journal article·2022-06Open access

Cracking behaviour of high-strength AA2024 aluminium alloy produced by Laser Powder Bed Fusion

G. Del Guercio, D.G. McCartney, N.T. Aboulkhair, S. Robertson, R. Maclachlan, C. Tuck, M. Simonelli

Abstract

Most wrought aluminium alloys of the 2000 series are difficult to manufacture by laser powder bed fusion (L-PBF) due to the formation of cracks during building. To date, the effects of processing regimes on crack formation are still not well understood. In this study we performed a detailed microstructural characterisation of crack development in the AlCuMg alloy AA2024 to quantify the extent of cracking and porosity arising from a range of different process parameters. Two samples, produced with different build parameters, were selected for in-depth study by scanning and transmission electron microscopy; these had similar low levels of porosity but high (H - 2.6 ± 0.4 mm/mm2) and low (L - 1.5 ± 0.3 mm/mm2) crack densities respectively. Based on distinct morphological features and characteristic length, we differentiate hot cracks from solid state cracks. Hot tears form at high angle grain boundaries and are associated with micron-sized gas pores as well as intermetallic phases in both samples. The solidification and cracking behaviour are modelled with the aid of a Scheil-Gulliver model that includes solute trapping. This approach predicts differences in hot-crack-susceptibilities, due to different solidification velocities, in line with experimental observations. The sample H, of high crack density, also experiences the higher cooling rate, and hence strain rate, which contributes to the greater propagation of cold cracks in the low fracture toughness AA2024. The observation of cracking associated with microporosity and the use of a Scheil-based solidification model, including solute trapping, provide new insights into the complex problem of hot tearing during L-PBF.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Metal alloys for fusion-based additive manufacturing10.1002/adem.201700952 ↗
3. Metallurgy of high-silicon steel parts produced using Selective Laser Melting10.1016/j.actamat.2016.03.037 ↗
4. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using Selective Laser Melting10.1016/j.pmatsci.2019.100578 ↗
5. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
6. Formation of metastable cellular microstructures in selective laser melted alloys10.1016/j.jallcom.2016.12.209 ↗
7. Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting10.1016/j.scriptamat.2019.04.036 ↗
8. A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting
9. Comparison of microstructure and mechanical properties of Scalmalloy® produced by selective laser melting and laser metal deposition10.3390/ma11010017 ↗
10. Process and mechanical properties: applicability of a scandium modified Al-alloy for laser additive manufacturing10.1016/j.phpro.2011.03.047 ↗
11. Microstructure and mechanical properties of as-processed scandium-modified aluminium using selective laser melting10.1016/j.cirp.2016.04.057 ↗
12. Selective laser melting of rare earth element Sc modified aluminum alloy: Thermodynamics of precipitation behavior and its influence on mechanical properties
13. The effect of scandium on the microstructure, mechanical properties and weldability of a cast Al-Mg alloy10.1016/S1359-6454(02)00259-8 ↗
14. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
15. Towards a high strength aluminium alloy development methodology for selective laser melting10.1016/j.matdes.2019.107775 ↗
16. An integrated computational materials engineering-anchored closed-loop method for design of aluminum alloys for additive manufacturing10.1016/j.mtla.2019.100574 ↗
17. Columnar to equiaxed transition in Al-Mg(-Sc)-Zr alloys produced by selective laser melting10.1016/j.scriptamat.2017.10.021 ↗
18. Effect of platform temperature on the porosity, microstructure and mechanical properties of an Al–Mg–Sc–Zr alloy fabricated by selective laser melting10.1016/j.msea.2018.06.049 ↗
19. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
20. Inoculation Treatment of an Additively Manufactured 2024 Aluminium Alloy with Titanium Nanoparticles
21. Selective laser melting of AlCu-TiB2 alloy using pulsed wave laser emission mode: processability, microstructure and mechanical properties10.1016/j.matdes.2021.109628 ↗
22. Association · 1984
23. On the corrosion of additively manufactured aluminium alloy AA2024 prepared by selective laser melting10.1016/j.corsci.2018.08.019 ↗
24. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
25. Laser powder bed fusion of nano-CaB6 decorated 2024 aluminum alloy10.1016/j.jallcom.2021.158714 ↗
