journal article·2022-10Open access

Deciphering the transformation pathway in laser powder-bed fusion additive manufacturing of Ti-6Al-4V alloy

J. Chen, D. Fabijanic, T. Zhang, E.W. Lui, M. Brandt, W. Xu

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Additive manufacturing and postprocessing of Ti-6Al-4V for superior mechanical properties10.1557/mrs.2016.215 ↗
2. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
4. The role of lattice defects, element partitioning and intrinsic heat effects on the microstructure in selective laser melted Ti-6Al-4V10.1016/j.actamat.2019.01.039 ↗
5. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
6. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
7. Mapping the geometry of Ti-6Al-4V: from martensite decomposition to localized spheroidization during selective laser melting10.1016/j.scriptamat.2020.02.043 ↗
8. Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties10.1007/s11837-015-1297-8 ↗
9. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective laser melted Ti-6Al-4V10.1016/j.msea.2017.04.033 ↗
10. Inducing stable alpha plus beta microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments10.3390/ma10030268 ↗
11. New development in selective laser melting of Ti-6Al-4V: a wider processing window for the achievement of fully lamellar alpha plus beta microstructures10.1007/s11837-017-2599-9 ↗
12. Microstructural tailoring of as-selective laser melted Ti-6Al-4V alloy for high mechanical properties10.1016/j.jallcom.2019.152536 ↗
13. S.M. Kelly, Thesis: Thermal and microstructure modeling of metal deposition processes with application to Ti-6Al-4V, Virginia Polytechnic Institute and State University, 2004.
14. G. Lütjering, J.C. Williams, Titanium, Springer Science & Business Media, 2007.
15. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging10.1126/science.aav4687 ↗
16. Automated image mapping and quantification of microstructure heterogeneity in additive manufactured Ti-6Al-4V10.1016/j.matchar.2018.10.027 ↗
17. J. Hiscocks, R. Hielscher, Parent beta phase reconstruction in titanium alloys, (2021). https://mtex-toolbox.github.io/TiBetaReconstruction.html. (Accessed 20 Jan 2022).
18. Defects-dictated tensile properties of selective laser melted Ti-6Al-4V10.1016/j.matdes.2018.08.004 ↗
19. Quantifying the dislocation structures of additively manufactured Ti-6Al-4V alloys using X-ray diffraction line profile analysis
20. On the origin of microstructural banding in Ti-6Al-4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
21. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
22. Phase transformations during cooling in alpha plus beta titanium alloys10.1016/S0921-5093(97)00802-2 ↗
23. Sympathetic nucleation: an overview10.1016/0921-5107(95)80022-0 ↗
24. The influence of heat treatment on the microstructure and properties of HIPped Ti-6Al-4V10.1016/j.actamat.2018.12.025 ↗
25. Crystallographic and morphological relationships between β phase and the Widmanstätten and allotriomorphic α phase at special β grain boundaries in an α/β titanium alloy10.1016/j.actamat.2007.08.029 ↗
26. Variant selection of grain boundary α by special prior β grain boundaries in titanium alloys10.1016/j.actamat.2014.05.003 ↗
27. Crystallography of grain boundary α precipitates in a β titanium alloy10.1007/BF02649821 ↗
28. 3D electron backscatter diffraction study of alpha lath morphology in additively manufactured Ti-6Al-4V10.1016/j.ultramic.2020.113073 ↗
29. Using transmission Kikuchi diffraction to characterise alpha variants in an alpha plus beta titanium alloy10.1111/jmi.12569 ↗
30. Influence of tempering temperature and time on the α′-Ti-6Al-4V martensite10.1016/0925-8388(95)02057-8 ↗
31. N. Sridharan, Y.M. Chen, P. Nandwana, R.M. Ulfig, D.J. Larson, S.S. Babu, On the potential mechanisms of beta to alpha' plus beta decomposition in two phase titanium alloys during additive manufacturing: a combined transmission Kikuchi diffraction and 3D atom probe study, J. Mater. Sci. 55 (2020) 1715–1726.10.1007/s10853-019-03984-w ↗
32. Effect of self-accommodation on α/α boundary populations in pure titanium10.1016/S1359-6454(03)00035-1 ↗
33. Introducing transformation twins in titanium alloys: an evolution of alpha-variants during additive manufacturing10.1080/21663831.2020.1850536 ↗
34. The role of crystallographic and geometrical relationships between alpha and beta phases in an alpha/beta titanium alloy10.1016/S1359-6454(03)00179-4 ↗
35. Massive transformation in Ti-6Al-4V additively manufactured by selective electron beam melting10.1016/j.actamat.2015.11.011 ↗
36. Study on transformation mechanism and kinetics of alpha' martensite in TC4 alloy isothermal aging process10.3390/cryst10030229 ↗
37. Static coarsening behaviour of lamellar microstructure in selective laser melted Ti-6Al-4V10.1016/j.jmst.2019.04.008 ↗
38. Resistivity study and computer modelling of the isothermal transformation kinetics of Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.08Si alloys10.1016/S0925-8388(00)01227-5 ↗
39. G.F.V. Voort, Atlas of time-temperature diagrams for nonferrous alloys, ASM International, 1991.
40. Formation of Widmanstätten alpha structure in a Ti–6Al–4V alloy10.2320/matertrans1989.35.238 ↗
41. In-situ observation of single variant alpha colony formation in Ti-6Al-4V10.1016/j.actamat.2021.117315 ↗
42. Diffusion-controlled phase transformations in steels
43. H. Fujii, H.G. Suzuki, Effect of cooling rates on microstructures of beta treated alpha plus beta titanium alloys, Tetsu-to-Hagane 77 (1991) 1481–1488.10.2355/tetsutohagane1955.77.9_1481 ↗
44. The effect of microstructure on the mechanical properties of two-phase titanium alloys10.1016/S0924-0136(02)00248-0 ↗
45. Y. Kuang, Thesis: Generation of TTT and CCT curves for cast Ti-6Al-4V alloy, University of Florida, 2004.
46. The kinetics of phase transformations during continuous cooling of the Ti-6Al-4V alloy from the single-phase beta range10.2478/v10172-011-0077-x ↗
47. Thermal and microstructural analysis of laser-based directed energy deposition for Ti-6Al-4V and Inconel 625 deposits10.1016/j.msea.2018.01.060 ↗
48. D.A. Porter, K.E. Easterling, Phase transformations in metals and alloys (revised reprint), CRC press, 2009.10.1201/9781439883570 ↗
49. Computational assessment of thermokinetics and associated microstructural evolution in laser powder bed fusion manufacturing of Ti6Al4V alloy10.1038/s41598-020-63281-4 ↗