
14. Invited review article: strategies and processes for high quality wire arc additive manufacturing
15. Mechanical properties of Ti-6Al-4V specimens produced by shaped metal deposition10.1088/1468-6996/10/1/015008 ↗
16. Microstructural evolution and mechanical properties of Inconel 625 alloy during pulsed plasma arc deposition process10.1016/j.jmst.2013.02.010 ↗
17. Mechanical properties of 2219-Al components produced by additive manufacturing with TIG10.1007/s00170-015-8168-x ↗
18. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
19. Arc welding processes for additive manufacturing: a review
20. Wire and arc additive manufacturing of a Ni-rich NiTi shape memory alloy: microstructure and mechanical properties
21. Microstructure and mechanical properties of double-wire + arc additively manufactured Al-Cu-Mg alloys10.1016/j.jmatprotec.2017.12.019 ↗
22. The effect of location on the microstructure and mechanical properties of titanium aluminides produced by additive layer manufacturing using in-situ alloying and gas tungsten arc welding10.1016/j.msea.2015.02.051 ↗
23. The formation and Kr-ion irradiation behaviour of new microstructural features in additively manufactured titanium aluminium alloy
24. Effect of interpass temperature on in-situ alloying and additive manufacturing of titanium aluminides using gas tungsten arc welding
25. The effect of postproduction heat treatment on γ-TiAl alloys produced by the GTAW-based additive manufacturing process10.1016/j.msea.2016.01.060 ↗
26. Introduction of ternary alloying element in wire arc additive manufacturing of titanium aluminide intermetallic
27. Microstructure and mechanical properties of TOP-TIG-wire and arc additive manufactured super duplex stainless steel (ER2594)10.1016/j.msea.2019.138097 ↗
28. Wire and arc additive manufacturing: a comparison between CMT and TopTIG processes applied to stainless steel10.1007/s40194-018-0606-6 ↗
29. TiAl alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
30. Microstructural characterization of laser melting deposited Ti–5Al-5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.jallcom.2013.03.243 ↗
31. Analysis of gamma titanium aluminide welds produced by gas tungsten arc welding
32. Densification of rapidly solidified titanium aluminide powders-I. Comparison of experiments to hiping models10.1016/0956-7151(90)90090-4 ↗
33. Nanometer-scaled lamellar microstructures in Ti-45Al-7.5Nb-(0;0.5)C alloys and their influence on hardness10.1016/j.intermet.2008.03.009 ↗
34. Mechanical size-effects in miniaturized and bulk materials10.1002/adem.200600153 ↗
35. Hall-Petch relationships in gamma titanium aluminides10.1016/1359-6462(96)00097-8 ↗
36. Hardness and modulus of the lamellar microstructure in PST-TiAl studied by nanoindentations and AFM10.1016/S1359-6454(00)00375-X ↗
37. Microstructural design for thermal creep and radiation damage resistance of titanium aluminide alloys for high-temperature nuclear structural applications10.1016/j.cossms.2014.07.003 ↗