journal article·2023-04Open access

Microstructural evolution and strengthening mechanism of Mg-Y-RE-Zr alloy fabricated by quasi-directed energy deposition

Xin Tong, Guohua Wu, Mark A. Easton, Ming Sun, Qiman Wang, Liang Zhang

Abstract

In this work, the highest yield strength and elongation in an Mg-Y-RE-Zr alloy produced by an additive manufacturing (AM) process is reported. A combination of a large-diameter welding wire and a pulsed current was used to inhibit the oxidation of WE43 alloy fabricated by quasi-directed energy deposition using electric arc (quasi-DED-Arc). The results show that the amount of Y2O3 in this work is only 2∼5% of that of the sample produced by powder bed fusion (PBF) reported previously. Moreover, the variable solidification conditions and in-situ heat treatments induced by the multiple thermal cycles (MTCs) were found to result in an inhomogeneous microstructure along the building direction, which are responsible for the variations in mechanical properties. The WE43 alloy exhibits excellent mechanical properties due to the intrinsic heat treatment that occurs during the build process. The 8th layer exhibits a maximum tensile strength of 347 MPa and a good elongation of 7.1%, which exceeds the strength-ductility combinations for cast WE43 alloy. The strengthening mechanisms in different layers have been discussed. A physical model depicting the microstructural transformation during quasi-DED-Arc has been proposed based on the measured thermal cycling data and microstructure observations.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Formation and evolution of the hardening precipitates in a Mg–Y–Nd alloy10.1016/j.actamat.2011.03.038 ↗
2. Hardening precipitation in a Mg–4Y–3RE alloy10.1016/S1359-6454(03)00391-4 ↗
3. On the strain accommodation of β1 precipitates in magnesium alloy WE5410.1016/j.actamat.2014.04.073 ↗
4. In situ neutron diffraction and polycrystal plasticity modeling of a Mg–Y–Nd–Zr alloy: effects of precipitation on individual deformation mechanisms10.1016/j.actamat.2013.03.010 ↗
5. Creep resistance of WE43 magnesium alloy joints10.4028/www.scientific.net/SSP.191.177 ↗
6. Hot cracking in ZK60 magnesium alloy produced by laser powder bed fusion process10.1016/j.matlet.2021.130283 ↗
7. Effective control of microstructure evolution in AZ91D magnesium alloy by SiC nanoparticles in laser powder-bed fusion10.1016/j.matdes.2021.109787 ↗
8. Microstructure evolution of laser powder bed fusion ZK60 Mg alloy after different heat treatment10.1016/j.jallcom.2021.163046 ↗
9. In-situ aging treatment by preheating to obtain high-strength ZK60 Mg alloy processed by laser powder bed fusion10.1016/j.matchar.2022.112361 ↗
10. Recent progress and perspectives in additive manufacturing of magnesium alloys10.1016/j.jma.2022.03.001 ↗
11. Formability, microstructure evolution and mechanical properties of wire arc additively manufactured AZ80M magnesium alloy using gas tungsten arc welding10.1016/j.jma.2020.01.003 ↗
12. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion
13. Microstructure and mechanical behavior of an additive manufactured (AM) WE43-Mg alloy
14. Laser additive manufacturing of biodegradable magnesium alloy WE43: a detailed microstructure analysis10.1016/j.actbio.2019.05.056 ↗
15. Additive manufactured WE43 magnesium: a comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE4310.1016/j.matchar.2018.11.011 ↗
16. A detailed microstructural and corrosion analysis of magnesium alloy WE43 manufactured by selective laser melting
17. Microstructure evolution and mechanical properties of a high-strength Mg-10Gd-3Y–1Zn-0.4Zr alloy fabricated by laser powder bed fusion
18. Development of a laser powder bed fusion process tailored for the additive manufacturing of high-quality components made of the commercial magnesium alloy WE4310.3390/ma14040887 ↗
19. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
20. Microstructure and mechanical properties of repair welds of low-pressure sand-cast Mg–Y–RE–Zr alloy by tungsten inert gas welding10.1016/j.jma.2020.07.009 ↗
21. Effect of TIG welding and rare earth elements alloying on corrosion resistance of magnesium alloys10.1149/1945-7111/abb97e ↗
