journal article·2023-08

Precipitation behavior and strengthening-toughening mechanism of additive friction stir-deposited Al–Mg–Si–Cu alloy

Wenshen Tang, Xinqi Yang, Ting Luo, Ruilin Wang, Chao Gu

Publisher page

Abstract

An 18-layer thick-walled Al–Mg–Si–Cu alloy part with a width of 32 mm and single-layer thickness of 4 mm was fabricated using force-controlled additive friction stir welding. The evolution of the grain structure and second-phase particles during multilayer deposition was investigated in detail. After being subjected to multi-pass thermal cycles and plastic deformation, the recrystallization fraction and grain size of the final deposits were almost unaffected. Interface grain refinement was more pronounced, with grain sizes reaching 3.4–4.2 µm, owing to greater recrystallization compared to the interlayer. The reprecipitated Q` and β` precipitates, which were coherent or semicoherent with the aluminum matrix and attached to the diffusely distributed spherical Al(MnCrFe)Si dispersoids, played a critical role in strengthening the final deposits. After repeated heat input and plastic deformation thrice or more, the hardness and tensile properties of the deposits remained unchanged because the quantity and distribution of the precipitates did not vary. The average tensile strength (Rm) and elongation (A) after fracture of the final deposits along the tool traverse direction could reach 182.4 MPa and 37.3%, respectively. The mean values of Rm and A along the build direction reached 92.2% and 50.5% of those along the tool traverse direction. Owing to the refined grains produced at the metallurgically bonded interface, fine diffusely distributed dispersoids, and coordinated deformation of alternating coarse and fine-grain regions, the tear toughness of the as-printed deposits could reach 132.4–208.7% of that of the wrought 6061-T6 Al alloy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
2. Aluminum with dispersed nanoparticles by laser additive manufacturing10.1038/s41467-019-12047-2 ↗
3. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
4. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
5. A high-performance WAAM process for Al–Mg–Mn using controlled short-circuiting metal transfer at increased wire feed rate and increased travel speed10.1016/j.matdes.2020.109040 ↗
6. Rationalization of anisotropic mechanical properties of Al-6061 fabricated using ultrasonic additive manufacturing10.1016/j.actamat.2016.06.048 ↗
7. Non-beam-based metal additive manufacturing enabled by additive friction stir deposition10.1016/j.scriptamat.2018.03.025 ↗
8. Influence of texture and grain refinement on the mechanical behavior of AA2219 fabricated by high shear solid state material deposition10.1016/j.msea.2018.03.088 ↗
9. Microstructures and mechanical behavior of Inconel 625 fabricated by solid-state additive manufacturing10.1016/j.msea.2017.03.105 ↗
10. Microstructural heterogeneity and bonding strength of planar interface formed in additive manufacturing of Al−Mg−Si alloy based on friction and extrusion10.1007/s12613-022-2506-4 ↗
11. In situ investigation into temperature evolution and heat generation during additive friction stir deposition: a comparative study of Cu and Al-Mg-Si
12. Influence of rotation speed on interfacial bonding mechanism and mechanical performance of aluminum 6061 fabricated by multilayer friction-based additive manufacturing10.1007/s00170-023-11378-1 ↗
13. Microstructure-deformation relationship of additive friction stir-deposition Al–Mg–Si10.1016/j.mtla.2019.100387 ↗
14. Effect of thermomechanical processing on fatigue behavior in solid-state additive manufacturing of Al-Mg-Si alloy
15. Solid-state additive manufacturing of aluminum and copper using additive friction stir deposition: Process-microstructure linkages10.1016/j.mtla.2020.100967 ↗
16. Precipitation in AA6063 produced from swarf using additive friction stir deposition
17. Microstructure evolution of Al6061 alloy made by additive friction stir deposition
18. Effect of rotation speed on microstructure and mechanical anisotropy of Al-5083 alloy builds fabricated by friction extrusion additive manufacturing10.1016/j.msea.2022.144237 ↗
