Microcrack mitigation during laser scanning of tungsten via preheating and alloying strategies
Source abstract
Abstract
When tungsten is processed by laser powder bed fusion additive manufacturing, the combination of high residual stresses and tungsten’s inherent ductile-to-brittle transition leads to a network of microcracks. While preheating is widely accepted as the most efficient way to reduce residual stresses in additively manufactured parts, thus far it has proven ineffective in completely eliminating microcracking in tungsten. In addition to preheating, changing the alloy composition is an increasingly popular approach to circumvent cracking. This work utilizes in situ high-speed optical imaging combined with thermomechanical modeling to elucidate the effect of preheating and alloying with 2 wt% rare earth oxides on the cracking behavior in powderless single track and hatch strategy laser scans. Optical imaging reveals two distinct cracking mechanisms in the fusion zone and the heat affected zone, both of which are eliminated by substrate preheating temperatures of 773–873 K. Due to the lower melting point of the rare earth oxide inclusions, the melt behavior becomes more turbulent and processing parameters need to be adjusted accordingly, but the cracking characteristics remained the same. The response to preheating was similar for both pure tungsten and the alloys tested in this study; there was no beneficial effect of the alloy additions. This work shows that the fundamental metallurgical cause of microcracking in tungsten can be circumvented, in a step towards structural applications of additively manufactured tungsten.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Use of tungsten material for the ITER divertor10.1016/j.nme.2016.07.003 ↗
2. Mechanical and microstructural investigations of tungsten and doped tungsten materials produced via powder injection molding10.1016/j.nme.2015.04.002 ↗
3. Controlling factors for the brittle-to-ductile transition in tungsten single crystals10.1126/science.282.5392.1293 ↗
4. Dislocation dynamic modelling of the brittle–ductile transition in tungsten10.1080/14786430902992619 ↗
5. Brittle–ductile transitions in polycrystalline tungsten10.1080/14786435.2010.502145 ↗
6. The nature of the brittle-to-ductile transition of ultra fine grained tungsten (W) foil10.1016/j.ijrmhm.2014.11.005 ↗
7. G. Liu, G.J. Zhang, F. Jiang, D. Ding, Y.J. Sun, J. Sun, E. Ma, Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility, Nat. Mater. (n.d.). 〈https://www.nature.com/articles/nmat3544〉. (Accessed 3 December 2020).
8. J.R. Stephens, Effects of Interstitial Impurities on the Low-Temperature Tensile Properties of Tungsten, National Aeronautics and Space Administration Cleveland OH Lewis Research Center, 1964. 〈https://apps.dtic.mil/sti/citations/ADA396979〉. (Accessed 15 September 2020).
9. M. Garfinkle, W.D. Klopp, W.R. Witzke, Superplasticity in tungsten--rhenium alloys, Undefined, 1968. /paper/SUPERPLASTICITY-IN-TUNGSTEN--RHENIUM-ALLOYS.-Garfinkle-Klopp/fea377190f40a82be0712ff7dcdfc6499f4cf6d7 . (Accessed 3 December 2020).
10. Yielding and fracture in tungsten and tungsten-rhenium alloys10.1016/0022-5088(69)90047-2 ↗
11. Tungsten–vanadium–yttria alloys for fusion power reactors (II): mechanical characterization10.1016/j.ijrmhm.2015.07.031 ↗
12. W–2wt%Y2O3 composite: microstructure and mechanical properties10.1016/j.msea.2012.01.011 ↗
13. Selective laser melting of Ti6Al4V alloy for biomedical applications: temperature monitoring and microstructural evolution10.1016/j.jallcom.2013.08.183 ↗
14. Assessing and comparing influencing factors of residual stresses in selective laser melting using a novel analysis method10.1177/0954405412437085 ↗
15. Residual stress via the contour method in compact tension specimens produced via selective laser melting10.1016/j.scriptamat.2014.05.016 ↗
16. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
17. Additive manufacturing of Ni-based superalloys: the outstanding issues10.1557/mrs.2016.211 ↗
18. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
19. Analysis of laser-induced microcracking in tungsten under additive manufacturing conditions: experiment and simulation10.1016/j.actamat.2020.04.060 ↗
20. Rapid additive manufacturing of MR compatible multipinhole collimators with selective laser melting of tungsten powder10.1118/1.4769122 ↗
21. The effect of powder characteristics on build quality of high-purity tungsten produced via laser powder bed fusion (LPBF)10.1007/s11661-019-05601-6 ↗
22. Effect of processing parameters on the densification, microstructure and crystallographic texture during the laser powder bed fusion of pure tungsten10.1016/j.ijrmhm.2018.10.004 ↗
23. B. Vrancken, R. Wauthlé, J.-P. Kruth, J. Van Humbeeck, Study of the influence of material properties on residual stress in selective laser melting, in: Proceedings of the Solid Freeform Fabrication Symposium, 2013, pp. 393–407. 〈https://lirias.kuleuven.be/1572878〉. (Accessed 31 March 2020).