22. Repairing the WE43 magnesium cast alloys10.4028/www.scientific.net/SSP.176.99 ↗
23. Additive manufacturing of high performance AZ31 magnesium alloy with full equiaxed grains: microstructure, mechanical property, and electromechanical corrosion performance10.1016/j.jmatprotec.2021.117430 ↗
24. Towards high strength cast Mg-RE based alloys: phase diagrams and strengthening mechanisms10.1016/j.jma.2022.03.008 ↗
25. An investigation into wire arc additive manufacturing of Mg-Y-RE-Zr alloy10.1016/j.matlet.2022.132922 ↗
26. Effects of homogenization treatment on recrystallization behavior of 7150 aluminum sheet during post-rolling annealing10.1016/j.matchar.2016.02.008 ↗
27. X-ray micro-tomography an attractive characterisation technique in materials science10.1016/S0168-583X(02)01689-0 ↗
28. Wire-arc additive manufacturing of AZ31 magnesium alloy fabricated by cold metal transfer heat source: Processing, microstructure, and mechanical behavior10.1016/j.jmatprotec.2020.116895 ↗
29. Grain structure control during metal 3D printing by high-intensity ultrasound10.1038/s41467-019-13874-z ↗
30. The response of dislocations, low angle grain boundaries and high angle grain boundaries at high strain rates10.1016/j.msea.2021.141704 ↗
31. Microstructure, mechanical properties, corrosion resistance and cytocompatibility of WE43 Mg alloy scaffolds fabricated by laser powder bed fusion for biomedical applications10.1016/j.msec.2020.111623 ↗
32. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
33. The role of crystallography and thermodynamics on phase selection in binary magnesium–rare earth (Ce or Nd) alloys10.1016/j.actamat.2012.04.039 ↗
34. Recent developments in high-strength Mg-RE-based alloys: focusing on Mg-Gd and Mg-Y systems10.1016/j.jma.2018.08.001 ↗
35. Elucidating the effect of additive friction stir deposition on the resulting microstructure and mechanical properties of magnesium alloy WE4310.3390/met11111739 ↗
36. The effect of powder size on the mechanical and corrosion properties and the ignition temperature of WE43 alloy prepared by spark plasma sintering10.1016/j.jma.2020.12.012 ↗
37. Effect of pre-deformation on microstructure and mechanical properties of WE43 magnesium alloy II: aging at 250 and 300 °C10.1016/j.jma.2019.11.012 ↗
38. Microstructure and impact mechanical properties of multi-layer and multi-pass TIG welded joints of Al-Zn-Mg alloy plates10.1016/S1003-6326(19)65157-5 ↗
39. Review on effect of heat input for wire arc additive manufacturing process10.1016/j.jmrt.2021.02.002 ↗
40. Abnormal macropore formation during double-sided gas tungsten arc welding of magnesium AZ91D alloy10.1016/j.matchar.2007.08.021 ↗
41. In situ differential scanning calorimetry analysis of dissolution and precipitation kinetics in Mg–Y–RE alloy WE4310.1016/j.jma.2019.01.002 ↗
42. Grain refinement in laser remelted Mg-3Nd-1Gd-0.5Zr alloy10.1016/j.scriptamat.2020.03.006 ↗
43. The effect of heat accumulation on the local grain structure in laser-directed energy deposition of aluminium10.3390/met12101601 ↗
44. Effect of laser scanning speed on the microstructure, phase transformation and mechanical property of NiTi alloys fabricated by LPBF10.1016/j.matdes.2022.110460 ↗
45. A review on hot tearing of magnesium alloys10.1016/j.jma.2016.08.003 ↗
46. The Interdependence Theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
47. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
48. Current research progress in grain refinement of cast magnesium alloys: a review article10.1016/j.jallcom.2014.09.061 ↗
49. Exceptional grain refinement of Mg-Zr master alloy treated by tungsten inert gas arc re-melting with ultra-high frequency pulses10.1016/j.scriptamat.2022.114700 ↗
50. Mechanisms of grain refinement by intensive shearing of AZ91 alloy melt10.1016/j.actamat.2010.08.016 ↗
51. Enhanced heterogeneous nucleation in AZ91D alloy by intensive melt shearing10.1016/j.actamat.2009.06.052 ↗
52. Additive manufactured Mg-Gd-Y-Zr alloys: effects of Gd content on microstructure evolution and mechanical properties
53. Hall-Petch relationship in Mg alloys: a review10.1016/j.jmst.2017.07.022 ↗
54. Eutectic phase strengthening and strain rate sensitivity behavior of AZ80 magnesium alloy10.1016/j.msea.2019.138548 ↗