journal article·2022-02

Unique opportunities for microstructure engineering via trace B4C addition to Ti-6Al-4V through laser powder bed fusion process: As-built and heat-treated scenarios

Eskandar Fereiduni, Ali Ghasemi, Mohamed Elbestawi

Publisher page

Abstract

This research study examines the role of minor B4C addition (0.2 wt%) in improving the mechanical properties of the laser powder bed fusion (L-PBF) fabricated Ti-6Al-4V (Ti64) alloy in the as-built and heat-treated conditions. The fabricated titanium matrix composites (TMCs) were subjected to two different heat treatment scenarios, i.e., subtransus and supertransus, and were compared to the Ti64 counterparts exposed to the same thermal cycles. Both as-built and heat-treated Ti64 and TMC samples were characterized in terms of the grain structure, microstructure within the grains, and the size, morphology, volume fraction, and crystallographic orientation of the phases. The knowledge gained from microstructural investigations was correlated to the mechanical behavior of components, including compressive strength and ductility, microhardness, and scratch resistance. The governing strengthening mechanisms were identified, and the contribution of each mechanism in the overall yield strength was explored. Results revealed that TMCs possessed higher yield and ultimate compressive strengths than their Ti64 counterparts owing to the hard TiB needles homogeneously dispersed in the microstructure. However, except for the supertransus heat-treated condition, the TMCs showed slightly lower fracture strain than the Ti64 samples. The elimination of GB-α in the supertransus heat-treated TMC sample caused by the TiB needles led to a higher fracture strain than the corresponding Ti64 case. While the implemented heat treatment strategies could tailor the mechanical properties, the optimum thermal cycles for Ti64 were not necessarily applicable to TMC components.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (79)

