Abstract
Abstract The surface roughness of components built using the laser powder bed fusion (L-PBF) process is poor. Surface finishing the internal channels of L-PBF components is a challenge. We propose a multi-jet hydrodynamic approach to enhance the surface finish quality of the internal channels. We investigate the hydrodynamic finishing on L-PBF Inconel 625 linear, stepped, and non-linear internal channels with diameters 5 to 1 mm and length up to 100 mm (replicating the geometries in rocket injectors, fuel nozzles, and cooling channels). The multi-jet hydrodynamic finishing approach improved the surface quality by 60–90 % (final Ra, Sa ≤ 1 μm and Rz, Sz ≤ 20 μm), using an abrasive concentration of ≤1 % in 15 min. of processing time. Areal surface texture parameters Sdr and roughness ratio r ≈1, evidenced the uniformity of the surface finish with dominant abrasive microcuts, regardless of the initial non-uniform additive manufactured surface. Most of the surface finished channels had excellent dimensional integrity and internal contour circularity. We then discussed the advancements required in metal additive manufacturing and internal surface finishing—to safely deploy L-PBF components with micro internal channels in fuel injection and fluid transfer applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Top surface and side roughness of Inconel 625 parts processed using selective laser melting10.1108/13552540910943397 ↗
2. Analysis and optimisation of vertical surface roughness in micro selective laser melting10.1088/2051-672X/3/3/034007 ↗
3. Influences of processing parameters on surface roughness of Hastelloy X produced by selective laser melting
4. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
5. Surface roughness prediction in additive manufacturing using machine learning
6. Synergistic effects in hydrodynamic cavitation abrasive finishing for internal surface-finish enhancement of additive-manufactured components
7. Cutting force and surface finish analysis of machining additive manufactured titanium alloy Ti-6Al-4V10.1016/j.promfg.2016.12.071 ↗
8. Surface quality and material removal in magnetic abrasive finishing of selective laser melted 316L stainless steel10.1016/j.jmapro.2019.07.044 ↗
9. Laser polishing of additive manufactured CoCr alloy components with complex surface geometry10.1016/j.jmatprotec.2018.06.019 ↗
10. Laser polishing of additive manufactured Ti alloys10.1016/j.optlaseng.2017.02.005 ↗
11. Abrasive-based nano-finishing techniques: an overview10.1080/10910340802278133 ↗
12. Abrasive flow machining of laser powder bed-fused parts: numerical modeling and experimental validation10.1016/j.jmatprotec.2019.116262 ↗
13. Abrasive flow machining (AFM) finishing of conformal cooling channels created by selective laser melting (SLM)10.1016/j.precisioneng.2020.03.006 ↗
14. Surface finish control of additively-manufactured Inconel 625 components using combined chemical-abrasive flow polishing10.1016/j.jmatprotec.2017.10.020 ↗
15. Novel rotating-vibrating magnetic abrasive polishing method for double-layered internal surface finishing10.1016/j.jmatprotec.2018.09.024 ↗
16. Reducing the roughness of internal surface of an additive manufacturing produced 316 steel component by chempolishing and electropolishing
17. Effect of process parameters and electropolishing on the surface roughness of interior channels in additively manufactured nickel-titanium shape memory alloy actuators
18. Study of selective laser melting (SLM) Inconel 718 part surface improvement by electrochemical polishing10.1016/j.matdes.2016.11.103 ↗
19. Electropolishing and electropolishing-related allowances for powder bed selectively laser-melted Ti-6Al-4V alloy components10.1016/j.jmatprotec.2016.11.014 ↗
20. Electropolishing of laser powder bed-fused IN625 components in an ionic electrolyte
21. Gradl · 2018
22. Alloys 625 and 725: trends in properties and applications
23. Kim · 2014
24. Modeling of cavitation dynamics and interaction with material
25. ISO 4288 BE. BS EN ISO 4288 · 1988
26. ISO25178-2 BE. BS EN ISO 25178-2 · 2012
