Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
Source abstract
Abstract
Abstract The longstanding issue in additive manufacturing (AM) of titanium alloys is the large, columnar grains created by the intrinsic directional heat flow along the build direction. These long grains lead to strongly anisotropic mechanical properties that impede the qualification and applications of the final products. In this work, a novel in-situ rolling technique coupled with the direct energy deposition (DED) was developed to fabricate a Ti-6Al-4V alloy part. Through this hybrid technique, excellent isotropic tensile properties were achieved for thin-wall components. The strength and uniform elongation along two mutually perpendicular directions exhibited good consistency with negligible property scatter. Further studies revealed that the isotropic tensile properties were associated with the formation of nearly equiaxed prior-β grains uniformly distributed throughout the whole sample. Meanwhile, the internal α grains exhibited around 2.5 times weaker textures in the rolled compared to the unrolled DED samples. Moreover, strength increases were observed for samples produced by in-situ rolling in DED. This enhanced tensile strength was attributed to the heavily refined prior-β grains compared to those in the unrolled sample. In addition, an interface phase with a face-centred cubic structure (FCC, a = 0.43 nm) was observed between the α and β phases in both unrolled and in-situ rolled samples. The processing method in this work is applicable to other metallic materials to remove the columnar grain structures and provide improved mechanical performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
2. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. An overview of direct laser deposition for additive manufacturing; Part I: transport phenomena, modeling and diagnostics
4. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
5. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
6. P.A. Kobryn, S.L. Semiatin, Mechanical Properties of Laser-deposited Ti-6Al-4V P.A. Kobryn and S.L. Semiatin Air Force Research Laboratory, AFRL/MLLMP OH 45433-7817Wright-Pattern Air Force Base 2013 179 186.
7. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
8. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
9. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
10. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
11. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition10.1016/j.matdes.2019.108191 ↗
12. A review of laser fabrication of metallic engineering components and of materials10.1179/174328407X179593 ↗
13. Microstructures of laser-deposited Ti-6Al-4V10.1016/j.matdes.2003.09.009 ↗
14. A three-dimensional finite element analysis of the temperature field during laser melting of metal powders in additive layer manufacturing10.1016/j.ijmachtools.2009.07.004 ↗
15. Microstructural control in a Ti-based alloy by changing laser processing mode and power during direct laser deposition10.1016/j.matlet.2016.05.038 ↗
16. Multi-scale microstructural development and mechanical properties of a selectively laser melted β titanium alloy
17. Quantitative relationship between anisotropic strain to failure and grain morphology in additively manufactured Ti-6Al-4V10.1016/j.msea.2017.09.017 ↗
18. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
19. Peritectic titanium alloys for 3D printing10.1038/s41467-018-05819-9 ↗
20. Trace carbon addition to refine microstructure and enhance properties of additive-manufactured Ti-6Al-4V10.1007/s11837-018-2994-x ↗
21. Grain refinement of wire arc additively manufactured titanium by the addition of silicon10.1016/j.jallcom.2016.11.049 ↗
22. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components10.1016/j.scriptamat.2016.10.031 ↗
23. Improvement of microstructure and mechanical properties in Wire + Arc additively manufactured Ti-6Al-4V with machine hammer peening10.1016/j.proeng.2018.02.083 ↗
24. Interpass rolling of Ti-6Al-4V wire + arc additively manufactured features for microstructural refinement
25. The effectiveness of combining rolling deformation with wire-arc additive manufacture on β-grain refinement and texture modification in Ti-6Al-4V10.1016/j.matchar.2016.02.001 ↗
26. On the observation of annealing twins during simulating β-grain refinement in Ti–6Al–4V high deposition rate AM with in-process deformation10.1016/j.actamat.2020.01.009 ↗
27. Grain structure control during metal 3D printing by high-intensity ultrasound10.1038/s41467-019-13874-z ↗
28. Hot forging wire and arc additive manufacturing (HF-WAAM)
29. Texture analysis with MTEX- free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
30. TOPAS and TOPAS-Academic: an optimization program integrating computer algebra and crystallographic objects written in C++10.1107/S1600576718000183 ↗
31. Reliability of reconstructed β-orientation maps in titanium alloys10.1016/j.ultramic.2007.01.012 ↗
32. An advanced approach to reconstructing parent orientation maps in the case of approximate orientation relations: application to steels10.1016/j.actamat.2012.04.034 ↗
33. Contrast factors of dislocations in the hexagonal crystal system10.1107/S0021889802009536 ↗
34. Effect of reverted austenite on tensile and impact strength in a martensitic stainless steel−An in-situ X-ray diffraction study10.1016/j.msea.2016.11.039 ↗
35. Fabrication of large Ti-6Al-4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
36. Tensile properties and microstructures of laser-formed Ti-6Al-4V10.1007/s11665-010-9670-9 ↗
37. I. Kelbassa, Qualifizieren des Laserstrahl-Auftragschweißens von BLISKs aus Nickel-und Titanbasislegierungen, Ph.D. Thesis, RWTH Aachen University, 2006.
38. Role of geometry on properties of additively manufactured Ti-6Al-4V structures fabricated using laser based directed energy deposition10.1016/j.matdes.2016.05.045 ↗
39. Lütjering · 2007
40. Formation characteristics of the α/β interface phase in Ti-6Ai-4v10.1007/BF02817630 ↗
41. Observations of an interface phase in the α/β boundaries in titanium alloys10.1007/BF02641987 ↗
42. Revealing competitive columnar grain growth behavior and periodic microstructural banding in additively manufactured Ti-6Al-4 V parts by selective electron beam melting10.1016/j.mtla.2019.100365 ↗
43. Influence of microstructure on mechanical properties of laser metal10.1016/j.msea.2016.07.038 ↗
44. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
45. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
46. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
47. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti–6Al–4V alloy10.1016/j.actamat.2019.03.003 ↗
48. High cycle fatigue in selective laser melted Ti-6Al-4V10.1016/j.actamat.2020.05.041 ↗
49. Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)
50. Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy10.1016/j.matchar.2017.01.014 ↗
51. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
52. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
53. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
54. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
55. M. Salib, L. Germain, J. Teixeira, N. Gey, E. Aeby-Gautier, Influence of phase transformation kinetics on variant selection and microtexture development associated with α precipitation at β grain boundaries in a β-metastable titanium alloy 2015PTM 2015 - Proc. Int. Conf. Solid-Solid Phase Transform. Inorg. Mater. 61 2015 261 262.
56. Influence of transformation temperature on microtexture formation associated with α precipitation at β grain boundaries in a β metastable titanium alloy10.1016/j.actamat.2013.03.007 ↗
57. Crystallographic variant selection in Ti-6Al-4V10.1016/j.actamat.2004.07.034 ↗
58. The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy10.1016/S1359-6454(03)00179-4 ↗
59. Polmear · 2017
60. Could face-centered cubic titanium in cold-rolled commercially-pure titanium only be a Ti-hydride?10.1016/j.scriptamat.2019.11.010 ↗
61. Characterizing solute hydrogen and hydrides in pure and alloyed titanium at the atomic scale10.1016/j.actamat.2018.02.064 ↗
62. Revealing martensitic transformation and α/β interface evolution in electron beam melting three-dimensional-printed Ti-6Al-4V
63. Deformation induced FCC lamellae and their interaction in commercial pure Ti10.1016/j.scriptamat.2018.11.037 ↗
64. Rolling-induced face centered cubic titanium in hexagonal close packed titanium at room temperature
65. Graded microstructure and mechanical properties of additive manufactured Ti-6Al-4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