19. Interfacial grain structure, texture and tensile behavior of multilayer deformation-based additively manufactured Al 6061 alloy10.1016/j.matchar.2023.112646 ↗
20. Coupled precipitation and yield strength modelling for non-isothermal treatments of a 6061 aluminium alloy10.1016/j.actamat.2013.09.041 ↗
21. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al-Mg-Si alloys10.1016/j.actamat.2015.07.039 ↗
22. Aging behavior of Al 6061 alloy processed by high-pressure torsion and subsequent aging10.1007/s11661-015-2840-5 ↗
23. Modelling of the age hardening behaviour of Al-Mg-Si alloys10.1016/S1359-6454(00)00301-3 ↗
24. Improving thermal stability in Cu-containing Al-Mg-Si alloys by precipitate optimization10.1007/s11661-014-2250-0 ↗
25. Microstructure behavior of Al-Mg-Sc alloy processed by ECAP at elevated temperature10.1016/j.actamat.2007.10.029 ↗
26. The influence of post-weld tempering temperatures on microstructure and strength in the stir zone of friction stir welded reduced activation ferritic/martensitic steel10.1016/j.msea.2021.141224 ↗
27. Bobbin and conventional friction stir welding of thick extruded AA6005-T6 profiles10.1016/j.matdes.2016.06.089 ↗
28. Texture control by thermomechanical processing of AA6xxx Al-Mg-Si sheet alloys for automotive applications - a review10.1016/S0921-5093(01)01968-2 ↗
29. The structural and compositional evolution of precipitates in Al-Mg-Si-Cu alloy10.1016/j.actamat.2017.12.036 ↗
30. Hot deformation of AA6082 containing fine intermetallic particles10.1007/s11661-012-1487-8 ↗
31. Microstructure and mechanical properties of Al−Mg−Si alloy U-shaped profile10.1016/S1003-6326(20)65431-0 ↗
32. Metastable phases in an Al-Mg-Si alloy containing copper10.1007/s11661-001-0219-2 ↗
33. Study of intergrown L and Q′ precipitates in Al-Mg-Si-Cu alloys10.1016/j.scriptamat.2011.01.008 ↗
34. Phase relations and precipitation in Al-Mg-Si alloys with Cu additions10.1016/S0079-6425(03)00031-8 ↗
35. The effects of low Cu additions and predeformation on the precipitation in a 6060 Al-Mg-Si alloy10.1007/s11661-013-1754-3 ↗
36. Precipitate characteristics and selected area diffraction patterns of the β′ and Q′ precipitates in Al-Mg-Si-Cu alloys10.1080/09500839.2010.541165 ↗
37. The effect of constituent particles on the tear resistance of three 6000-series aluminium alloys10.1007/s10704-022-00658-8 ↗
38. The effect of Ag on the tensile strength and fracture toughness of novel Al-Mg-Zn alloys10.1016/j.jallcom.2022.164640 ↗
39. Effects of Cu content and preaging on precipitation characteristics in aluminum alloy 602210.1007/s11661-000-0272-2 ↗
40. Study of the developed precipitates in Al-0.63Mg-0.37Si-0.5Cu (wt%) alloy by using DSC and TEM techniques10.1016/j.jallcom.2006.06.004 ↗
41. Effect of cryorolling and warm rolling on precipitation evolution in Al 6061 alloy10.1016/j.msea.2014.03.031 ↗
42. The effects of preaging treatments on aging kinetics and mechanical properties in AA6111 aluminum autobody sheet10.1007/s11661-999-0010-3 ↗
43. The interaction between Mn and Fe on the precipitation of Mn/Fe dispersoids in Al-Mg-Si-Mn-Fe alloys10.1016/j.scriptamat.2018.04.012 ↗
44. Precipitation of dispersoids containing Mn and/or Cr in Al-Mg-Si alloys10.1016/S0921-5093(00)00734-6 ↗
45. Crystallographic study of grain refinement in aluminum alloys using the edge-to-edge matching model10.1016/j.actamat.2004.11.037 ↗
46. Transition of tensile deformation behaviors in ultrafine-grained aluminum10.1016/j.actamat.2005.05.005 ↗
47. Transmission electron microscopy study of the β′ phase (Al-Mg-Si alloys) and QC phase (Al-Cu-Mg-Si alloys): ordering mechanism and crystallographic structure10.1016/S1359-6454(00)00057-4 ↗
48. Recovery of deformation substructure and coarsening of particles on annealing severely plastically deformed Al-Mg-Si alloy and analysis of strengthening mechanisms10.1557/jmr.2006.0063 ↗
49. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
50. Tensile behavior of bulk nanostructured and ultrafine grained aluminum alloys10.1023/A:1025150407956 ↗
51. Creep of magnesium strengthened with high volume fractions of yttria dispersoids10.1016/S0921-5093(00)01781-0 ↗
52. Strengthening mechanisms in a Zr-modified 5083 alloy deformed to high strains10.1016/j.msea.2014.10.030 ↗