27. ISO 25178-3 BE. BS EN ISO 25178-3 · 2012
28. Introduction of a surface characterization parameter sdrprime for analysis of re-entrant features10.1007/s10921-019-0573-x ↗
29. Towards a new definition of areal surface texture parameters on freeform surface10.1016/j.measurement.2017.05.028 ↗
30. Stout · 1993 · 130
31. 1993 · 557
32. Abrasive flow machining: a case study10.1016/0924-0136(91)90210-6 ↗
33. A review of microscopic interactions between cavitation bubbles and particles in silt-laden flow10.1016/j.rser.2015.11.052 ↗
34. The synergistic effect of cavitation erosion and corrosion of nickel-aluminum copper surface layer on nickel-aluminum bronze alloy10.1016/j.jallcom.2018.03.103 ↗
35. Electropolishing of CuZn brasses and 316L stainless steels: influence of alloy composition or preparation process (ALM vs. standard method)10.1016/j.surfcoat.2016.08.076 ↗
36. Surface modification of Ti6Al4V open porous structures produced by additive manufacturing10.1002/adem.201100344 ↗
37. Chemical surface finishing of AlSi10Mg components made by additive manufacturing10.1016/j.mfglet.2018.12.002 ↗
38. Reducing surface roughness by chemical polishing of additively manufactured 3D printed 316 stainless steel components
39. Experimental study on finishing of internal laser melting (SLM) surface with abrasive flow machining (AFM)10.1016/j.precisioneng.2018.03.006 ↗
40. Study on improvement of surface roughness and induced residual stress for additively manufactured metal parts by abrasive flow machining10.1016/j.procir.2018.05.046 ↗
41. CFD-based study of the abrasive flow characteristics within constrained flow passage in polishing of complex titanium alloy surfaces10.1016/j.powtec.2018.04.046 ↗
42. Abrasive fluidized bed (AFB) finishing of AlSi10Mg substrates manufactured by direct metal laser sintering (DMLS)
43. Fluidised bed machining of metal additive manufactured parts
44. Progress in abrasive fluidized bed machining10.1016/j.jmatprotec.2009.04.009 ↗
45. Fluidized bed assisted abrasive jet machining (FB-AJM): precision internal finishing of inconel 718 components10.1115/1.2752831 ↗
46. Development of an abrasive jet machining system assisted by two fluidized beds for internal polishing of circular tubes10.1016/j.ijmachtools.2005.05.014 ↗
47. Progress in fluidized bed assisted abrasive jet machining (FB-AJM): internal polishing of aluminium tubes10.1016/j.ijmachtools.2006.06.005 ↗
48. Enhancing surface finish of additively manufactured titanium and cobalt chrome elements using laser based finishing10.1016/j.phpro.2016.08.021 ↗
49. Laser polishing of parts built up by selective laser sintering10.1016/j.ijmachtools.2007.01.013 ↗
50. Laser polishing of selective laser melted components10.1016/j.ijmachtools.2015.05.002 ↗
51. Laser polishing of additive manufactured 316L stainless steel synthesized by selective laser melting10.3390/ma12060991 ↗
52. A.P. Nagalingam, K.L. Tan, M.S. Vohra, W.L. Tan, S.H. Yeo, W. Arthur, Method and apparatus for finishing an internal channel of a component. Patent application no: US20190308292A1, Google Patents, 2019.
53. Multiphase hydrodynamic flow finishing for surface integrity enhancement of additive manufactured internal channels10.1016/j.jmatprotec.2020.116692 ↗
54. Development of an abrasive jet machining system assisted by two fluidized beds for internal polishing of circular tubes10.1016/j.ijmachtools.2005.05.014 ↗
55. CoCr F75 scaffolds produced by additive manufacturing: influence of chemical etching on powder removal and mechanical performance10.1016/j.jmbbm.2017.02.005 ↗
56. Overmelting and closing of thin horizontal channels in AlSi10Mg samples obtained by selective laser melting
57. Build direction effects on microchannel tolerance and surface roughness10.1115/1.4031071 ↗
58. A.P. Nagalingam, S.H. Yeo, A method and apparatus for finishing a surface of a component. Patent application no: GB1905215.8, (2019).
59. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
60. Fatigue life and microstructure of additive manufactured Ti6Al4V after different finishing processes10.1016/j.msea.2019.03.119 ↗
61. ASTM International · 2018