Tensile and fatigue crack growth behavior of commercially pure titanium produced by laser powder bed fusion additive manufacturing
Source abstract
Abstract
Abstract The effects of build orientation and post heat treatments on the tensile and fatigue crack growth (FCG) behavior of commercially pure titanium (CP-Ti) manufactured by laser powder bed fusion (LPBF) using grade 2 powder were examined. Two orthogonal build orientations were used in conjunction with hot isostatic pressing (HIP) both above (950 °C) and below (730 °C) the β-transus temperature and property comparisons were also made to commercially available wrought material. The HIP treatments coarsened the α grain structure, reduced the tensile strength, and increased the fatigue crack growth threshold. The LPBF materials were generally stronger and more fatigue resistant than the wrought material due higher interstitial oxygen and nitrogen content. Additionally, higher tensile strength values were found for one build orientation with higher nitrogen content that was attributed to the different thermal histories during LPBF. However, the build orientation effect was not observed for the FCG behavior of the LPBF material and the FCG resistance at low growth rates were mainly controlled by the grain size. This was in sharp contrast to the wrought material which showed strong anisotropy in the microstructure sensitive fatigue crack growth regime due to strong crystallographic texture. At higher growth rates, FCG became microstructure insensitive when the cyclic plastic zone size became of similar order of magnitude to the grain size.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (91)
Show source-provided references
1. Lütjering · 2007
2. Leyens · 2003
3. Osteoinduction of porous Ti implants with a channel structure fabricated by selective laser melting10.1016/j.actbio.2011.01.037 ↗
4. Bioactive Ti metal analogous to human cancellous bone: fabrication by selective laser melting and chemical treatments10.1016/j.actbio.2010.09.034 ↗
5. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM)10.1016/j.jmatprotec.2016.10.022 ↗
6. Effect of laser power and scan speed on melt pool characteristics of commercially pure titanium (CP-Ti)10.1007/s11665-017-2768-6 ↗
7. On the texture, phase and tensile properties of commercially pure Ti produced via selective laser melting assisted by static magnetic field10.1016/j.msec.2016.09.011 ↗
8. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
9. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
10. Microstructure and mechanical properties of pure titanium models fabricated by selective laser melting10.1243/0954406041319545 ↗
11. Preparation of weak-textured commercially pure titanium by electron beam melting
12. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
13. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: A study from laser power perspective10.1016/j.matdes.2016.12.019 ↗
14. Evaluation of the mechanical and wear properties of titanium produced by three different additive manufacturing methods for biomedical application10.1016/j.msea.2019.06.024 ↗
15. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
16. Evolution of solidification texture during additive manufacturing10.1038/srep16446 ↗
17. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
18. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
19. The importance of crystallographic texture in the use of titanium as an orthopedic biomaterial10.1039/C4RA05440G ↗
20. The effect of grain orientation on fracture morphology during high-cycle fatigue of Ti–6Al–4V10.1016/j.actamat.2009.04.018 ↗