24. Crack suppression in additively manufactured tungsten by introducing secondary-phase nanoparticles into the matrix10.1016/j.ijrmhm.2018.11.013 ↗
25. Cracking in laser additively manufactured W: initiation mechanism and a suppression approach by alloying10.1016/j.matdes.2018.12.010 ↗
26. Selective laser melting of tungsten and tungsten alloys10.1016/j.ijrmhm.2017.12.005 ↗
27. Effect of Ta addition on the fuzz formation of additively manufactured W based materials
28. Densification and crack suppression in selective laser melting of pure molybdenum10.1016/j.matdes.2017.04.094 ↗
29. Effect of processing parameters on microstructure and properties of tungsten heavy alloys fabricated by SLM10.1016/j.ijrmhm.2019.03.020 ↗
30. Selective laser melting of crack-free high density M2 high speed steel parts by baseplate preheating10.1115/1.4028513 ↗
31. Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting10.2351/1.4828755 ↗
32. B. Vrancken, S. Buls, J.-P. Kruth, J. Van Humbeeck, Influence of preheating and oxygen content on Selective Laser Melting of Ti6Al4V, in: Proceedings of the 16th RAPDASA Conference, 2015. 〈https://lirias.kuleuven.be/1748568〉 (accessed March 31, 2020).
33. Additive manufacturing of pure tungsten by means of selective laser beam melting with substrate preheating temperatures up to 1000 ∘C10.1016/j.nme.2019.02.034 ↗
34. J. Wright, Additive Manufacturing of Tungsten via Selective Laser Melting and Electron Beam Melting (PhD), University of Sheffield, 2019. 〈http://etheses.whiterose.ac.uk/26247/〉. (Accessed 3 December 2020).
35. R.I. Jaffee, G.T. Hahn, Structural Considerations in Developing Refractory Metal Alloys, Defense Metals Information Center, Battelle Memorial Institute, 1963.
36. Gludovatz · 2010
37. Fracture toughness of polycrystalline tungsten alloys10.1016/j.ijrmhm.2010.04.007 ↗
38. R.I. Jaffee, B.C. Allen, D.J. Maykuth, Effects of dispersions on the recrystallization and ductile to brittle transition behavior of tungsten, in: Powder Metallurgy in the Nuclear Age: Plansee Proceedings 1961, Metallwerk Plansee AG, Reutte/Tyrol, n.d., pp. 770–798.
39. Solberg · 2018
40. Kinetic evaporation and condensation rates and their coefficients10.1016/0021-9797(92)90205-Z ↗
41. A new finite element model for welding heat sources10.1007/BF02667333 ↗
42. Direct measurements of laser absorptivity during metal melt pool formation associated with powder bed fusion additive manufacturing processes10.2351/1.5040636 ↗
43. Analytical expressions for thermophysical properties of solid and liquid tungsten relevant for fusion applications10.1016/j.nme.2017.08.002 ↗
44. Thermophysical properties
45. Appendix A to ITER SDC-IC, 2013.
46. Evaluation of a thermomechanical model for prediction of residual stress during laser powder bed fusion of Ti-6Al-4V
47. Implementation of a thermomechanical model for the simulation of selective laser melting10.1007/s00466-014-1024-2 ↗
48. Strain-rate dependence of the brittle-to-ductile transition temperature in tungsten10.1080/14786430701253197 ↗
49. Physical changes in tungsten and thoriated tungsten electrodes after subsecond heating10.1007/BF01441992 ↗
50. Overview No. 3 Fracture-mechanism maps and their construction for f.c.c. metals and alloys10.1016/0001-6160(79)90105-6 ↗
51. Rare earths. I. Vaporization of La2O3 and Nd2O3: dissociation energies of gaseous LaO and NdO110.1021/j100826a029 ↗
52. Vaporization of rare-earth oxides10.1111/j.1151-2916.1960.tb14589.x ↗
53. Optical properties of TiO2, Y2O3 and CeO2 thin films deposited by electron beam evaporation10.1016/0040-6090(93)90534-V ↗
54. The theory of moving sources of heat and its application to metal treatments
55. Thermal shock behavior of tungsten based alloys manufactured via powder injection molding10.1016/j.jnucmat.2013.01.342 ↗
56. Measurement of thermophysical properties by a pulse-heating method: thoriated tungsten in the range 1200 to 3600 K10.1007/BF01458839 ↗
57. W-1% La2O3 submitted to a single laser pulse: effect of particles on heat transfer and surface morphology10.3390/met8060389 ↗
58. Thermal boundary resistance10.1103/RevModPhys.61.605 ↗
59. Energy-coupling mechanisms revealed through simultaneous keyhole depth and absorptance measurements during laser-metal processing10.1103/PhysRevApplied.13.064070 ↗
60. Energy coupling mechanisms and scaling behavior associated with laser powder bed fusion additive manufacturing10.1002/adem.201900185 ↗
61. Tekna, Spherical Tungsten Metal Powder, Tekna, n.d. 〈http://www.tekna.com/spherical-powders/tungsten〉. (Accessed 15 December 2020).
62. Fully dense and crack free molybdenum manufactured by Selective Laser Melting through alloying with carbon10.1016/j.ijrmhm.2019.105000 ↗
63. On the role of carbon in molybdenum manufactured by Laser Powder Bed Fusion10.1016/j.ijrmhm.2020.105283 ↗
64. Selective Laser Melting process optimization of Ti–Mo–TiC metal matrix composites10.1016/j.cirp.2019.04.120 ↗