Pore analysis and mechanical performance of selective laser sintered objects

Göran Flodberg, Henrik Pettersson, Li Yang

Abstract

In this work, systematic studies were carried out on SLS (selective laser sintering) printed samples, with two different geometries, standard test samples dumb-bells (dog bones) and tubes (Ø 30 mm and 150 mm long), consisting of two different materials, viz. PA12 (polyamide) with and without the addition of carbon fibres (CFs). These samples were tested according to their respective ISO standards. The standard test samples exhibited relatively small differences with regards to printing directions when PA12 was used alone. Their tensile strengths (σm) were approx. 75%–80% of the injection-moulded sample. The addition of carbon fibres significantly enhanced the tensile strengths, namely 50% greater for the vertically printed test sample and more than 100% greater for the horizontally printed samples, compared to the respective objects consisting of PA12 alone. The strong difference in printing directions can be attributed to the orientation of the carbon fibres. Mechanical tests on the SLS printed tubes confirmed the trends that were found in the standard test samples. Porosity and pore structure inside the SLS printed tubes were studied by combining optical microscopy and X-ray microtomography with image analysis. It was found that porosity was a general phenomenon inside the SLS printed samples. Nevertheless, there were significant differences in porosity, which probably depended on the properties of the materials used, both with and without carbon fibres, thus causing significant differences in light absorption and heat conductivity. The printed samples made of PA12 alone possessed quite a high level of porosity (4.7%), of which the size of the biggest pore was hundreds of microns. The twenty biggest pores with an average size of 75*104 μ m3 accounted for 43% of the total porosity. However, the porosity of the printed samples made from PA12 + CF was only 0.68%, with the biggest pore being only tens of microns. The corresponding average pore size of the 20 biggest pores was 72*103 μ m3, which was one order of magnitude smaller than the printed samples made from PA12 alone. Pores inside the SLS printed samples were probably responsible for a spread in the mechanical properties measured, e.g. tensile strengths, tensile (Young’s) modulus, strain at break, etc. The ratios of their standard deviations to their corresponding mean values in the standard test samples could probably be used as an indicator of porosity, i.e. the bigger the ratio, the higher the porosity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Additive Manufacturing Materials and Processes · Manufacturing Process and Optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Mechanical characterization of 3D-printed polymers
2. Columbus · 2017
3. Emerging rapid manufacturing process
4. Additive manufacturing-enabled design theory and methodology: a critical review10.1007/s00170-015-6994-5 ↗
5. Rosato · 1995
6. Barnatt · 2013
7. Measured energy densities for polyamide 12 and comparision of values calculated for laser sintering
8. Nelson · 1993
9. Selective laser melting of titanium alloy with 50 wt% tantalum: effect of laser process parameters on part quality10.1016/j.ijrmhm.2018.08.006 ↗
10. Experimental investigation of process parameters on layer thickness and density in direct metal laser sintering: a response surface methodology approach10.1080/17452759.2017.1293274 ↗
11. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
12. Correlation of process parameters with mechanical properties of laser sintered PA12 parts
13. Performance limitations in polymer laser sintering10.1016/j.phpro.2014.08.157 ↗
14. Effect of the degree of particle melt on mechanical properties in selective laser-sintered Nylon-12 parts10.1243/09544054JEM1122 ↗
15. Experimental study of porosity and its relation to fatigue mechanisms of model Al-Si7-Mg0. 3 cast Al alloys10.1016/S0921-5093(01)01225-4 ↗
16. Process dependent porosity and the influence of shot peening on porosity morphology regarding selective laser melted AlSi10Mg parts
17. Reducing porosity in additive manufacturing10.1016/j.mprp.2015.01.002 ↗
18. Dependence of mechanical properties of polyamide components on build parameters in the SLS process10.1016/j.jmatprotec.2006.09.007 ↗
19. Investigation of polyamide 11 embrittlement during oxidative degradation10.1016/j.polymer.2015.11.025 ↗
20. ISO 10328:2016 Prosthetics - Structural testing of lower - limb prostheses - Requirements and test methods, 2016.
21. Investigating mechanical anisotropy and end-of-vector effect in laser-sintered nylon parts
22. Leigh · 2012 · 574
23. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
24. Thermal conductivity and Raman spectra of carbon fibres10.1103/PhysRevB.32.6742 ↗
25. Yuan · 2011
26. 3D printing of polymer matrix composites: a review and prospective10.1016/j.compositesb.2016.11.034 ↗