Influence of friction stir processing and aging heat treatment on microstructure and mechanical properties of selective laser melted Mg-Gd-Zr alloy
Source abstract
Abstract
Abstract The low ductility of Mg alloy fabricated by selective laser melting (SLM) technique usually restricts its application in several fields. Friction stir processing (FSP) is a promising post-treatment method to solve this problem. A detailed study of how FSP affect pore defects, molten pool boundary, grain morphology, aging precipitates and mechanical properties of SLMed Mg-10Gd-0.2Zr (G10K, wt.%) alloy was conducted. The results show that FSP can lead to porosity reduction from 0.779% to 0.015%, vanishment of molten pool boundary, columnar to equiaxed transition and grain refinement. Thus, a significant enhancement of room temperature tensile properties is reported with a remarkable increase of elongation (EL) from 2.2% to 7.5% without the sacrifice of strength after FSP (while yield strength (YS) and ultimate tensile strength (UTS) increased from 180 MPa, 228 MPa to 202 MPa, 272 MPa respectively). After peak aging heat treatment, the plate aspect ratio and area number density of β' aging precipitates in the FSP-T5 G10K alloy are higher than those of SLM-T5 G10K alloy, resulting in a stronger aging hardening response (hardness increment 28.3 HV versus 22.7 HV). As a result, the FSP-T5 G10K alloy exhibits YS of 285 MPa, UTS of 356 MPa and EL of 1.3%, while those of the SLM-T5 G10K alloy are only 243 MPa, 260 MPa and 0.3%. These findings demonstrate that FSP is very effective for modifying microstructure and enhancing mechanical properties of the SLMed alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Research progress on selective laser melting (SLM) of magnesium alloys: a review10.1016/j.ijleo.2019.163842 ↗
2. A review of SLMed magnesium alloys: processing, properties, alloying elements and postprocessing10.3390/met10081073 ↗
3. Additive manufacturing of magnesium alloys
4. Mg bone implant: features, developments and perspectives10.1016/j.matdes.2019.108259 ↗
5. The potential of SLM technology for processing magnesium alloys in aerospace industry10.1007/s43452-020-00033-1 ↗
6. Microstructure evolution and texture tailoring of reduced graphene oxide reinforced Zn scaffold
7. Latest research advances on magnesium and magnesium alloys worldwide10.1016/j.jma.2020.02.003 ↗
8. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment10.1016/j.msea.2013.10.023 ↗
9. Fabrication of high-strength Mg-Gd-Zn-Zr alloy via selective laser melting10.1016/j.matchar.2020.110377 ↗
10. Additive manufactured WE43 magnesium: a comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE4310.1016/j.matchar.2018.11.011 ↗
11. Effect of energy input on formability, microstructure and mechanical properties of selective laser melted AZ91D magnesium alloy10.1016/j.msea.2014.05.092 ↗
12. Influence of laser process parameters on the densification, microstructure, and mechanical properties of a selective laser melted AZ61 magnesium alloy10.1016/j.jallcom.2019.06.261 ↗
13. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion
14. Study of pore defect and mechanical properties in selective laser melted Ti6Al4V alloy based on X-ray computed tomography10.1016/j.msea.2020.139981 ↗
15. Ductilisation and fatigue life enhancement of selective laser melted AlSi10Mg by friction stir processing10.1016/j.scriptamat.2019.05.044 ↗
16. An overview of residual stresses in metal powder bed fusion
17. Selective laser melting of magnesium and magnesium alloy powders: a review10.3390/met7010002 ↗
18. Comparative study of fatigue properties of Ti-6Al-4V specimens built by electron beam melting (EBM) and selective laser melting (SLM)10.1016/j.matchar.2018.03.028 ↗
19. Influence of hot isostatic pressing (HIP) on mechanical properties of magnesium alloy produced by selective laser melting (SLM)10.1016/j.matlet.2020.127463 ↗
20. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
21. Microstructure, texture and mechanical properties of friction stir processed Mg-14Gd alloys10.1016/j.matdes.2017.05.046 ↗
22. Enhancing mechanical properties of AZ61 magnesium alloy via friction stir processing: Effect of processing parameters10.1016/j.msea.2020.139945 ↗
23. Effects of friction stir process and subsequent aging treatment on the microstructure evolution and mechanical properties of Mg-Gd-Y-Zn-Zr alloy10.1016/j.matchar.2019.109832 ↗
24. Modification of long period stacking ordered phase and improvement of mechanical properties of Mg–Gd–Zn–Zr alloy by friction stir processing10.1016/j.matlet.2013.09.054 ↗
25. Ductilization of selective laser melted Ti6Al4V alloy by friction stir processing10.1016/j.msea.2019.03.133 ↗
26. A detailed HAADF-STEM study of precipitate evolution in Mg–Gd alloy10.1016/j.jallcom.2018.10.193 ↗
27. Effects of nanoprecipitates and LPSO structure on deformation and fracture behaviour of high-strength Mg-Gd-Y-Zn-Mn alloys10.1016/j.matchar.2020.110396 ↗
28. Selective variant growth of precipitates in an as-extruded Mg-Gd-Zn-Mn alloy10.1016/j.matlet.2020.127853 ↗
29. Ductilization of aluminium alloy 6056 by friction stir processing10.1016/j.actamat.2017.01.047 ↗
30. Microstructure and mechanical properties of selective laser melted Mg-9wt%Al powder mixture10.1016/j.matlet.2018.03.068 ↗
31. Laser additive manufacturing of biodegradable magnesium alloy WE43: a detailed microstructure analysis10.1016/j.actbio.2019.05.056 ↗
32. A study of microstructure, mechanical behavior and strengthen mechanism in the Mg-10Gd-0.2Zn-(Y)-0.4Zr alloy10.1016/j.msea.2020.139881 ↗
33. Microstructure evolution and fracture behavior of Mg-9.5Gd-0.9Zn-0.5Zr alloy subjected to different heat treatments10.1016/j.matchar.2020.110516 ↗
34. Characterization and strengthening effects of γ′ precipitates in a high-strength casting Mg-15Gd-1Zn-0.4Zr (wt%) alloy10.1016/j.matchar.2017.02.010 ↗
35. The Interdependence Theory: The relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
36. Development of high strength sand cast Mg–Gd–Zn alloy by co-precipitation of the prismatic β′ and β1 phases10.1016/j.matchar.2019.04.036 ↗
37. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
38. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
39. A super high-strength Mg-Gd-Y-Zn-Mn alloy fabricated by hot extrusion and strain aging10.1016/j.matdes.2019.107666 ↗
40. On the ductility of magnesium based materials: a mini review10.1016/j.jallcom.2019.04.031 ↗