High strength Al–Li alloy development for laser powder bed fusion
Source abstract
Abstract
Abstract With laser powder bed fusion (LPBF) of aluminum alloys growing in recent years, the research focus is progressively shifting from processing attempts on mature cast and wrought aluminum alloys to developing new aluminum alloy systems. This paper reports a novel Al–Li alloy specifically developed for the LPBF technology. The methodology of laser glazing on cast parts was applied to approximate solidification conditions of LPBF. Five variants of Al–Cu–Li ingots with different Sc and Zr contents were developed, and the optimized chemical composition was obtained and converted to Al–Cu–Li–Sc–Zr powder. This newly developed Al–Cu–Li–Sc–Zr alloy was successfully processed by LPBF with a high building rate and a low Li loss rate. The novel alloy shows excellent tensile properties including yield strength of 482 ± 1 MPa, ultimate tensile strength of 539 ± 1 MPa, and elongation of 8.8 ± 0.7%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
2. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
4. Design approaches for printability-performance synergy in Al alloys for laser-powder bed additive manufacturing10.1016/j.matdes.2021.109640 ↗
5. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
6. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
7. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
8. Selective laser melting of high strength Al–Cu–Mg alloys: processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
9. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
10. Selective laser melting of Al7050 powder: melting mode transition and comparison of the characteristics between the keyhole and conduction mode10.1016/j.matdes.2017.09.014 ↗
11. Effect of defocusing distance on laser powder bed fusion of high strength Al–Cu–Mg–Mn alloy10.1080/17452759.2020.1760895 ↗
12. Process and mechanical properties: applicability of a scandium modified al-alloy for laser additive manufacturing10.1016/j.phpro.2011.03.047 ↗
13. Microstructural features of Sc- and Zr-modified Al–Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
14. SLM-processed Sc- and Zr- modified Al–Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
15. Effect of laser rescanning on the grain microstructure of a selective laser melted Al–Mg–Zr alloy10.1016/j.matchar.2018.03.033 ↗
16. Microstructure and mechanical properties of Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
17. Effects of Sc and Zr on microstructure and properties of 1420 aluminum alloy10.1016/j.matchar.2019.06.001 ↗
18. Role of Zr and Sc addition in controlling the microstructure and tensile properties of aluminum–copper based alloys10.1016/j.matdes.2015.09.090 ↗
19. High strength aluminum cast alloy: a Sc modification of a standard Al–Si–Mg cast alloy10.1016/j.msea.2014.03.005 ↗
20. Influence of the degree of scandium supersaturation on the precipitation kinetics of rapidly solidified Al–Mg–Sc–Zr alloys10.1016/j.actamat.2016.07.001 ↗
21. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al–Cu–Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
22. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al–4.24Cu–1.97Mg–0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
23. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
24. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
25. Characterisation of AlScZr and AlErZr alloys processed by rapid laser melting10.1016/j.scriptamat.2018.03.035 ↗
26. Novel Al-X alloys with improved hardness10.1016/j.matdes.2020.108699 ↗
27. Towards a high strength aluminium alloy development methodology for selective laser melting10.1016/j.matdes.2019.107775 ↗
28. Selective laser melting of a high strength Al Mn Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
29. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
30. Recent advances in the development of aerospace materials10.1016/j.paerosci.2018.01.001 ↗
31. Investigation of the lithium-containing aluminum copper alloy (AA2099) for the laser powder bed fusion process [L-PBF]: effects of process parameters on cracks, porosity, and microhardness10.1007/s11837-019-03367-1 ↗
32. Characterising the microstructure of an additively built Al–Cu–Li alloy10.3390/ma13225188 ↗
33. Microstructure, metallurgical defects and hardness of Al–Cu–Mg–Li–Zr alloy additively manufactured by selective laser melting10.1016/j.jallcom.2020.155372 ↗
34. A high strength Al–Li alloy produced by laser powder bed fusion: densification, microstructure, and mechanical properties
35. Understanding grain refinement of Sc addition in a Zr containing Al–Zn–Mg–Cu aluminum alloy from experiments and first-principles10.1016/j.intermet.2020.106823 ↗
36. Scandium overtakes zirconium10.1038/nmat1663 ↗
37. Complex precipitation pathways in multicomponent alloys10.1038/nmat1652 ↗
38. Scandium in aluminium alloys10.1179/174328005X14311 ↗
39. Dispersoid composition in zirconium containing Al-Zn-Mg-Cu (AA7010) aluminium alloy10.1016/j.actamat.2019.02.047 ↗
40. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
41. Microstructure and mechanical properties of Al-Cu alloys fabricated by selective laser melting of powder mixtures10.1016/j.jallcom.2017.10.168 ↗
42. Microstructure, mechanical properties and strengthening mechanisms of AlCu5MnCdVA aluminum alloy fabricated by selective laser melting10.1016/j.msea.2019.04.114 ↗
43. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
44. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
45. Rapid solidification: selective laser melting of AlSi10Mg10.1007/s11837-015-1763-3 ↗
46. Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting10.1016/j.scriptamat.2019.04.036 ↗
47. Cracking mechanism and its sensitivity to processing conditions during laser powder bed fusion of a structural aluminum alloy10.1016/j.mtla.2020.100976 ↗
48. Vaporization of alloying elements and explosion behavior during laser powder bed fusion of Cu–10Zn alloy10.1016/j.ijmachtools.2020.103686 ↗
49. Gale · 2003
50. Influence of element vaporization on formability, composition, microstructure, and mechanical performance of the selective laser melted Mg–Zn–Zr components10.1016/j.matlet.2015.05.074 ↗
51. Microstructural features of Sc- and Zr-modified Al–Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
52. Heat treatment of aluminium alloys produced by laser powder bed fusion: a review10.1016/j.matdes.2021.109651 ↗
53. Quantification and modelling of the microstructure/strength relationship by tailoring the morphological parameters of the T1 phase in an Al–Cu–Li alloy10.1016/j.actamat.2014.04.046 ↗
54. Selective laser melting of Al–3.48Cu–2.03Si–0.48Sc–0.28Zr alloy: microstructure evolution, properties and metallurgical defects10.1016/j.intermet.2020.107008 ↗
55. A novel crack-free Ti-modified Al–Cu–Mg alloy designed for selective laser melting
56. Microstructure and mechanical properties of a TiB2-modified Al–Cu alloy processed by laser powder-bed fusion10.1016/j.msea.2020.140209 ↗
57. Intensive processing optimization for achieving strong and ductile Al–Mn–Mg–Sc–Zr alloy produced by selective laser melting10.1016/j.matdes.2020.109317 ↗
58. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
59. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
60. Effect of aging treatment on the microstructure and mechanical properties of Al–3.02Mg–0.2Sc–0.1Zr alloy printed by selective laser melting10.1016/j.matdes.2019.107668 ↗
61. Effect of bimodal microstructure on the tensile properties of selective laser melt Al–Mg–Sc–Zr alloy10.1016/j.jallcom.2019.152422 ↗
62. Microstructure and tensile property of a novel AlZnMgScZr alloy additively manufactured by gas atomization and laser powder bed fusion10.1016/j.scriptamat.2018.08.025 ↗
63. Development of a high strength Al–Zn–Si–Mg–Cu alloy for selective laser melting10.1016/j.jallcom.2019.06.123 ↗