journal article·2019-08

On microstructure and early stage corrosion performance of heat treated direct metal laser sintered AlSi10Mg

Mehran Rafieazad, Mohsen Mohammadi, Ali M. Nasiri

Publisher page

Abstract

Abstract This study examines the impact of low-temperature heat-treatment on the microstructure and corrosion performance of direct metal laser sintered (DMLS)-AlSi10Mg alloy. Differential scanning calorimetry (DSC) was used to determine the phase(s) transition temperatures in the alloy. Two exothermic phenomena were detected and associated with the Mg2Si precipitation and Si phase precipitation in the as-printed alloy. Based on DSC results, thermal-treatments including below and above the active Si precipitation temperature at 200 °C and 300 °C, respectively, and 350 °C as an upper limit temperature for 3 h were applied to the as-printed samples. Scanning electron microscopy and X-ray diffraction analysis confirmed that heat-treatment from 200 °C to 350 °C promotes the homogeneity of the microstructure, characterized by uniform distribution of eutectic Si in α-Al matrix. To investigate the impact of the applied heat-treatment cycles on corrosion resistance of DMLS-AlSi10Mg at early stage of immersion, anodic polarization testing and electrochemical impedance spectroscopy were performed in aerated 3.5 wt.% NaCl solution. The results revealed more uniformly distributed pitting attack on the corroded surfaces by increasing the heat-treatment temperature up to 300 °C, attributed to the more protective nature of the spontaneously air-formed passive layer on the surface of the alloy at initial immersion time. Further increase of the heat treatment temperature to 350 °C induced severe localized corrosion attacks near the coarse Si particles, ascribed to the increased potential difference between the coalesced Si particles and aluminum matrix galvanic couple. In comparison, the corrosion of the as-printed and 200 °C heat treated samples was characterized by a penetrating selective attack along the melt pool boundaries, leading to a higher corrosion current density and an active surface at early exposure, associated with the weakness of the existing passive film on their surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. On microstructure and mechanical properties of additively manufactured AlSi10Mg_200C using recycled powder10.1016/j.msea.2017.09.041 ↗
2. Micro-CT-based improvement of geometrical and mechanical controllability of selective laser melted Ti6Al4V porous structures10.1016/j.msea.2011.06.045 ↗
3. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by selective laser melting (SLM)10.1016/j.matchar.2017.06.029 ↗
4. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al–7.5Si–0.5Mg alloy10.1016/j.matdes.2010.08.040 ↗
5. A comparative study on corrosion and microstructure of direct metal laser sintered AlSi10Mg_200C and die cast A360.1 aluminum10.1016/j.jmatprotec.2018.04.013 ↗
6. Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment
7. Comparison of AlSi10Mg and Al 6061 processed through DMLS
8. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
9. Direct metal laser sintering: an additive manufacturing technology ready to produce lightweight structural parts for robotic applications
10. On the precipitation hardening of selective laser melted AlSi10Mg10.1007/s11661-015-2980-7 ↗
11. Thermal treatments of AlSi10Mg processed by laser beam melting
12. Effect of thermal annealing on microstructure evolution and mechanical behavior of an additive manufactured AlSi10Mg part10.1557/jmr.2018.82 ↗
13. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
14. Influence of annealing on mechanical properties of Al-20Si processed by selective laser melting10.3390/met4010028 ↗
15. Effect of heat treatment on corrosion resistance of DMLS AlSi10Mg alloy10.1016/j.electacta.2016.04.157 ↗
16. Corrosion behavior of heat-treated AlSi10Mg manufactured by laser powder bed fusion10.3390/ma11071051 ↗
17. Influence of heat treatments on the corrosion mechanism of additive manufactured AlSi10Mg
18. Materials · 2014
19. Comparison of methods for removal of corrosion product from AA2024-T310.5006/1.3290336 ↗
20. Precipitation and dissolution reactions in a 6061 aluminum alloy10.2320/matertrans1989.41.300 ↗
21. Low temperature annealing dedicated to AlSi10Mg selective laser melting products10.1016/j.jallcom.2016.12.019 ↗
22. Effect of reinforcement on the aging response of cast 6061 Al-Al2O3 particulate composites10.1007/BF02851349 ↗
23. On the silicon spheroidization in Al-Si alloys10.1016/S1471-5317(03)00010-5 ↗
24. Dynamic loading of direct metal laser sintered AlSi10Mg alloy: strengthening behavior in different building directions10.1016/j.matdes.2018.08.045 ↗
25. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
26. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
27. Kurz · 1986
28. Columnar to equiaxed transition during direct metal laser sintering of AlSi10Mg alloy: effect of building direction
29. On the selective laser melting (SLM) of the AlSi10Mg alloy: process, microstructure, and mechanical properties10.3390/ma10010076 ↗
30. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
31. Contribution of Mg2Si precipitates to the strength of direct metal laser sintered AlSi10Mg10.1016/j.msea.2018.10.055 ↗
32. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
33. Local corrosion behavior of additive manufactured AlSiMg alloy assessed by SEM and SKPFM10.1149/2.0461702jes ↗
34. G.S. Peng, K.H. Chen, H.C. Fang, H. Chao, S.Y. Chen, EIS study on pitting corrosion of 7150 aluminum alloy in sodium chloride and hydrochloric acid solution, Mater. Corros. 61 (n.d.) 783–789. doi:10.1002/maco.200905413.10.1002/maco.200905413 ↗
35. Evaluation of corrosion resistance of Al–10Si–Mg alloy obtained by means of direct metal laser sintering10.1016/j.jmatprotec.2015.12.033 ↗
36. Impedance and transient study of aluminium barrier-type oxide films10.1007/BF00242197 ↗
37. EIS study on pitting corrosion of AA5083-H321 aluminum-magnesium alloy in stagnant 3.5% NaCl solution
38. Pitting corrosion of rheocast A356 aluminium alloy in 3.5wt.% NaCl solution10.1016/j.corsci.2013.04.023 ↗