Abstract The in-situ strengthening approach has attracted increasing attention in the selective laser melting (SLM) of high-performance alloy. In the present work, the argon-nitrogen (Ar-N2) reactive atmosphere was introduced in the SLM of Ti6Al4V alloy to achieve in-situ strengthening. The microstructure evolution and mechanical performance were studied under various atmosphere conditions and laser processing parameters, respectively. The results show that the solid-solution of 871 ppm ~ 1460 ppm nitrogen was obtained in the titanium matrix through the SLM in the Ar-N2 atmosphere, whereas no trace of nitride was found. Compared with the pure Ar atmosphere condition, an increasing ratio of nano-scale β phase and coarser martensites could be found after the addition of 5 vol% N2 in the Ar atmosphere, and the twinning phenomenon becomes more conspicuous as well. Under the Ar-N2 reactive atmosphere, the as-built Ti6Al4V alloy exhibits a significantly high yield strength of 1336 MPa and ultimate tensile strength of 1418 MPa, which are notably higher than previously reported SLM and conventionally manufactured Ti6Al4V alloys. Meanwhile, the fracture elongation of ~6% was obtained while attaining the high tensile strength. Analysis exhibits that the solid solution of the nitrogen atom is the main reason for improving strength in the nitrogen-strengthened Ti6Al4V samples. The strength of Ti6Al4V alloy was improved without excessive sacrifice of ductility, which was attributed to the multiple effects of the nitrogen solid-solution and the intrinsic heat treatment. This work adopts a practical methodology with designed low nitrogen content in the SLM process to achieve an in-situ strengthening of Ti6Al4V alloy without the formation of brittle nitrides.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
3. Fatigue strength improvement of selective laser melted Ti6Al4V using ultrasonic surface mechanical attrition10.1080/21663831.2019.1609110 ↗
4. Invited review article: metal-additive manufacturing - modeling strategies for application-optimized designs
5. Effect of heat treatment on the phase transformation and mechanical properties of Ti6Al4V fabricated by selective laser melting10.1016/j.jallcom.2018.06.076 ↗
6. Influence of the pore size and porosity of selective laser melted Ti6Al4V ELI porous scaffold on cell proliferation, osteogenesis and bone ingrowth10.1016/j.msec.2019.110289 ↗
7. Experimental investigations on natural fiber embedded additive manufacturing-based biodegradable structures for biomedical applications10.1108/RPJ-08-2017-0162 ↗
8. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
9. Selective laser melting of Ti6Al4V alloy: process parameters, defects and post-treatments10.1016/j.jmapro.2021.01.009 ↗
10. Microstructural evolution and stress state related to mechanical properties of electron beam melted Ti-6Al-4V alloy modified by laser shock peening10.1016/j.jmst.2019.11.039 ↗
11. Influence of trace boron addition on microstructure, tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
12. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: microstructure evolution and tribological behavior10.1016/j.powtec.2018.09.088 ↗
13. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
14. Laser additive manufacturing of nano-TiC reinforced Ni-based nanocomposites with tailored microstructure and performance10.1016/j.compositesb.2018.12.146 ↗
15. Rapid in situ fabrication of Fe/SiC bulk nanocomposites by selective laser melting directly from a mixed powder of microsized Fe and SiC10.1016/j.scriptamat.2013.11.031 ↗
16. Microstructure and mechanical properties of functionally graded TiCp/Ti6Al4V composite fabricated by laser melting deposition10.1016/j.ceramint.2017.09.054 ↗
17. Microstructure and tensile properties of TiCp/Ti6Al4V titanium matrix composites manufactured by laser melting deposition10.1016/j.jmatprotec.2017.10.005 ↗
18. In-situ TiB/near α Ti matrix composites manufactured by selective laser melting
19. Laser deposition-additive manufacturing of in situ TiB reinforced titanium matrix composites: TiB growth and part performance10.1007/s00170-017-0769-0 ↗
20. Electronic cigarette use among patients with cancer: Characteristics of electronic cigarette users and their smoking cessation outcomes
21. Effect of processing parameters on microstructure during laser-sustained plasma (LSP) nitriding of commercially-pure titanium10.1016/j.actamat.2016.01.051 ↗
22. Microstructure, hardness and cavitation erosion behaviour of Ti–6Al–4V laser nitrided under different gas atmospheres10.1179/174329407X169430 ↗
23. Laser gas–assisted nitriding of Ti alloys10.1016/B978-0-08-096532-1.00912-2 ↗
24. Improved high cycle fatigue performance of additively manufactured 17-4 pHstainless steel via in-process refining micro-/defect-structure
