Abstract
Additively manufactured Ti6Al4V are high strength alloys but associated with inferior ductility and inherent defects. These process-induced defects act as a stress raiser and deteriorates the mechanical and fatigue properties of the alloy. Post-processing is generally done to enhance the ductility and fatigue properties but at the expense of strength of the additively manufactured Ti6Al4V alloy. In this study, the effect of defects on mechanical properties and fatigue performance of additively manufactured (selective laser melting) Ti6Al4V alloy has been investigated based on experimentally calibrated defects-based model. The as-built specimens were subjected to different heat treatments in order to optimize their mechanical properties and the most optimum heat treatment was then selected for investigation of changes in fatigue properties. The beneficial effect of heat treatment on mechanical properties was mainly associated with the reduction in fraction of α ’-martensitic microstructure and increase in α -lamellae thickness. Most of the fatigue failures occurred from surface and sub-surface defects, owing to the high stress concentration factor associated with them, and improved fatigue lives as a result of optimum heat treatment. A process–structure–property (PSP) linkage has been established to predict the mechanical properties. Experimentally calibrated defects’ based fatigue model has been formulated to predict the fatigue performance using the experimentally observed data i.e. the process induced defects’ size and their locations.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects10.1016/j.ijfatigue.2019.105358 ↗
2. Surface chemistry of Ti6Al4V components fabricated using selective laser melting for biomedical applications10.1016/j.msec.2016.05.054 ↗
3. Consolidation phenomena in laser and powder-bed based layered manufacturing10.1016/j.cirp.2007.10.004 ↗
4. A study on the residual stress during selective laser melting (SLM) of metallic powder10.1007/s00170-016-8466-y ↗
5. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
6. A review on high-strength titanium alloys: microstructure, strengthening, and properties
7. A comparative study of corrosion resistance of biocompatible coating on titanium alloy and stainless steel10.1016/j.matchemphys.2019.121923 ↗
8. Electrochemical study of three stainless steel alloys and titanium metal in cola soft drinks10.33961/JECST.2017.8.4.294 ↗
9. Biocompatibility and biological corrosion resistance of Ti–39Nb–6Zr+ 0.45 Al implant alloy10.3390/jfb12010002 ↗
10. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
11. OpenGGCM simulations for the THEMIS mission10.1007/s11214-008-9421-5 ↗
12. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
13. Martensite formation and decomposition during traditional and AM processing of two-phase titanium alloys—An overview10.3390/met11030481 ↗
14. The martensitic transformation and mechanical properties of Ti6Al4V prepared via selective laser melting10.3390/ma12020321 ↗
15. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
16. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
17. Controlling martensitic decomposition during selective laser melting to achieve best ductility in high strength Ti-6Al-4V10.1016/j.msea.2018.12.047 ↗
18. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
19. Residual stress analysis of additive manufacturing of metallic parts using ultrasonic waves: State of the art review10.1016/j.jmrt.2020.05.092 ↗
20. Surface texture metrology for metal additive manufacturing: a review10.1016/j.precisioneng.2016.06.001 ↗
21. Defects and anomalies in powder bed fusion metal additive manufacturing10.1016/j.cossms.2021.100974 ↗
22. Kim · 2018
23. Defect-based fatigue life prediction of L-PBF additive manufactured metals10.1016/j.engfracmech.2021.107541 ↗
24. Surface versus internal fatigue crack initiation in steel: Influence of mean stress10.1016/j.ijfatigue.2015.08.028 ↗
25. A study on fatigue behavior of MIG-welded Al-Mg alloy with different filler-wire materials under mean stress10.1016/j.ijfatigue.2017.11.001 ↗
26. Effect of biaxial cyclic tension on the fatigue life and damage mechanisms of Cr–Mo steel10.1016/j.ijfatigue.2016.01.021 ↗
27. Very-high-cycle fatigue behavior of AlSi10Mg manufactured by selective laser melting: Effect of build orientation and mean stress10.1016/j.ijfatigue.2020.105696 ↗
28. A review on the Fatigue behaviour of AlSi10Mg alloy fabricated using Laser Powder Bed Fusion technique10.1016/j.jmrt.2022.01.028 ↗
29. Micro-mechanical investigation of fatigue behavior of Al alloys containing surface/superficial defects10.1016/j.msea.2020.138958 ↗
30. High cycle fatigue behavior and life prediction for additively manufactured 17-4 PH stainless steel: Effect of sub-surface porosity and surface roughness10.1016/j.tafmec.2020.102477 ↗
31. The microstructure and fatigue performance of Inconel 718 produced by laser-based powder bed fusion and post heat treatment10.1016/j.ijfatigue.2021.106700 ↗
32. High-cycle fatigue behavior of a laser powder bed fusion additive manufactured Ti-6Al-4V titanium: effect of pores and tested volume size10.1016/j.ijfatigue.2021.106206 ↗
33. Fatigue of additive manufactured Ti-6Al-4V, Part II: The relationship between microstructure, material cyclic properties, and component performance10.1016/j.ijfatigue.2019.105363 ↗
34. Parent grain reconstruction from partially or fully transformed microstructures in MTEX10.1107/S1600576721011560 ↗
35. Murakami · 2002
36. Tensile and creep properties improvement of Ti-6Al-4V alloy specimens produced by electron beam powder bed fusion additive manufacturing10.3390/met9111207 ↗
37. Effect of single and duplex stage heat treatment on the microstructure and mechanical properties of cast Ti-6Al-4V alloy10.1007/s13632-013-0103-7 ↗
38. Improving the mechanical properties of TIG welding Ti-6Al-4V by post weld heat treatment10.1016/j.proeng.2017.10.1033 ↗
39. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
40. Microstructure and mechanical properties of wrought and additive manufactured Ti-6Al-4 V cylindrical bars10.1016/j.protcy.2015.07.037 ↗
41. Effect of α texture on the tensile deformation behavior of Ti–6Al–4V alloy produced via electron beam rapid manufacturing10.1016/j.msea.2018.11.012 ↗
42. Habraken · 2013
43. The Hall–Petch effect as a manifestation of the general size effect10.1098/rspa.2015.0890 ↗
44. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective Laser Melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
45. Influence of processing on microstructure and mechanical properties of (α+ β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
46. Qualification of AM parts: Extreme value statistics applied to tomographic measurements10.1016/j.matdes.2017.05.091 ↗
47. Largest-extreme-value distribution analysis of multiple inclusion types in determining steel cleanliness10.1007/s11663-001-0036-4 ↗
48. Fatigue properties of AlSi10Mg obtained by additive manufacturing: Defect-based modelling and prediction of fatigue strength10.1016/j.engfracmech.2017.11.002 ↗
49. Defect analysis and fatigue design basis for Ni-based superalloy 718 manufactured by selective laser melting10.1016/j.ijfatigue.2018.08.002 ↗
50. Effects of defects, surface roughness and HIP on fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.prostr.2017.11.055 ↗