Effects of post-processing route on fatigue performance of laser powder bed fusion Inconel 718
Source abstract
Abstract
Abstract Fatigue performance of Inconel 718 (IN718) parts built using laser powder bed fusion (L-PBF) is often poorer than that of the cast and wrought alloy parts. This is because of detrimental effects arising from the microstructures such as brittle phases and anisotropy as well as porosities. To improve fatigue performance of L-PBF IN718, two types of post processes namely hot isostatic pressing (HIP) (performed at 980 °C, 100 MPa and 4 h) and shot peening (performed at 0.45 mmA intensity and 200 % coverage) were employed individually as well as sequentially on different specimens in addition to a standard processing route consisting of L-PBF build followed by solution annealing and double aging heat treatment. Porosities were considerably reduced by HIP-ing (from 0.39 % to 0.08 % porosity volume ratio) but this did not translate to improvements in fatigue performance. This can be attributed to the presence of inclusions and yield strength reduction resulting from γ” solutionisation. High compressive residual stresses of close to 1 GPa were recorded following shot peening regardless of whether HIP-ing was carried out prior to the shot peening. Improvement in fatigue lives particularly at high stress levels was observed on shot peened specimens without HIP-ing (H + SP) which can be explained by the compressive residual stresses that delay the onset of fatigue crack initiation. Shot peening applied on the HIP-ed specimens (H + HIP + SP) however, resulted in fatigue performance deterioration. This is related to the harmful tensile stresses that must exist alongside the compressive residual stresses in a shot peened surface, as evident from the location of the sub-surface crack initiations near the residual stress transition region approximately 300 μm from the free surface. In this case, detrimental effects arising from tensile stresses appear to have outweighed the benefits from compressive stresses on fatigue performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
2. Influence of defects and as-built surface roughness on fatigue properties of additively manufactured Alloy 71810.1016/j.msea.2018.08.072 ↗
3. Microstructural and texture development in direct laser fabricated IN71810.1016/j.matchar.2013.12.012 ↗
4. Studies of standard heat treatment effects on microstructure and mechanical properties of laser net shape manufactured INCONEL 71810.1007/s11661-009-9949-3 ↗
5. Influence of laser processing parameters on porosity in Inconel 718 during additive manufacturing10.1007/s00170-019-03655-9 ↗
6. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
7. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes
8. Influence of processing parameters on the evolution of melt pool, porosity, and microstructures in Ti-6Al-4V alloy parts fabricated by selective laser melting10.1007/s40964-017-0030-2 ↗
9. The effectiveness of hot isostatic pressing for closing porosity in titanium parts manufactured by selective electron beam melting10.1007/s11661-016-3429-3 ↗
10. On selective laser melting of Inconel 718: densification, surface roughness, and residual stresses10.1016/j.matdes.2020.108818 ↗
11. Effect of hatch length on the development of microstructure, texture and residual stresses in selective laser melted superalloy Inconel 71810.1016/j.matdes.2017.08.049 ↗
12. Effects of Selective Laser melting additive manufacturing parameters of Inconel 718 on porosity, microstructure and mechanical properties10.1016/j.msea.2018.08.037 ↗
13. Hot isostatic pressing of IN718 components manufactured by selective laser melting
14. Improvement in the Microstructure and Tensile Properties of Inconel 718 Superalloy by HIP Treatment10.2320/matertrans.47.2877 ↗
15. Microstructure and mechanical behavior of direct metal laser sintered Inconel alloy 71810.1016/j.matchar.2016.01.003 ↗
16. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
17. Post-processing of the Inconel 718 alloy parts fabricated by selective laser melting: Effects of mechanical surface treatments on surface topography, porosity, hardness and residual stress10.1016/j.surfcoat.2019.125136 ↗
18. Deep surface rolling for fatigue life enhancement of laser clad aircraft aluminium alloy10.1016/j.apsusc.2014.09.139 ↗
19. Improving the surface quality and mechanical properties by shot peening of 17-4 stainless steel fabricated by additive manufacturing10.1016/j.matdes.2016.08.037 ↗
20. On the effect of shot-peening on fatigue resistance of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting (AM-SLM)
21. Laser peening: a tool for additive manufacturing post-processing
22. Regain the fatigue strength of laser additive manufactured Ti alloy via laser shock peening10.1016/j.jallcom.2018.04.029 ↗
23. 3D laser shock peening – a new method for improving fatigue properties of selective laser melted parts
24. 3D laser shock peening – a new method for the 3D control of residual stresses in Selective Laser Melting10.1016/j.matdes.2017.05.083 ↗
25. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
26. Correlation of mechanical properties to microstructure in Inconel 718 fabricated by Direct Metal Laser Sintering10.1016/j.msea.2017.11.125 ↗
27. A review of mechanical properties of additively manufactured Inconel 718
28. Microstructure and directional fatigue behavior of Inconel 718 produced by selective laser melting10.1016/j.prostr.2016.06.298 ↗
29. Low cycle fatigue behaviour of direct metal laser sintered Inconel alloy 71810.1016/j.ijfatigue.2016.08.019 ↗
30. Microstructural influence on fatigue crack propagation during high cycle fatigue testing of additively manufactured Alloy 71810.1016/j.matchar.2019.01.018 ↗
31. Laser sintering of parts with complex internal structures
32. From powders to dense metal parts: characterization of a commercial AlSiMg alloy processed through direct metal laser sintering
33. Recrystallization and its influence on microstructures and mechanical properties of laser solid formed nickel base superalloy Inconel 71810.1007/s12598-011-0319-0 ↗
34. Microstructural characteristics of the nickel-based alloy IN738LC and the cobalt-based alloy Mar-M509 produced by selective laser melting10.1016/j.msea.2016.01.058 ↗
35. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment10.1016/j.matchar.2016.02.004 ↗
36. The influence of Laves phases on the high-cycle fatigue behavior of laser additive manufactured Inconel 71810.1016/j.msea.2017.03.098 ↗
37. Delta phase precipitation in Inconel 71810.1016/j.matchar.2004.07.004 ↗
38. The influence of Laves phases on the high-cycle fatigue behavior of laser additive manufactured Inconel 71810.1016/j.msea.2017.03.098 ↗
39. Structure, texture and phases in 3D printed IN718 alloy subjected to homogenization and HIP treatments
40. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
41. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
42. Residual stress evaluation in selective-laser-melting additively manufactured titanium (Ti-6Al-4V) and inconel 718 using the contour method and numerical simulation
43. Laser powder bed fusion of Inconel 718: residual stress analysis before and after heat treatment10.3390/met9121290 ↗
44. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments10.1016/j.msea.2017.12.043 ↗
45. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR100010.1016/j.actamat.2013.01.031 ↗
46. Evaluating surface deformation and near surface strain hardening resulting from shot peening a tempered martensitic steel and application to low cycle fatigue10.1016/j.ijfatigue.2013.03.019 ↗
47. Assessment of surface hardening effects from shot peening on a Ni-based alloy using electron backscatter diffraction techniques10.1016/j.actamat.2011.04.025 ↗
48. Effects of high-temperature deep rolling on fatigue, work hardening, and residual stress relaxation of martensitic stainless steel AISI 42010.1007/s11665-020-04656-6 ↗
49. Prevey · 1998
50. An analysis of fatigue failure mechanisms in an additively manufactured and shot peened IN 718 nickel superalloy10.1016/j.matdes.2020.108605 ↗