Additive manufacturing of high-strength Al alloys (such as 2xxx, 6xxx and 7xxx series alloys) by laser powder bed fusion (LPBF) encounters a challenge because of their high susceptibility to solidification crack. The current work develops a crack-free and novel high-strength Al-Cu-Mg-Y alloy fabricated by LPBF using the rare earth yttrium (Y) modified 2024 alloy powders. In the LPBF-fabricated Al-Cu-Mg-Y alloy, the rare earth element Y is revealed as an effective alloying element for the solidification crack elimination, which is mainly attributed to the combination of the narrowed brittle temperature range, the decreased solidification crack susceptibility index and the refined grains. The element Y can also react with Al and Cu to form the Al8Cu4Y phases during the LPBF process. In the LPBF-fabricated Al-Cu-Mg-Y alloy, the larger number of Al8Cu4Y phases and the finer grains result in higher compressive yield strength than most LPBF-fabricated Al alloys. Interestingly, the LPBF-fabricated Al-Cu-Mg-Y alloy can be highly deformed without collapse up to a large compressive strain of ~70 %. After T6 heat treatment, the LPBF-fabricated Al-Cu-Mg-Y alloy exhibits a significant increase in the compressive stress after the yield point, corresponding to the homogeneously distributed Ω precipitate in the Al matrix. In addition, the tensile strength is lower than the compressive strength for the LPBF-fabricated and T6 heat-treated Al-Cu-Mg-Y alloys. This difference is related to the internal pores in the two alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Additive manufacturing of metallic components: process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. 3D printing of aluminum alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
3. Laser powder bed fusion of compositionally graded CoCrMo-InConel 718
4. Research trends in laser powder bed fusion of Al alloys within the last decade
5. A review of laser powder bed fusion additive manufacturing of aluminium alloys: Microstructure and properties
6. Assessment of AlZnMgCu alloy powder modification for crack-free laser powder bed fusion by differential fast scanning calorimetry10.1016/j.matdes.2021.109677 ↗
7. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
8. Effect of nano-TiB2 particles on the anisotropy in an AlSi10Mg alloy processed by selective laser melting10.1016/j.jallcom.2019.05.279 ↗
9. A selective laser melting and solution heat treatment refined Al-12Si alloy with a controllable ultrafine eutectic microstructure and 25 % tensile ductility10.1016/j.actamat.2015.05.017 ↗
10. Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures10.1016/j.matchar.2018.01.028 ↗
11. On the selective laser melting based additive manufacturing of AlSi10Mg: the process parameter investigation through multiphysics simulation and experimental validation10.1016/j.jallcom.2021.161873 ↗
12. Porosity formation mechanisms and fatigue response in Al-Si-Mg alloys made by selective laser melting10.1016/j.msea.2017.11.078 ↗
13. Microstructure and mechanical properties of Al-12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
14. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
15. Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures10.1016/j.matchar.2018.01.028 ↗
16. Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment10.1016/j.matchar.2018.04.022 ↗
17. Influence of heat treatment on the high-cycle fatigue properties and fatigue damage mechanism of selective laser melted AlSi10Mg alloy10.1016/j.msea.2021.141486 ↗
18. Achieving superior mechanical properties of selective laser melted AlSi10Mg via direct aging treatment10.1016/j.jmst.2021.07.059 ↗
19. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
20. Selective laser melting of a high strength Al-Mn-Sc alloy: Alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
21. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure
22. Selective laser melting of a novel Sc and Zr modified Al-6.2 Mg alloy: Processing, microstructure, and properties10.1016/j.powtec.2017.06.050 ↗
23. Selective laser melting of rare earth element Sc modified aluminum alloy: Thermodynamics of precipitation behavior and its influence on mechanical properties
24. Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
25. SLM-processed Sc- and Zr- modified Al-Mg alloy: Mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
26. Manipulating the microstructure and tensile properties of selective laser melted Al-Mg-Sc-Zr alloy through heat treatment10.1016/j.jallcom.2020.154773 ↗
27. Additive manufacturing of a high strength Al-5Mg2Si-2Mg alloy: Microstructure and mechanical properties10.1016/j.jmst.2021.02.048 ↗
28. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
29. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: Cracking elimination by co-incorporation of Si and TiB2
30. Selective laser melting of high strength Al-Cu-Mg alloys: processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
