journal article·2022-07

An approach to improve the microstructure and mechanical properties: A hybrid manufacturing of laser directed energy deposition and shot peening

Xiaoyu Zhang, Sheng Huang, Dichen Li, Jiale Geng, Fan Yang, Qingyu Li

Publisher page

Abstract

As one of the most popular additive manufacturing technologies, laser directed energy deposition (LDED) has been extensively and deeply studied to improve the microstructure and properties of formed materials. Hybrid additive manufacturing(HAM) of LDED and shot peening is an innovative technology that combines the principle of surface strengthening and additive manufacturing. It can improve the mechanical properties and optimize the microstructure of the formed materials by strengthening the surface layer-by-layer. In this paper, the phase, oxygen content, microstructure, tensile properties, hardness and fracture morphology of the samples formed by LDED and HAM are compared. It is found that the mechanical properties of the forming samples are significantly improved by HAM, and the yield strength, ultimate tensile strength and average hardness are increased by 53%, 12% and 7%, respectively. Meanwhile, the microstructure of the sample is improved, some of the coarse columnar grains are refined, the heterogeneity of grain size is reduced, and the fibrous microstructure between layers is reduced. The hybrid additive manufacturing of LDED and shot peening can achieve high efficiency and high quality integrated manufacturing of forming parts, which is expected to promote its efficiency and applicability in practical cases in the future.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Gibson · 2015
2. Additive manufacturing
3. Overview of current additive manufacturing technologies and selected applications10.3184/003685012X13420984463047 ↗
4. Additive manufacturing (3D printing): a review of materials, methods, applications and challenges10.1016/j.compositesb.2018.02.012 ↗
5. Additive manufacturing in aerospace: examples and research outlook
6. Additive manufacturing: technology, applications and research needs10.1007/s11465-013-0248-8 ↗
7. A review of additive manufacturing10.5402/2012/208760 ↗
8. Additive manufacturing technologies—from rapid prototyping to rapid manufacturing—10.2493/jjspe.76.1340 ↗
9. R.M. Vilar, Laser cladding, in: Proc.SPIE, 11 (2003) 385–392. https://doi.org/10.1117/12.543724.10.1117/12.543724 ↗
10. Mechanical properties of laser-deposited Ti-6Al-4V
11. Laser additive manufacturing of high-performance metal compo- nents
12. J.-P. Kruth, B. Vandenbroucke, J. Vaerenbergh, P. Mercelis, Benchmarking of different SLS/SLM processes as Rapid Manufacturing techniques, Int. Conf. Polym. Mould. Innov. (2005). 〈http://purl.utwente.nl/publications/52902〉.
13. Selective laser melting of iron-based powder10.1016/j.jmatprotec.2003.11.051 ↗
14. Effects of cooling techniques after heat treatment of reinforced HSLA steels on their structure, tensile and impact properties
15. Y. Li, Y. Lee, J. Marchal, S. Kelly, W. Zhang, Meso-scale modeling of formation of balling defect in laser-powder bed fusion additive manufacturing, 10th Int. Conf. Trends Weld. Res, 2016. 〈https://www.osti.gov/servlets/purl/1408619〉.
16. High density selective laser melting of Waspaloy (R)10.1016/j.jmatprotec.2007.04.117 ↗
17. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
18. J. Donoghue, J. Sidhu, A. Wescott, P. Prangnell, Integration of Deformation Processing with Additive Manufacture of Ti-6A1–4V Components for Improved β Grain Structure and Texture, TMS2015 Suppl. Proc. (2015) 437–444. https://doi.org/https://doi.org/10.1002/9781119093466.ch55.10.1002/9781119093466.ch55 ↗
19. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling10.1016/j.jmatprotec.2013.04.012 ↗
20. 3D laser shock peening – a new method for the 3D control of residual stresses in Selective Laser Melting10.1016/j.matdes.2017.05.083 ↗
21. Numerical modeling design for the hybrid additive manufacturing of laser directed energy deposition and shot peening forming Fe-Cr-Ni-B-Si alloy10.3390/ma13214877 ↗
22. K.J. Kramer, A. Bayramian, B.S. El-Dasher, J.C. Farmer, System And Method For Enhanced Additive Manufacturing, 2014.