25. The effect of Ar and N2 shielding gas on laser weld porosity in steel, stainless steels, and nickel
26. Refined grain formation behavior and strengthening mechanism of α-titanium with nitrogen fabricated by selective laser melting
27. Selective laser-melted titanium materials with nitrogen solid solutions for balanced strength and ductility10.1016/j.msea.2020.139641 ↗
28. Strength-ductility improvement of extruded Ti-(N) materials using pure Ti powder with high nitrogen solution10.1016/j.msea.2020.139136 ↗
29. Selective laser melting under the reactive atmosphere: a convenient and efficient approach to fabricate ultrahigh strength commercially pure titanium without sacrificing ductility10.1016/j.msea.2019.138078 ↗
30. Study of pore defect and mechanical properties in selective laser melted Ti6Al4V alloy based on X-ray computed tomography10.1016/j.msea.2020.139981 ↗
31. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
32. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
33. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
34. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
35. Revealing martensitic transformation and α/β interface evolution in electron beam melting three-dimensional-printed Ti-6Al-4V10.1038/srep26039 ↗
36. Microstructural tailoring of As-selective laser melted Ti6Al4V alloy for high mechanical properties10.1016/j.jallcom.2019.152536 ↗
37. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective laser melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
38. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective laser melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
39. Examination of the twinning activity in additively manufactured Ti-6Al-4V10.1016/j.matdes.2018.02.015 ↗
40. The effect of SLM process parameters on density, hardness, tensile strength and surface quality of Ti-6Al-4V
41. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
42. Ductilization of selective laser melted Ti6Al4V alloy by friction stir processing10.1016/j.msea.2019.03.133 ↗
43. Controlling martensitic decomposition during selective laser melting to achieve best ductility in high strength Ti-6Al-4V10.1016/j.msea.2018.12.047 ↗
44. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
45. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
46. The influence of oxygen on the chemical composition and mechanical properties of Ti-6Al-4V during laser powder bed fusion (L-PBF)
47. Effects of oxygen content on tensile and fatigue performance of Ti-6Al-4V manufactured by selective laser melting10.1007/s11837-017-2590-5 ↗
48. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
49. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
50. Laser gas alloying of titanium alloy with nitrogen10.1016/0257-8972(93)90039-Q ↗
51. A.M. Kamat, S.M. Copley, J.A. Todd, Effect of CO2 laser-sustained nitrogen plasma on heat and mass transfer during laser-nitriding of commercially-pure titanium, in: Proceedings of the 13th World Conference Titan., 2016, pp. 893–898.10.1002/9781119296126.ch153 ↗
52. Investigations of laser-sustained plasma and its role in laser nitriding of titanium10.1088/0022-3727/45/18/185401 ↗
53. Lattice expansion of Ti-6Al-4V by nitrogen and oxygen absorption10.1016/j.matchar.2006.12.014 ↗
54. Oxygen and nitrogen concentrations in the Ti-6Al-4V alloy manufactured by direct metal laser sintering (DMLS) process10.1016/j.matlet.2017.08.037 ↗
55. Titanium and nitrogen interactions under laser additive manufacturing conditions10.1016/j.surfcoat.2019.124955 ↗
56. The interaction of titanium and titanium alloys with nitrogen at elevated temperatures. I. The kinetics and mechanism of the titanium-nitrogen reaction10.1007/BF00611698 ↗
57. The role of lattice defects, element partitioning and intrinsic heat effects on the microstructure in selective laser melted Ti-6Al-4V10.1016/j.actamat.2019.01.039 ↗
58. Inducing stable α + β microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments10.3390/ma10030268 ↗
59. Achieving Ti6Al4V alloys with both high strength and ductility via selective laser melting10.1016/j.msea.2019.138319 ↗
60. Diffusion of oxygen and nitrogen into titanium under laser irradiation in air10.1016/j.apsusc.2019.144578 ↗
61. A statistical theory of solid solution hardening10.1002/pssb.19700410221 ↗
62. Quantitative analysis on light elements solution strengthening in pure titanium sintered materials by Labusch model using experimental data10.2320/matertrans.Y-M2018849 ↗
63. Effect of interstitial solutes on the strength and ductility of titanium10.1016/0079-6425(81)90001-3 ↗
64. Six decades of the Hall–Petch effect – a survey of grain-size strengthening studies on pure metals10.1080/09506608.2016.1191808 ↗
65. Achieving grain refinement and enhanced mechanical properties in Ti–6Al–4V alloy produced by multidirectional isothermal forging10.1016/j.msea.2017.03.024 ↗