21. Texture effects under tension and torsion loading conditions in titanium alloys10.1016/j.ijfatigue.2005.06.045 ↗
22. Crystallography of fracture facets in a near-alpha titanium alloy10.1007/s11661-006-0144-5 ↗
23. Microstructural influences on fatigue crack growth in Ti-6Al-4V10.1016/0025-5416(74)90104-9 ↗
24. Fatigue crack propagation resistance of beta-annealed Ti-6Al-4V alloys of differing interstitial oxygen contents10.1007/BF02661812 ↗
25. Quantitative analysis of microstructural effects on fatigue crack growth in widmanstätten Ti-6A1–4V and Ti-8Al-1Mo-1V10.1016/0013-7944(79)90138-3 ↗
26. Observations on microstructurally sensitive fatigue crack growth in a widmanstätten Ti-6Al-4V alloy10.1007/BF02646877 ↗
27. Fatigue crack growth transitions in Ti-6Al-4V alloy10.1016/0036-9748(89)90343-8 ↗
28. A study on the change of fatigue fracture mode in two titanium alloys10.1046/j.1460-2695.1998.00095.x ↗
29. TEM observations of fatigue damage accumulation at the surface of the near-alpha titanium alloy IMI 83410.1016/1359-6454(96)00024-9 ↗
30. Characterization of mechanical anisotropy in titanium alloys10.1016/S0921-5093(98)00832-6 ↗
31. The effects of texture in titanium alloys for engineering components under fatigue10.1016/S0142-1123(01)00124-4 ↗
32. The effect of grain size on fatigue crack propagation in commercial pure titanium investigated by acoustic emission10.1007/s11665-015-1545-7 ↗
33. Crystallographic fatigue crack growth in titanium single crystals10.1016/j.msea.2011.06.079 ↗
34. The effects of load ratio, interstitial content, and grain size on low-stress fatigue-crack propagation in α-titanium10.1179/030634573790445550 ↗
35. The influence of grain orientation on the mode and rate of fatigue crack growth in α-titanium10.1007/BF02654715 ↗
36. Z.N. Ismarrubie, H. Yussof, M. Sugano, Fatigue damage mechanism of titanium in vacuum and in air, (eds.), Procedia Eng. 41, 2012, 1559–1565.10.1016/j.proeng.2012.07.350 ↗
37. S. Ando, T. Sakamoto, Y. Ikejiri, M. Tsushida, H. Tonda, Crack orientation dependence of fatigue behavior in titanium single crystals by thin sheet plain bending, in: S.B. Lee, Y.J. Kim (eds.), Experimental Mechanics in Nano and Biotechnology, Pts 1 and 2, Trans Tech Publications Ltd, Stafa-Zurich, 2006, pp. 967–970.10.4028/0-87849-415-4.967 ↗
38. The effect of grain size on small fatigue crack growth in pure titanium10.1016/0142-1123(94)90483-9 ↗
39. Fatigue behavior of titanium
40. The fatigue deformation and fracture characteristics of coarse grained polycrystalline α-titanium10.1016/0036-9748(85)90015-8 ↗
41. A crystallographic study of fatigue damage in titanium10.1007/BF02670692 ↗
42. Near-threshold fatigue crack growth rates of laser powder bed fusion produced Ti-6Al-4V10.1016/j.actamat.2020.07.049 ↗
43. Microstructures and mechanical properties of laser-sintered commercially pure Ti and Ti-6Al-4V alloy for dental applications10.3390/ma13030609 ↗
44. Binding mechanisms in selective laser sintering and selective laser melting10.1108/13552540510573365 ↗
45. Selective laser melting of low-modulus biomedical Ti-24Nb-4Zr-8Sn alloy: effect of laser point distance10.4028/www.scientific.net/KEM.520.226 ↗
46. Comparison of density measurement techniques for additive manufactured metallic parts10.1108/13552541111156504 ↗
47. ASTM Standard E8/E8M-16ae1Standard Test Methods for Tension Testing of Metallic Materials, ASTM International, West Conshohocken, PA, 2016. www.astm.org.
48. 2015
49. 2019
50. Conversion of intercept density to grain size
51. ISO Standard ISO/DIS 21920-3, Geometrical Product Specifications (GPS)–Surface Texture: Profile – Part 3: Specification Operators, International Organization for Standardization; Switzerland, www.iso.org.