23. Stress relaxation of austenitic stainless steels at 290 °c10.1007/BF02643812 ↗
24. Effect of orientation and lamellar spacing of Fe2B on interfaces and corrosion behavior of Fe-B alloy in hot-dip galvanization10.1016/j.actamat.2016.06.016 ↗
25. Comparison of the microstructure and mechanical properties of FeCrNiBSi alloy fabricated by laser metal deposition in nitrogen and air
26. Microstructure and tensile behaviour of pure titanium produced after high-energy shot peening10.1080/02670836.2015.1121598 ↗
27. Microstructure and properties of Fe314 alloy cladding layer by laser cladding on EA4T steel
28. Improving the surface quality and mechanical properties by shot-peening of 17-4 stainless steel fabricated by additive manufacturing10.1016/j.matdes.2016.08.037 ↗
29. Effect of shot peening on mechanical and fatigue properties of AZ31 magnesium alloy processed by multi-axial alternative forging10.2464/jilm.62.265 ↗
30. The effect of surface plastic deformation produced by shot peening on corrosion behavior of a low-alloy steel10.1016/j.surfcoat.2019.01.003 ↗
31. Influences of fine-particle bombarding and conventional shot peening on surface properties of steel10.2320/matertrans.M2013322 ↗
32. The effect of shot peening on the cavitation erosion of pure iron and austenitic stainless steel in distilled and 1% salt waters10.1016/0043-1648(87)90145-1 ↗
33. S. Clitheroe, M. Turski, A. Evans, J. Kelleher, D. Hughes, P. Withers, Comparison of peening techniques on 304 austenitic stainless steel. 〈https://www.shotpeener.com/library/pdf/2008044.pdf〉, 2012, (accessed 26 March 2012).
34. Impact of the grain size distribution on the yield stress of heterogeneous materials10.1016/j.ijplas.2006.03.004 ↗
35. Tailoring the mechanical properties of laser cladding-deposited ferrous alloys with a mixture of 410L alloy and Fe–Cr–B–Si–Mo alloy powders10.3390/ma12030410 ↗
36. Additive manufacturing of 316L stainless steel by electron beam melting for nuclear fusion applications10.1016/j.jnucmat.2016.12.042 ↗
37. In-situ distortion prediction in metal additive manufacturing considering boundary conditions10.1007/s12541-021-00496-z ↗
38. Effect of shot peening on oxidation behavior of SS304H upon long term steam exposure10.1166/jnn.2018.15631 ↗
39. The effect of shot peening on steam oxidation of 304H stainless steel10.1007/s11085-019-09951-9 ↗
40. An approach to reduce stress and defects: a hybrid process of laser cladding deposition and shot peening10.1108/RPJ-06-2020-0129 ↗
41. Recrystallization behavior and tensile properties of laser metal deposited Inconel 718 upon in-situ ultrasonic impact peening and heat treatment10.1016/j.msea.2020.139434 ↗
42. Residual stress, mechanical properties, and grain morphology of Ti-6Al-4V alloy produced by ultrasonic impact treatment assisted wire and arc additive manufacturing10.3390/met8110934 ↗
43. Recrystallization behavior and tensile properties of laser metal deposited Inconel 718 upon in-situ ultrasonic impact peening and heat treatment10.1016/j.msea.2020.139434 ↗
44. Improvement in geometrical accuracy and mechanical property for arc-based additive manufacturing using metamorphic rolling mechanism10.1115/1.4032079 ↗
45. High-performance integrated additive manufacturing with laser shock peening –induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components10.1016/j.ijmachtools.2019.103475 ↗
46. Effects of heat treatment combined with laser shock peening on wire and arc additive manufactured Ti17 titanium alloy: microstructures, residual stress and mechanical properties
47. Microstructure and anisotropy of high performance TC4 obtained by micro forging laser cladding deposition
48. The effectiveness of combining rolling deformation with wire–arc additive manufacture on β-grain refinement and texture modification in Ti–6Al–4V10.1016/j.matchar.2016.02.001 ↗
49. Laser shock peening: a promising tool for tailoring metallic microstructures in selective laser melting10.1016/j.jmatprotec.2018.11.024 ↗
50. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
51. Defects in a laser powder bed fused tool steel
52. On the relationship between yield stress and fatigue crack initiation life of metals