Show source-provided references
1. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
2. Additive manufacturing: scientific and technological challenges, market uptake and opportunities10.1016/j.mattod.2017.07.001 ↗
3. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
4. Influence of alloying elements on laser powder bed fusion processability of aluminum: a new insight into the oxidation tendency
5. The rise of 3-D printing: the advantages of additive manufacturing over traditional manufacturing10.1016/j.bushor.2017.05.011 ↗
6. Selective laser melting of aluminum and titanium matrix composites: recent progress and potential applications in the aerospace industry10.3390/aerospace7060077 ↗
7. Heat treatment possibilities for an in situ βTi-TiC composite made by laser powder bed fusion
8. Achieving high strength and high ductility in WC-reinforced iron-based composites by laser additive manufacturing
9. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: a state of the art review10.1016/j.pmatsci.2019.04.006 ↗
10. Laser powder bed fusion processability of Ti-6Al-4V powder decorated by B4C particles10.1016/j.matlet.2021.129923 ↗
11. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
12. Part deflection and residual stresses in laser powder bed fusion of H13 tool steel10.1016/j.matdes.2021.109659 ↗
13. A new insight on the analysis of residual stresses related distortions in selective laser melting of Ti-6Al-4V using the improved bridge curvature method
14. An immersed boundary approach for residual stress evaluation in selective laser melting processes
15. Enhanced strength–ductility synergy and transformation-induced plasticity of the selective laser melting fabricated 304L stainless steel
16. Selective laser melting of an Al–Fe–V–Si alloy: microstructural evolution and thermal stability10.1016/j.jmst.2016.09.015 ↗
17. Microstructure and tensile property of a precipitation strengthened high entropy alloy processed by selective laser melting and post heat treatment
18. Martensite decomposition during post-heat treatments and the aging response of near-α Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy processed by selective laser melting (SLM)10.1142/S2424913020500186 ↗
19. Electron beam melted Ti–6Al–4V: microstructure, texture and mechanical behavior of the as-built and heat-treated material10.1016/j.msea.2015.11.052 ↗
20. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
21. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
22. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
23. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
24. TiB reinforced Ti-6Al-4V matrix composites with improved short-term creep performance fabricated by laser powder bed fusion10.1016/j.jmapro.2021.08.063 ↗
25. Progress on discontinuously reinforced titanium matrix composites10.1016/j.jallcom.2018.07.100 ↗
26. Influence of trace boron addition on microstructure, tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
27. Metallurgical features of direct laser-deposited Ti6Al4V with trace boron10.1016/j.jmapro.2018.09.018 ↗
28. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition10.1016/j.matdes.2019.108191 ↗
29. Effect of trace lanthanum hexaboride on the phase, grain structure, and texture of electron beam melted Ti-6Al-4V
30. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
31. Grain refinement of cast titanium alloys via trace boron addition10.1016/j.scriptamat.2005.08.020 ↗
32. Laser deposition-additive manufacturing of TiB-Ti composites with novel three-dimensional quasi-continuous network microstructure: effects on strengthening and toughening10.1016/j.compositesb.2017.09.019 ↗
33. Embedding boron into Ti powder for direct laser deposited titanium matrix composite: microstructure evolution and the role of nano-TiB network structure10.1016/j.compositesb.2021.108683 ↗
34. Microstructure and mechanical properties of (TiB + TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders
35. Microstructure evolution and mechanical properties of selective laser melted bulk-form titanium matrix nanocomposites with minor B4C additions10.1016/j.matdes.2019.108245 ↗
36. Selective laser melting of hybrid ex-situ/in-situ reinforced titanium matrix composites: laser/powder interaction, reinforcement formation mechanism, and non-equilibrium microstructural evolutions10.1016/j.matdes.2019.108185 ↗
37. Boron modified titanium alloys10.1016/j.pmatsci.2020.100653 ↗
38. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB + TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
39. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
40. Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by selective laser melting (SLM): densification, growth mechanism and wear behavior10.1016/j.compscitech.2011.07.010 ↗
41. Characterization of composite powder feedstock from powder bed fusion additive manufacturing perspective10.3390/ma12223673 ↗
42. Texture analysis with MTEX–free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
43. A. C-05, Standard test method for adhesion strength and mechanical failure modes of ceramic coatings by quantitative single point scratch testing, 2005.
44. Formation of equiaxed alpha in TiB reinforced Ti alloy composites10.1016/j.scriptamat.2004.10.019 ↗
45. Modification of the α-Ti laths to near equiaxed α-Ti grains in as-sintered titanium and titanium alloys by a small addition of boron10.1016/j.jallcom.2013.07.097 ↗
46. Heat-treatment effects on the microstructure and tensile properties of powder metallurgy Ti-6Al-4V alloys modified with boron10.1007/s11661-009-0157-y ↗
47. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
48. Microstructure and texture evolution during solidification processing of Ti–6Al–4V10.1016/S0924-0136(02)00865-8 ↗
49. Microstructural characterization and mechanical properties of nano-scale/sub-micron TiB-reinforced titanium matrix composites fabricated by laser powder bed fusion10.1016/j.jallcom.2021.163054 ↗
50. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: a comparative study10.1016/j.msea.2020.140415 ↗
51. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
52. Formation of α-Widmanstätten structure: effects of grain size and cooling rate on the Widmanstätten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
53. G. Welsch, R. Boyer, E. Collings, Materials Properties Handbook: Titanium Alloys, ASM international, 1993.
54. Specific heat treatment of selective laser melted Ti–6Al–4V for biomedical applications10.1007/s11706-015-0315-7 ↗
55. Modification of α-phase of wire + arc additive manufactured Ti-6Al-4 V alloy with boron addition10.1016/j.matchar.2020.110616 ↗
56. Crystallographic orientation relationships of boride and carbide particles with α and β phases in a β-Ti alloy10.1016/j.jallcom.2014.05.202 ↗
57. Manufacturing of a nanosized TiB strengthened Ti-based alloy via electron beam powder bed fusion
58. Nucleation and growth of α-Ti on TiB precipitates in Ti–15Mo–2.6Nb–3Al–0.2Si–0.12B10.1080/14786435.2010.533134 ↗
59. Effect of hypoeutectic boron additions on the grain size and mechanical properties of Ti-6Al-4V manufactured with powder bed electron beam additive manufacturing10.1007/s11837-016-2210-9 ↗
60. Development of solidification microstructure in boron-modified alloy Ti–6Al–4V–0.1 B10.1016/j.actamat.2011.05.023 ↗
61. C. Leyens, M. Peters, Titanium and Titanium Alloys: Fundamentals and Applications, Wiley Online Library, 2006.
62. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
63. Solid solution strengthening in Ti-Al alloys10.1007/BF02644529 ↗
64. Process-structure-property relationships in additively manufactured metal matrix composites
65. Developing a phenomenological equation to predict yield strength from composition and microstructure in β processed Ti-6Al-4V10.1016/j.msea.2016.02.052 ↗
66. K.D. Rekedal, Investigation of the high-cycle fatigue life of selective laser melted and hot isostatically pressed Ti-6Al-4V, 2015.10.2514/6.2015-0894 ↗
67. Evaluation of dislocation densities in various microstructures of additively manufactured Ti6Al4V (Eli) by the method of X-ray diffraction10.3390/ma13235355 ↗
68. Callister · 2011 · NY
69. A probabilistic theory of the strength of short-fibre composites with variable fibre length and orientation10.1007/BF00543519 ↗
70. U.o.S, Mark Winter, UK, WebElements.
71. A constitutive equation relating composition and microstructure to properties in Ti-6Al-4V: as derived using a novel integrated computational approach10.1007/s11661-015-3072-4 ↗
72. Impact of hot isostatic pressing on the mechanical and microstructural properties of additively manufactured Ti–6Al–4V fabricated using directed energy deposition10.1016/j.msea.2020.139454 ↗
73. Effects of degree of deformation on the microstructure, mechanical properties and texture of hybrid-reinforced titanium matrix composites10.1016/j.actamat.2012.01.032 ↗
74. G.E. Dieter, D.J. Bacon, Mechanical Metallurgy, McGraw-hill, New York, 1986.
75. Meyers · 2008
76. The work-hardening of copper-silica v. equilibrium plastic relaxation by secondary dislocations10.1080/14786437608222028 ↗
77. A modified Hall–Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing10.1016/j.scriptamat.2012.02.008 ↗
78. Effect of trace boron addition on microstructures, textures, mechanical properties and fracture behaviors of near α titanium alloy10.1016/j.msea.2019.138749 ↗
79. Balance of strength and plasticity of additive manufactured Ti-6Al-4V alloy by forming TiB whiskers with cyclic gradient distribution