journal article·2022-07

Solidification microstructure, aging evolution and creep resistance of laser powder-bed fused Al-7Ce-8Mg (wt%)

Jovid U. Rakhmonov, David Weiss, David C. Dunand

Publisher page

Abstract

The solidification microstructure and the aging- and creep-resistances of a laser powder-bed fused (LPBF) hypoeutectic Al-7.3Ce-7.7Mg (wt%) alloy were investigated. Optimized process parameters allowed to produce specimens with > 99.7% relative density and high hardness (~1650 MPa), without solidification cracking despite a relatively coarse grain size (~ 30 µm). Two distinct solidification microstructures are observed within the solidified melt pools: (i) eutectic α-Al(Mg) and Al13CeMg6 (a metastable phase) at the bottom pool region, and (ii) eutectic α-Al(Mg) and Al11Ce3 (a stable phase) precipitates at the top pool region. The high hardness is predominantly attributed to Orowan strengthening and load-transfer effects from the Ce-rich precipitates, but solid-solution hardening from Mg is also quite pronounced, as most Mg resides in α-Al. Aging at 325 or 400 °C causes a continuous, slow hardness drop, but 85–90% of the initial hardness is retained after over 1000 h aging, consistent with the observation that the Ce-rich precipitates within the grains show very sluggish coarsening, making the alloy highly resistant to aging. The alloy exhibits two creep regimes at 300 ºC. At stresses below 18–20 MPa, diffusional creep is operating with signs of grain-boundary sliding inhibition due to Ce-rich precipitates at grain boundaries. At higher stresses, dislocation climb with either stress-invariant or stress-dependent subgrain structure is dominant, with additional load-transfer contributions and possibly a threshold stress due to dislocation-precipitate interactions. The alloy also exhibits much lower steady-state strain rates (e.g., two orders of magnitude lower at 20 MPa) as compared to a compositionally-similar, but conventionally-cast Al-Ce-Mg alloy with much coarser microstructure, demonstrating that LPBF Al-7.3Ce-7.7Mg alloy – because of its fine precipitates and despite its fine grain size - is well suited for long-term uses under stress at 300 ºC.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion
2. Improving mechanical properties of wire arc additively manufactured AA2196 Al–Li alloy by controlling solidification defects
3. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
4. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
5. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
6. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al–Si-based alloys
7. Microstructural consistency in the additive manufactured metallic materials: a study on the laser powder bed fusion of AlSi10Mg
8. Metallurgy, mechanistic models and machine learning in metal printing10.1038/s41578-020-00236-1 ↗
9. Additive manufacturing of metallic components – Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
10. Coarsening- and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
11. Microstructure characterization of SLM-processed Al-Mg-Sc-Zr alloy in the heat treated and HIPed condition
12. Laser powder bed fusion of a near-eutectic Al–Fe binary alloy: processing and microstructure
13. Change in microstructural characteristics of laser powder bed fused Al–Fe binary alloy at elevated temperature10.1016/j.jmst.2021.04.038 ↗
14. Design, microstructure and thermal stability of a novel heat-resistant Al-Fe-Ni alloy manufactured by selective laser melting10.1016/j.jallcom.2021.160949 ↗
15. Microstructure and properties of additively manufactured Al–Ce–Mg alloys10.1038/s41598-021-86370-4 ↗
16. Elevated temperature ductility dip in an additively manufactured Al-Cu-Ce alloy10.1016/j.actamat.2021.117285 ↗
17. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
18. Evaluation of an Al-Ce alloy for laser additive manufacturing10.1016/j.actamat.2016.12.065 ↗
19. Enhanced thermal coarsening resistance in a nanostructured aluminum-cerium alloy produced by additive manufacturing10.1016/j.matdes.2021.109988 ↗
20. Enhanced mechanical performance via laser induced nanostructure formation in an additively manufactured lightweight aluminum alloy
21. Anticipating impacts of introducing aluminum-cerium alloys into the United States automotive market10.1016/j.resconrec.2019.02.009 ↗
22. High performance aluminum–cerium alloys for high-temperature applications10.1039/C7MH00391A ↗
23. Thermal stability of aluminum-cerium binary alloys containing the Al-Al11Ce3 eutectic10.1016/j.msea.2021.140973 ↗
24. Enhanced load transfer and ductility in Al–9Ce alloy through heterogeneous lamellar microstructure design by cold rolling and annealing10.1016/j.msea.2021.141591 ↗
25. Cerium in aluminum alloys10.1007/s10853-019-03892-z ↗
26. Cast near-eutectic Al-12.5 wt% Ce alloy with high coarsening and creep resistance10.1016/j.msea.2019.138440 ↗
27. Aging- and creep-resistance of a cast hypoeutectic Al-6.9Ce-9.3Mg (wt%) alloy10.1016/j.msea.2020.139398 ↗
28. Microstructure and properties of novel heat resistant Al–Ce–Cu alloy for additive manufacturing10.1007/s12540-018-00211-0 ↗
29. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
30. High strength aluminum-cerium alloy processed by laser powder bed fusion
31. Solid solution strengthening mechanism in high pressure die casting Al-Ce-Mg alloys
32. Strengthening mechanisms in solid solution aluminum alloys10.1007/s11661-006-0142-7 ↗
33. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing
34. Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
35. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
36. Laser powder bed fusion of Al–10 wt% Ce alloys: microstructure and tensile property10.1007/s10853-020-05037-z ↗
37. Improved high-temperature aluminum alloys containing cerium10.1007/s11665-019-3884-2 ↗
38. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
39. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
40. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
41. Laser powder bed fusion of high-strength Sc/Zr-modified Al–Mg alloy: phase selection, microstructural/mechanical heterogeneity, and tensile deformation behavior10.1016/j.jmst.2021.03.069 ↗
42. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior10.1016/j.jmst.2020.08.003 ↗
43. Origin of non-uniform plasticity in a high-strength Al-Mn-Sc based alloy produced by laser powder bed fusion10.1016/j.jmst.2021.06.042 ↗
44. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
45. Influence of grain size, solute atoms and second-phase particles on creep behavior of polycrystalline solids10.1016/S0921-5093(01)01121-2 ↗
46. Thermal stability and crystal structure of high-temperature compound Al13CeMg610.1016/j.intermet.2017.05.003 ↗
47. Microstructure diversity dominated by the interplay between primary intermetallics and eutectics for Al-Ce heat-resistant alloys
48. The magnetic structures of Ce3Al11: a single crystal study10.1016/0304-8853(95)00051-8 ↗
49. Amirkhiz, On the Al–Al11Ce3 eutectic transformation in aluminum–cerium binary alloys10.3390/ma13204549 ↗
50. Thermal mismatch dislocations produced by large particles in a strain-hardening matrix10.1016/0921-5093(91)90557-4 ↗
51. Quantifying internal strains, stresses, and dislocation density in additively manufactured AlSi10Mg during loading-unloading-reloading deformation10.1016/j.matdes.2020.109339 ↗
52. Effect of laser rescanning on the grain microstructure of a selective laser melted Al-Mg-Zr alloy10.1016/j.matchar.2018.03.033 ↗
53. Creep properties and microstructure evolution at 260–300 °C of AlSi10Mg manufactured via laser powder-bed fusion10.1016/j.msea.2022.143075 ↗
54. Recent advances in the metallurgy of aluminum alloys. Part II: Age hardening10.1016/j.crhy.2018.10.012 ↗
55. General relationship between strength and hardness10.1016/j.msea.2011.08.061 ↗
56. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
57. Nabarro · 1967
58. Strengthening of an Al–Cu–Sn alloy by deformation-resistant precipitate plates10.1016/j.actamat.2008.03.028 ↗
59. Frost · 1982
60. Strengthening mechanisms in nanostructured high-purity aluminium deformed to high strain and annealed10.1016/j.actamat.2009.05.017 ↗
61. Microstructural features, texture and strengthening mechanisms of nanostructured AA6063 alloy processed by powder metallurgy10.1016/j.msea.2011.01.082 ↗
62. The Al−Mg (aluminum−magnesium) system10.1007/BF02873413 ↗
63. Enhanced thermal stability of precipitates and elevated-temperature properties via microalloying with transition metals (Zr, V and Sc) in Al–Cu 224 cast alloys10.1016/j.msea.2021.142090 ↗
64. Enhanced mechanical properties of high-temperature-resistant Al–Cu cast alloy by microalloying with Mg10.1016/j.jallcom.2020.154305 ↗
65. Effects of Al(MnFe)Si dispersoids with different sizes and number densities on microstructure and ambient/elevated-temperature mechanical properties of extruded Al-Mg-Si AA6082 alloys with varying Mn content
66. The effect of transition elements on high-temperature mechanical properties of AlSi foundry alloys: a review10.1002/adem.201500468 ↗
67. The applicability of Norton’s creep power law and its modified version to a single-crystal superalloy type CMSX-210.1016/0921-5093(96)10400-7 ↗
68. High-temperature creep mechanism in an Al-2 at% Mg alloy determined by stress-relaxation tests10.1016/0036-9748(76)90206-4 ↗
69. Warm-temperature tensile ductility in Al-Mg alloys10.1007/s11661-998-0300-1 ↗
70. H. Sato, H. Oikawa, Effects of solute concentration on creep characteristics of solution hardened ai-mg alloys at 600K, The 4th International Conference on Aluminum Alloys, Their Physical and Mechanical Properties, 1995.
71. Dislocation mechanics of creep10.1016/j.msea.2008.04.110 ↗
72. The Mg-concentration dependence of the strength of A1Mg alloys during glide-controlled deformation10.1016/0036-9748(89)90338-4 ↗
73. High temperature deformation of oxide dispersion strengthened al and Al‧Mg solid solutions10.1016/0001-6160(82)90153-5 ↗
74. Flow stress, subgrain size, and subgrain stability at elevated temperature10.1007/BF02661565 ↗
75. Strengthening mechanisms in AlNiSc alloys containing Al3Ni microfibers and Al3Sc nanoprecipitates10.1016/j.actamat.2018.10.059 ↗