journal article·2023-01

Multilayered gradient titanium-matrix composites fabricated by multi-material laser powder bed fusion using metallized ceramic: Forming characteristics, microstructure evolution, and multifunctional properties

Rui Wang, Dongdong Gu, Guangjing Huang, Keyu Shi, Luhao Yuan, Han Zhang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Recent developments and opportunities in additive manufacturing of titanium-based matrix composites: A review10.1016/j.ijmachtools.2018.06.003 ↗
2. In-situ formation of laser Ti6Al4V-TiB composite coatings on Ti6Al4V alloy for biomedical application10.1016/j.surfcoat.2015.10.079 ↗
3. Multiscale architecture and superior high-temperature performance of discontinuously reinforced titanium matrix composites
4. High-mass-proportion TiCp/Ti6Al4V titanium matrix composites prepared by directed energy deposition
5. Microstructure, mechanical and thermal properties of titanium matrix composites with different reinforcements10.1088/2053-1591/ac8f1f ↗
6. Microstructure evolution of sub-critical annealed laser deposited Ti-6Al-4V alloy10.1016/j.matdes.2011.12.016 ↗
7. Microstructure and mechanical properties of functionally graded TiCp/Ti6Al4V composite fabricated by laser melting deposition10.1016/j.ceramint.2017.09.054 ↗
8. Direct fabrication of compositionally graded Ti-Al2O3 multi-material structures using Laser Engineered Net Shaping
9. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: Microstructure evolution and tribological behavior10.1016/j.powtec.2018.09.088 ↗
10. The influences of melting degree of TiC reinforcements on microstructure and mechanical properties of laser direct deposited Ti6Al4V-TiC composites10.1016/j.matdes.2017.09.063 ↗
11. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders
12. Microstructure and properties of insitu titanium boride (TiB)/titanium (TI) composites10.1016/j.msea.2015.09.067 ↗
13. Selective laser melting of in situ titanium-titanium boride composites: Processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
14. Comparative study of microstructures and mechanical properties of in situ Ti-TiB composites produced by selective laser melting, powder metallurgy, and casting technologies10.1557/jmr.2014.122 ↗
15. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting10.1016/j.compositesb.2020.108567 ↗
16. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: A comparative study10.1016/j.msea.2020.140415 ↗
17. Microstructure and tensile properties of TiCp/Ti6Al4V titanium matrix composites manufactured by laser melting deposition10.1016/j.jmatprotec.2017.10.005 ↗
18. Melt pool geometry and microstructure of Ti6Al4V with B additions processed by selective laser melting additive manufacturing10.1016/j.matdes.2019.108126 ↗
19. Graded layered titanium composite structures with TiB2 inclusions fabricated by selective laser melting10.1016/j.compstruct.2016.11.013 ↗
20. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
21. Formation mechanisms of TiB2 tracks on Ti6Al4V alloy during selective laser melting of ceramic-metal multi-material10.1016/j.powtec.2020.04.027 ↗
22. Microstructural characterization and failure mechanism of vacuum plasma sprayed Ti-6Al-4V/B4C composite10.1016/j.vacuum.2014.03.028 ↗
23. Metallic integrated thermal protection structures inspired by the Norway spruce stem: Design, numerical simulation and selective laser melting fabrication10.1016/j.optlastec.2019.02.003 ↗
24. Stress and deformation evaluations of scanning strategy effect in selective laser melting
25. Evolution of solidification texture during additive manufacturing10.1038/srep16446 ↗
26. Selective laser melted TiB2/Ti6Al4V graded materials and first-principle calculations10.1016/j.matlet.2019.07.015 ↗
27. First principles calculation of single-crystal elastic constants of titanium tetraboride (Ti3B4) and experimental validation10.1111/jace.15562 ↗
28. Microstructure evolution and mechanical properties of TiB/Ti6Al4V gradient-material lattice structure fabricated by laser powder bed fusion10.1016/j.compositesb.2020.108417 ↗
29. Effect of boron addition on microstructure, hardness and wear performance of Ti-6Al-4 V alloy manufactured by laser powder bed fusion additive manufacturing10.1016/j.matchar.2020.110848 ↗
30. Laser additive manufacturing of layered TiB2/Ti6Al4V multi-material parts: Understanding thermal behavior evolution10.1016/j.optlastec.2019.105666 ↗
31. Microstructure evolution and mechanical properties of TIG cladded TiB reinforced composite coating on Ti-6Al-4V alloy10.1016/j.vacuum.2017.09.019 ↗
32. Anisotropic corrosion resistance of TiC reinforced Ni-based composites fabricated by selective laser melting10.1016/j.jmst.2018.12.020 ↗
33. Multi-layered structures of Ti-6Al-4V alloy and TiC and TiB composites on its base fabricated using blended elemental powder metallurgy10.1016/j.jmatprotec.2019.02.006 ↗
34. Influence of spark plasma sintering and subsequent hot rolling on microstructure and flexural behavior of in-situ TiB and TiC reinforced Ti6Al4V composite10.1016/j.msea.2014.11.036 ↗
35. Analytical and experimental investigation of the effect of SPS and hot rolling on the microstructure and flexural behavior of Ti6Al4V matrix reinforced with in-situ TiB and TiC10.1016/j.jallcom.2016.09.026 ↗
36. Effect of aspect ratios of in situ formed TiB whiskers on the mechanical properties of TiB w/Ti-6Al-4V composites10.1016/j.scriptamat.2011.12.024 ↗
37. Microstructure and mechanical properties of TiB–TiB 2 ceramic matrix composites fabricated by spark plasma sintering10.1016/j.msea.2011.01.096 ↗
38. Mechanical behavior of titanium-based layered structures fabricated using blended elemental powder metallurgy10.1007/s11665-019-04263-0 ↗
39. Study on tribological properties of new TiAl based self-lubricating alloys10.1088/1757-899X/504/1/012006 ↗
40. Comparative investigation on microstructures and mechanical properties of (TiB + TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems10.1016/j.matchar.2018.04.010 ↗
41. Flexural properties, thermal conductivity and electrical resistivity of prealloyed and master alloy addition powder metallurgy Ti-6Al-4V10.1016/j.matdes.2013.06.036 ↗
42. Influence of the electric pulse on springback during stretch U-bending of Ti6Al4V titanium alloy sheets10.1016/j.jmatprotec.2018.05.030 ↗
43. Effect of coating thickness on microstructure, mechanical properties and fracture behaviour of cold sprayed Ti6Al4V coatings on Ti6Al4V substrates10.1016/j.surfcoat.2018.05.060 ↗
44. Experimental and numerical investigation on bending behavior of Ti-6Al-4V parts produced by additive metal laser sintering10.1007/s11665-021-06192-3 ↗
45. Influence of sintering parameters on the properties of powder metallurgy Ti-3Al-2.5V alloy10.1016/j.matchar.2013.07.009 ↗
46. The positive effect of hot isostatic pressing on improving the anisotropies of bending and impact properties in selective laser melted Ti-6Al-4V alloy10.1016/j.msea.2016.02.023 ↗
47. Interfacial characteristics and mechanical properties of TiAl/Ti6Al4V laminate composite (LMC) fabricated by vacuum hot pressing10.1016/j.msea.2018.07.086 ↗
48. Microstructure and properties of the Ti6Al4V / Inconel 625 bimetal obtained by explosive joining10.1007/s11665-016-2080-x ↗
49. Material properties of titanium diboride10.6028/jres.105.057 ↗
50. Additive manufacturing of Inconel 718—Copper alloy bimetallic structure using laser engineered net shaping (LENS™)