26. Grain structure evolution of Al-Cu alloys in powder bed fusion with laser beam for excellent mechanical properties
27. Comparing Xe+pFIB and Ga+FIB for TEM sample preparation of Al alloys: Minimising FIB-induced artefacts
28. Thermo-Calc & DICTRA, computational tools for materials science
29. Thermo-Calc, TCAL6: TCS Al-based Allot Database, (2019). https://thermocalc.com/products/databases/aluminum-based-alloys/.
30. Influence of process parameters on the quality of aluminium alloy en AW 7075 using Selective Laser Melting (SLM)10.1016/j.phpro.2016.08.096 ↗
31. Signatures of the unique microstructure of additively manufactured steel observed via diffraction10.1016/j.scriptamat.2018.06.008 ↗
32. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by Laser-Based Powder Bed Fusion10.1007/s11661-020-06073-9 ↗
33. S. Kou, Welding metallurgy, New Jersey, USA. (2003) 431–446.10.1002/0471434027 ↗
34. Messler · 2008
35. Reducing porosity in AlSi10Mg parts processed by selective laser melting
36. Welding metallurgy10.1007/978-1-349-10624-0_4 ↗
37. In search of the prediction of hot cracking in aluminium alloys
38. Bemerkungen zur schichtkristallbildung10.1515/ijmr-1942-340303 ↗
39. Solute trapping and solute drag in a phase-field model of rapid solidification10.1103/PhysRevE.58.3436 ↗
40. Model for solute redistribution during rapid solidification10.1063/1.329867 ↗
41. An atomistic model of solute trapping
42. Continuous growth model for interface motion during alloy solidification10.1016/0001-6160(88)90333-1 ↗
43. Stability of cellular microstructure in laser powder bed fusion of 316L stainless steel10.1016/j.msea.2018.10.051 ↗
44. Rapid solidification of lightweight metal alloys10.1016/0921-5093(89)90082-8 ↗
45. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
46. T.W. Clyne, C. TW, The influence of composition on solidification cracking susceptibility in binary alloy systems, (1981).
47. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
48. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗
49. A simple index for predicting the susceptibility to solidification cracking
50. Mechanisms for solidification crack initiation and growth in aluminum welding10.1007/s11661-009-9964-4 ↗
51. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
52. Analytical description of the influence of the welding parameters on the hot cracking susceptibility of laser beam welds in aluminum alloys10.1007/s11661-019-05430-7 ↗
53. Crack-free aluminium alloy welds using a twin laser process
54. Rapid solidification: selective laser melting of AlSi10Mg10.1007/s11837-015-1763-3 ↗
55. The effect of cooling rate on the dendrite spacing in splat-cooled aluminium alloys
56. Effects of process conditions on the mechanical behavior of aluminium wrought alloy EN AW-2219 (AlCu6Mn) additively manufactured by laser beam melting in powder bed10.3390/mi8010023 ↗
57. Selective laser melting of high strength Al-Cu-Mg alloys: Processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
58. Microstructure and mechanical properties of a heat-treatable Al-3.5Cu-1.5Mg-1Si alloy produced by selective laser melting10.1016/j.msea.2017.11.063 ↗
59. TearSim: a two-phase model addressing hot tearing formation during aluminum direct chill casting10.1007/s11661-006-0188-6 ↗
60. VI. The phenomena of rupture and flow in solids
61. Fracture and strength of solids10.1088/0034-4885/12/1/309 ↗
62. Mechanical properties of materials
63. Materials selection in mechanical design
64. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
65. L.A. Parry, Investigation of Residual Stress, (n.d.).
66. An improved prediction of residual stresses and distortion in additive manufacturing10.1016/j.commatsci.2016.10.003 ↗
67. Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting10.2351/1.4828755 ↗
68. Reducing hot tearing by grain boundary segregation engineering in additive manufacturing: example of an AlxCoCrFeNi high-entropy alloy10.1016/j.actamat.2020.116505 ↗
69. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron beam melting10.1016/j.actamat.2017.09.047 ↗
70. On the influence of alloy chemistry and processing conditions on additive manufacturability of Ni-based superalloys
71. Microstructures and tensile properties of a selective laser melted Al–Zn–Mg–Cu (Al7075) alloy by Si and Zr microalloying10.1016/j.msea.2020.139492 ↗
72. Evaluation of the effect of rare earth alloying additions on the hot tearing susceptibility of aluminum alloy 7150 during rapid solidification10.1007/s11661-020-05930-x ↗
73. Microstructural features and mechanical properties of artificially aged AA202410.1007/s11223-013-9504-8 ↗