31. An understanding of duplex microstructures encountered during high strength aluminium alloy laser beam melting processing10.1016/j.actamat.2021.117024 ↗
32. Davis · 1993
33. Heat treatment of aluminum alloys produced by laser powder bed fusion: a review10.1016/j.matdes.2021.109651 ↗
34. Design approaches for printability-performance synergy in Al alloys for laser-powder bed additive manufacturing10.1016/j.matdes.2021.109640 ↗
35. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
36. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: Crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
37. Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys
38. Recent advances in hot tearing during casting of aluminium alloys10.1016/j.pmatsci.2020.100741 ↗
39. Development of a high strength Al-Zn-Si-Mg-Cu alloy for selective laser melting10.1016/j.jallcom.2019.06.123 ↗
40. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗
41. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
42. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
43. Influence of grain refinement on hot cracking in laser welding of aluminum10.1007/s40194-014-0121-3 ↗
44. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
45. Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion
46. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by laser-based powder bed fusion10.1007/s11661-020-06073-9 ↗
47. Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability10.1016/j.msea.2020.139079 ↗
48. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
49. Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-Mg-Cu alloy manufactured by selective laser melting10.1016/j.jallcom.2021.163427 ↗
50. Laser powder bed fusion of crack-free TiN/Al7075 composites with enhanced mechanical properties10.1016/j.matlet.2020.128625 ↗
51. Novel approach to additively manufacture high-strength Al alloys by laser powder bed fusion through addition of hybrid grain refiners
52. Microstructure and mechanical properties of a novel Sc and Zr modified 7075 aluminum alloy prepared by selective laser melting10.1016/j.msea.2019.138478 ↗
53. Microstructure and materials characterisation of the novel Al-Cu-Y alloy10.1080/02670836.2018.1460536 ↗
54. Microstructure, mechanical properties and superplasticity of the Al-Cu-Y-Zr alloy10.1016/j.msea.2019.04.118 ↗
55. Effects of yttrium additions on microstructures and mechanical properties of cast Al-Cu-Mg-Ag alloys10.1016/j.jallcom.2021.159435 ↗
56. Effect of Y on the hot tearing susceptibility of 3Y2O3/Al5Cu composite10.1016/j.jallcom.2020.156152 ↗
57. The effect of Y on the hot-tearing resistance of Al-5 wt% Cu based alloy10.1016/j.matdes.2009.11.044 ↗
58. Main defects observed in aluminum alloy parts produced by SLM: From causes to consequences
59. Thermodynamic description of the Al-Cu-Y ternary system10.1016/j.calphad.2011.09.008 ↗
60. The Y-Cu-Al system10.1016/S0925-8388(02)00873-3 ↗
61. Microstructure and mechanical properties of a heat-treatable Al-3.5Cu-1.5Mg-1Si alloy produced by selective laser melting10.1016/j.msea.2017.11.063 ↗
62. Determination of interfacial atomic structure, misfits and energetics of Ω phase in Al-Cu-Mg-Ag alloy10.1016/j.actamat.2014.07.074 ↗
63. The effect of silver on microstructural evolution in two 2xxx series Al-alloys with a high Cu:Mg ratio during ageing to a T8 temper10.1016/j.msea.2008.03.014 ↗
64. Precipitation behavior of aluminum alloy 2139 fabricated using additive manufacturing10.1016/j.msea.2015.08.088 ↗
65. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
66. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
67. A new criterion for internal crack formation in continuously cast steels10.1007/s11663-000-0115-y ↗
68. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
69. Formability improvement, cracking behavior and control of Y-modified Ti-43Al-4Nb-1Mo-0.1B alloys produced by selective laser melting10.1016/j.jallcom.2020.157172 ↗
70. Structural, elastic and electronic properties of θ (Al2Cu) and S (Al2CuMg) strengthening precipitates in Al-Cu-Mg series alloys: First-principles calculations10.1016/j.ssc.2012.09.003 ↗
71. Effects of yttrium additions on microstructures and mechanical properties of cast Al-Cu-Mg-Ag alloys10.1016/j.jallcom.2021.159435 ↗
72. Reconsideration of the concept of critical nucleus and the Gibbs-Thomson equation10.1016/0022-0248(95)01033-5 ↗
73. Microstructural consistency in the additive manufactured metallic materials: A study on the laser powder bed fusion of AlSi10Mg
74. Effects of Mg and Si contents on the microstructure and mechanical properties of AA6014 alloys in T4P and T6P temper10.1016/j.msea.2018.10.043 ↗
75. Selective laser remelting of in-situ Al2O3 particles reinforced AlSi10Mg matrix composite: Densification, microstructure and microhardness10.1016/j.vacuum.2021.110365 ↗
76. Dislocation interaction with semicoherent precipitates (Ω phase) in deformed Al-Cu-Mg-Ag alloy10.1016/S1359-6454(98)00188-8 ↗
77. Processing of Al-12Si-TNM composites by selective laser melting and evaluation of compressive and wear properties10.1557/jmr.2015.326 ↗