Enhanced strength and ductility of nano-TiBw-reinforced titanium matrix composites fabricated by electron beam powder bed fusion using Ti6Al4V–TiBw composite powder
Source abstract
Abstract
Abstract TiB whisker (TiBw)-reinforced Ti6Al4V (Ti64) based composite powder (as an alternative to premixed Ti64+TiB2 powders) was designed and produced via electrode induction melting gas atomization as the feedstock for electron beam powder bed fusion (EB-PBF), to synthesize nanosized TiBw reinforced Ti64 based composites with a quasi-continuous network microstructure and well-matched strength and ductility. To understand the interactions among the TiBw morphology, microstructures and mechanical properties, the phase composition, microstructural orientation, interface relationships, tensile properties, and fracture mechanism were investigated systematically. The formation of a quasi-continuous network in the microstructure, with nanosized TiBw distributed along the grain boundary, is primarily attributed to the high cooling rates and low solid solubility of boron in the Ti matrix. In addition, the (102) plane of α-Ti and the cylindrical plane of the nanosized TiBw had a semi-coherent interface, whereas the transverse face of the TiBw had an incoherent interface with the Ti matrix in the EB-PBF-fabricated Ti64–TiBw composites. The ultimate tensile strength of EB-PBF-fabricated Ti64–TiBw composites reached 1121 MPa, which is 27% higher than that of the EB-PBF-fabricated Ti64 alloy, and the elongation after fracture remains at 8.9%, which is 82% remarkable higher than that of forged composites with the same TiBw volume content. This study provides a novel strategy for producing Ti matrix composites with matched high strength–ductility by additive manufacturing employing Ti-based composite powder as the feedstock.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Multiscale architecture and superior high-temperature performance of discontinuously reinforced titanium matrix composites
2. Titanium metal matrix composites: an overview10.1016/j.compositesa.2019.04.005 ↗
3. Comparative investigation on microstructures and mechanical properties of (TiB+TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems10.1016/j.matchar.2018.04.010 ↗
4. Hot deformation behavior of nano-sized TiB reinforced Ti-6Al-4V metal matrix composites10.1016/j.mechmat.2019.103260 ↗
5. Reactive-deposition-based additive manufacturing of Ti-Zr-BN composites
6. Pool geometry and microstructure of Ti6Al4V with B additions processed by selective laser melting additive manufacturing10.1016/j.matdes.2019.108126 ↗
7. Embedding boron into Ti powder for direct laser deposited titanium matrix composite: Microstructure evolution and the role of nano-TiB network structure10.1016/j.compositesb.2021.108683 ↗
8. Microstructurally inhomogeneous composites: is a homogeneous reinforcement distribution optimal?10.1016/j.pmatsci.2015.01.002 ↗
9. Selective laser melting additive manufacturing of Ti-based nanocomposites: the role of nano powder10.1007/s11661-013-1968-4 ↗
10. Balance of strength and plasticity of additive manufactured Ti-6Al-4V alloy by forming TiB whiskers with cyclic gradient distribution
11. Controlling the microstructure and properties of wire arc additive manufactured Ti-6Al-4V with trace boron additions10.1016/j.actamat.2015.03.035 ↗
12. Manufacturing of a nanosized TiB strengthened Ti-based alloy via electron beam powder bed fusion
13. Selective laser melting of in situ titanium-titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
14. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
15. Influence of spark plasma sintering and subsequent hot rolling on microstructure and flexural behavior of in-situ TiB and TiC reinforced Ti6Al4V composite10.1016/j.msea.2014.11.036 ↗
16. Mechanical properties of Ti-6Al-4V/TiB composites with randomly oriented and aligned TiB reinforcements10.1016/S1359-6454(02)00510-4 ↗
17. Microstructure and mechanical properties of P/M titanium matrix composites reinforced by in-situ synthesized TiC-TiB10.1016/j.msea.2015.01.033 ↗
18. Effects of boron additions and solutioning treatments on microstructures and ductility of forged Ti-6Al-4V alloys10.1016/j.jallcom.2014.11.008 ↗
19. Selective laser melting of nanocomposite Ti-6Al-4V and TiC powder10.4028/www.scientific.net/KEM.822.575 ↗
20. Progress in additive manufacturing on new materials: a review10.1016/j.jmst.2018.09.002 ↗
21. Additive manufacturing of metal matrix composites,
22. Strengthening of stainless steel by titanium carbide addition and grain refinement during selective laser melting10.1016/j.msea.2017.11.126 ↗
23. Microstructural evolution, mechanical and tribological properties of TiC/Ti6Al4V composites with unique microstructure prepared by SLM10.1016/j.msea.2021.141187 ↗
24. Effect of Cu content on microstructure and mechanical properties of in-situ phases reinforced Ti/Zr-based bulk metallic glass matrix composite by selective laser melting (SLM)10.1016/j.jmst.2020.06.024 ↗
25. Super-high-strength graphene/titanium composites fabricated by selective laser melting10.1016/j.carbon.2020.12.047 ↗
26. Selective laser melting of CP-Ti to overcome the low cost and high-performance trade-off
27. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting10.1016/j.compositesb.2020.108567 ↗
28. Refined microstructure and enhanced wear resistance of titanium matrix composites produced by selective laser melting10.1016/j.optlastec.2020.106644 ↗
29. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
30. Achieving near equiaxed α-Ti grains and significantly improved plasticity via heat treatment of TiB reinforced titanium matrix composite manufactured by selective laser melting10.1016/j.jallcom.2020.155344 ↗
31. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti-6Al-4V and TiB/Ti-6Al-4V composite: a comparative study10.1016/j.msea.2020.140415 ↗
32. Selective laser melting of in situ TiB/Ti6Al4V composites: formability, microstructure evolution and mechanical performance10.1007/s40195-020-01021-3 ↗
33. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: a state of the art review10.1016/j.pmatsci.2019.04.006 ↗
34. Effect of powder particle shape on the properties of in situ Ti-TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
35. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: microstructure evolution and tribological behavior10.1016/j.powtec.2018.09.088 ↗
36. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB/TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
37. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders
38. In situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
39. High-temperature microstructure stability and fracture toughness of TiAl alloy prepared via electron beam smelting and selective electron beam melting10.1016/j.intermet.2021.107259 ↗
40. In situ characterization of a high work hardening Ti-6Al-4V prepared by electron beam melting10.1016/j.actamat.2019.08.037 ↗
41. H.Z. Niu, B.G. Yin, H.R. Zhang, M.C. Zang, H. Tan, D.L. Zhang, Multiphase polymorphic nanoparticles reinforced titanium matrix composite produced by selective electron beam melting of a prealloyed composite powder, Scripta Mater. 〈https://doi.org/10.1016/j.scriptamat.2021.113916〉.10.1016/j.scriptamat.2021.113916 ↗
42. Structural investigation of selective laser melting and electron beam melting of Ti-6Al-4V using neutron diffraction
43. TiB nano-whiskers reinforced titanium matrix composites with novel nano-reticulated microstructure and high performance via composite powder by selective laser melting10.1016/j.msea.2020.140137 ↗
44. Characteristics and atomization behaviour of Ti-6Al- 4V powder produced by plasma rotating electrode process10.1016/j.apt.2019.07.015 ↗
45. Metrological characterization of X-ray diffraction methods at different acquisition geometries for determination of crystallite size in nano-scale materials10.1016/j.matchar.2013.09.002 ↗
46. Hot deformation behavior of nano-sized TiB reinforced Ti-6Al-4V metal matrix composites10.1016/j.mechmat.2019.103260 ↗
47. The mechanical behavior dependence on the TiB whisker realignment during hot-working in titanium matrix composites
48. Precipitation and distribution behavior of in situ-formed TiB whiskers in Ti64 composites fabricated by selective laser melting10.3390/cryst11040374 ↗
49. Synthesis of ductile titanium-titanium boride (Ti-TiB) composites with a beta-titanium matrix: The nature of TiB formation and composite properties10.1007/s11661-003-0249-z ↗
50. The kinetics and mechanism of interfacial reaction in sigma fibre-reinforced Ti MMCs10.1016/S1359-835X(96)00105-4 ↗
51. Direct laser deposition of in situ Ti-6Al-4V-TiB composites10.1016/S0921-5093(03)00299-5 ↗
52. Effects of heat treatments on the microstructure and mechanical properties of as-extruded TiBw/Ti6Al4V composites10.1016/j.msea.2012.08.071 ↗
53. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition10.1016/j.matdes.2019.108191 ↗
54. Nanoscale TiB precipitates in laser deposited Ti-matrix composites10.1016/j.scriptamat.2005.08.014 ↗
55. Nucleation and growth of α-Ti on TiB precipitates in Ti-15Mo-2.6Nb-3Al-0.2Si-0.12B10.1080/14786435.2010.533134 ↗
56. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
57. Influence of lattice misfit on the deformation behaviour of α2/γ lamellae in TiAl alloys10.1016/j.msea.2020.140053 ↗
58. Paul · 2014
59. Revisiting the Considère criterion from the viewpoint of dislocation theory fundamentals10.1016/j.scriptamat.2013.12.009 ↗
60. Effects of volume fraction on the microstructure and tensile properties of in situ TiBw/Ti6Al4V composites with novel network microstructure10.1016/j.matdes.2012.09.043 ↗
61. Direct laser fabrication of Ti6Al4V/TiB10.1016/j.jmatprotec.2007.05.024 ↗
62. In situ (TiBw+TiCp)/Ti6Al4V composites with a network reinforcement distribution10.1016/j.msea.2010.07.025 ↗
63. High-mass-proportion TiCp/Ti6Al4V titanium matrix composites prepared by directed energy deposition
64. Effect of extrusion dies angle on the microstructure and properties of (TiB-TiC)/Ti6Al4V in situ titanium matrix composite10.1016/j.msea.2016.05.021 ↗
65. Influence of trace boron addition on microstructure, tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
66. Effect of beam power on the distribution statues of aligned TiBw and tensile behavior of trace boron-modified Ti6Al4V alloy produced by electron beam freeform fabrication10.1016/j.vacuum.2019.109070 ↗
67. Reinforcements stimulated dynamic recrystallization behavior and tensile properties of extruded (TiB+TiC+La2O3)/Ti6Al4V composites10.1016/j.jallcom.2016.12.418 ↗
68. Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys10.1016/j.actamat.2007.05.009 ↗
69. Effects of direct rolling deformation on the microstructure and tensile properties of the 2.5 vol% (TiBw+TiCp)/Ti composites10.1016/j.msea.2016.12.113 ↗
70. The elevated-temperature fatigue behavior of boron-modified Ti-6Al-4V (wt%) castings10.1016/j.msea.2008.04.004 ↗
71. Effects of boron on the fracture behavior and ductility of cast Ti-6Al-4V alloys10.1016/j.scriptamat.2014.12.022 ↗
72. Boron modified titanium alloys10.1016/j.pmatsci.2020.100653 ↗
73. Tensile properties of fibre-reinforced metals: copper/tungsten and copper/molybdenum
74. On the strength of discontinuous silicon carbide reinforced aluminum composites10.1016/0036-9748(86)90210-3 ↗
75. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: a model for predicting their yield strength10.1016/j.scriptamat.2005.12.017 ↗