52. Fatigue crack growth behavior of laser powder bed fusion additive manufactured Ti-6Al-4V: Roles of post heat treatment and build orientation
53. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
54. Characterization of the variant selection occurring during the α→β→α phase transformations of a cold rolled titanium sheet10.1016/S1359-6454(01)00351-2 ↗
55. Texture formation and transition in Cold-rolled titanium10.1016/0025-5416(88)90245-5 ↗
56. Variant selection and its effect on phase transformation textures in cold rolled titanium sheet10.1016/S0921-5093(99)00666-8 ↗
57. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
58. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
59. Selective laser melting produced Ti-6Al-4V: post-process heat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
60. Diffraction-based misorientation mapping: a continuum mechanics description10.1016/j.jmps.2019.103709 ↗
61. A study of the tensile deformation and fracture behavior of commercially pure titanium and titanium alloy: influence of orientation and microstructure10.1007/s11665-010-9613-5 ↗
62. Fractographic and microstructural analysis of fatigue crack growth in a Ti-6Al-4V fan disc forging10.1016/0142-1123(89)90179-5 ↗
63. Texture evolution during grain growth in recrystallized commercially pure titanium10.1016/j.msea.2005.02.049 ↗
64. Effect of thermal treatments on tensile strength of commercially cast pure titanium and Ti-6Al-4V alloys10.1007/s10856-005-2614-5 ↗
65. Impact of phase transformation on mechanical properties anisotropy of commercially pure titanium10.1016/j.matdes.2011.12.040 ↗
66. Effects of three interstitial solutes (nitrogen, oxygen, and carbon) on the mechanical properties of high-purity, alpha titanium10.1007/BF03399001 ↗
67. Tensile properties improvement by homogenized nitrogen solid solution strengthening of commercially pure titanium through powder metallurgy process10.1016/j.matchar.2020.110700 ↗
68. Selective laser-melted titanium materials with nitrogen solid solutions for balanced strength and ductility10.1016/j.msea.2020.139641 ↗
69. Experimental and theoretical analysis of nitrogen solid-solution strengthening of PM titanium
70. Solid solution strengthening of hexagonal titanium alloys: Restoring forces and stacking faults calculated from first principles10.1016/j.actamat.2015.09.041 ↗
71. Fabrication of high-strength Ti materials by in-process solid solution strengthening of oxygen via P/M methods10.1016/j.msea.2012.11.058 ↗
72. Origin of dramatic oxygen solute strengthening effect in titanium10.1126/science.1260485 ↗
73. Microstructure and mechanical properties of a high nitrogen titanium alloy10.1016/j.msea.2007.08.074 ↗
74. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
75. R. Labusch, A Statistical Theory of Solid Solution Hardening, physica status solidi 41(2), 1970, pp. 659–669.10.1002/pssb.19700410221 ↗
76. Quantitative analysis on light elements solution strengthening in pure titanium sintered materials by labusch model using experimental data10.2320/matertrans.Y-M2018849 ↗
77. Tensile property enhancement by oxygen solutes in selectively laser melted titanium materials fabricated from pre-mixed pure Ti and TiO2 powder10.1016/j.msea.2020.139983 ↗
78. Anisotropy of tensile and fracture behavior of pure titanium after hydrostatic extrusion10.2320/matertrans.MF201928 ↗
79. A geometric model for fatigue crack closure induced by fracture surface roughness10.1007/BF02644803 ↗
80. Some considerations on fatigue crack closure at near-threshold stress intensities due to fracture surface morphology10.1007/BF02642409 ↗
81. Fatigue crack deflection and fracture surface contact: micromechanical models10.1007/BF02815306 ↗
82. The effect of microstructure and fracture surface roughness on fatigue crack propagation in a Ti-6A1–4 V alloy10.1111/j.1460-2695.1993.tb00132.x ↗
83. Fatigue crack growth behavior of titanium alloys10.1016/j.ijfatigue.2005.07.001 ↗
84. Evaluation of near-threshold fatigue crack propagation in harmonic-structured CP titanium with a bimodal grain size distribution10.1016/j.engfracmech.2017.06.026 ↗
85. Dislocation pile-up model of fatigue thresholds for 2024- and 7075-alike aluminium alloys10.1016/0167-8442(95)00040-2 ↗
86. Theoretical modelling of fatigue threshold for aluminium alloys10.1016/0013-7944(95)00206-5 ↗
87. Near-threshold fatigue: a review10.1016/S0142-1123(99)00053-5 ↗
88. Fatigue growth threshold of small cracks10.1007/BF00033345 ↗
89. Effect of build direction on the fracture toughness and fatigue crack growth in selective laser melted Ti-6Al-4V10.1111/ffe.12303 ↗
90. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
91. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