journal article·2022-12

Laser powder bed fusion of nano-titania modified 2219 aluminium alloy with superior mechanical properties at both room and elevated temperatures: The significant impact of solute

Gan Li, Yuhe Huang, Xinwei Li, Chuan Guo, Qiang Zhu, Jian Lu

Publisher page

Abstract

There is a strong demand for facile and cost-effective approaches for additive manufacturing (AM) of aluminium (Al) alloy parts with high mechanical properties at both room and elevated temperatures via laser powder bed fusion (L-PBF). Such alloys must be devoid of cracks and large pores while exhibiting excellent mechanical performance. In this study, we demonstrated that the addition of 1 wt% titania (TiO2) nanoparticles to a 2219 Al alloy could substantially prevent hot-crack formation during L-PBF by significantly refining grains, which resulted in the formation of a nearly fully dense alloy with a high relative density (99.97%). This pronounced grain refinement was due to the solute effect of the Ti element with a high grain growth restriction factor (Q value) instead of the in-situ formation of lattice-matched L12-ordered Al3Ti particles. The processed alloy displayed an excellent combination of high ultimate tensile strength and elongation at both room and elevated temperatures, with these properties being comparable to those of its wrought counterpart and greater than those of 2219 Al alloys fabricated via other AM techniques. This low-cost pathway can also be applied to the AM of other Al alloys, which demonstrates its commercial significance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Liu · Mater. Sci. Eng. R. · 2021 · 14510.1016/j.mser.2020.100596 ↗
2. Additive manufacturing of metals: microstructure evolution and multistage control10.1016/j.jmst.2021.06.011 ↗
3. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
4. Current progress in rheoforming of wrought aluminum alloys: A review10.3390/met10020238 ↗
5. A review of Laser Powder Bed Fusion Additive Manufacturing of aluminium alloys: Microstructure and properties
6. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
7. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
8. Microstructure, solidification behavior and mechanical properties of Al–Si–Mg–Ti/TiC fabricated by selective laser melting
9. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
10. A high strength Al–Li alloy produced by laser powder bed fusion: Densification, microstructure, and mechanical properties
11. Investigation into the effect of energy density on densification, surface roughness and loss of alloying elements of 7075 aluminium alloy processed by laser powder bed fusion10.1016/j.optlastec.2021.107621 ↗
12. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
13. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
14. Facile and cost-effective approach to additively manufacture crack-free 7075 aluminum alloy by laser powder bed fusion10.1016/j.jallcom.2022.167097 ↗
15. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
16. Grain refinement mechanisms in additively manufactured nano-functionalized aluminum10.1016/j.actamat.2020.09.043 ↗
17. Microstructure, mechanical properties, aging behavior, and corrosion resistance of a laser powder bed fusion fabricated Al–Zn–Mg–Cu–Ta alloy10.1016/j.msea.2021.142364 ↗
18. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
19. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
20. Dependence of mechanical properties and microstructure on solidification onset temperature for Al2024–CaB6 alloys processed using laser powder bed fusion10.1016/j.msea.2021.142552 ↗
21. Shakil · Mater. Sci. Eng. A · 2022 · 83210.1016/j.msea.2021.142453 ↗
22. Shakil · Micron · 2022 · 15610.1016/j.micron.2022.103246 ↗
23. Correlation between tensile properties, microstructure, and processing routes of an Al–Cu–Mg–Ag–TiB2 (A205) alloy: Additive manufacturing and casting10.1016/j.msea.2022.142989 ↗
24. On the microstructure and solidification behavior of new generation additively manufactured Al-Cu-Mg-Ag-Ti-B alloys
25. Novel approach to additively manufacture high-strength Al alloys by laser powder bed fusion through addition of hybrid grain refiners
26. A high-strength heat-resistant Al−5.7Ni eutectic alloy with spherical Al3Ni nano-particles by selective laser melting10.1016/j.scriptamat.2021.114034 ↗
27. Al-Cu-Ce(-Zr) alloys with an exceptional combination of additive processability and mechanical properties
28. Davis · 1993
29. S. Lakra, T.K. Bandyopadhyay, S. Das, K. Das, In situ dual matrix composite with segregated microstructure fabricated from Al–TiO2–B2O3 system by mechanical thermal process, 860 (2021) 158527, https://doi.org/10.1016/j.jallcom.2020.158527.10.1016/j.jallcom.2020.158527 ↗
30. Selective laser melting of a high strength AlMnSc alloy: Alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
31. Controlling process instability for defect lean metal additive manufacturing10.1038/s41467-022-28649-2 ↗
32. High power selective laser melting (HP-SLM) of aluminum parts10.1016/j.phpro.2011.03.035 ↗
33. Composition change of stainless steels during keyhole mode laser welding
34. Sieverts law pressure exponent for hydrogen permeation through Pd-based membranes: Coupled influence of non-ideal diffusion and multicomponent external mass transfer10.1016/j.ijhydene.2013.09.102 ↗
35. Formation mechanism of TiC–Al2O3 ceramic reinforcements and the influence on the property of ZL101 composites10.1016/j.ceramint.2021.10.040 ↗
36. Combustion synthesis of metal-matrix composites: Part I, the Ti-TiC-Al2O3 system10.1016/1359-6462(95)00447-5 ↗
37. Energy efficiency during conventional and novel sintering processes: the case of Ti–Al2O3–TiC composites10.1016/j.jclepro.2009.01.012 ↗
38. Effective Formation of Oxygen Vacancies in Black TiO2 Nanostructures with Efficient Solar-Driven Water Splitting10.1021/acssuschemeng.7b01774 ↗
39. Ye · 2002
40. A predictive equation for solute diffusivity in liquid metals10.1016/j.scriptamat.2006.04.019 ↗
41. On the role of atmospheric oxygen into mechanical properties and fracture behavior of selective laser melted AlCu5MnCdVA10.1016/j.matdes.2018.04.003 ↗
42. A hidden precipitation scenario of the θ′-phase in Al-Cu alloys10.1016/j.jmst.2020.09.039 ↗
43. Atomic-scale mechanism of the θ″ → θ′ phase transformation in Al-Cu alloys10.1016/j.jmst.2016.08.031 ↗
44. The enhanced theta-prime (θ′) precipitation in an Al-Cu alloy with trace Au additions10.1016/j.actamat.2016.12.012 ↗
45. Tension-compression asymmetry of stress-relaxation ageing behavior of AA2219 alloy over a wide range of stress levels10.1016/j.msea.2021.141730 ↗
46. Towards understanding metallurgical defect formation of selective laser melted wrought aluminum alloys
47. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
48. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
49. The interdependence theory: The relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
50. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles10.1007/s11661-005-0054-y ↗
51. Demonstrating the roles of solute and nucleant in grain refinement of additively manufactured aluminium alloys
52. Development of a high strength Zr/Sc/Hf-modified Al-Mn-Mg alloy using Laser Powder Bed Fusion: Design of a heterogeneous microstructure incorporating synergistic multiple strengthening mechanisms
53. Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys
54. Microstructure evolution and mechanical properties of the wire + arc additive manufacturing Al-Cu alloy
55. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
56. External filler wire based GMA-AM process of 2219 aluminum alloy10.1080/10426914.2020.1779936 ↗
57. The heterogeneous band microstructure and mechanical performance in a wire + arc additively manufactured 2219 Al alloy
58. Microstructure and mechanical properties of 2219 aluminum alloy fabricated by double-electrode gas metal arc additive manufacturing
59. Effect of Fe addition on heat-resistant aluminum alloys produced by selective laser melting10.3390/met9040468 ↗
60. Thermal stability of aluminum alloys