Sustained Immersion Tin Deposition on Copper from Choline Chloride Based Aqueous Solution without Reducing Agent
Source abstract
Abstract
Sustained immersion tin (Sn) deposition onto a copper (Cu) surface was achieved from choline chloride aqueous (ChCl-H 2 O) solution free of reducing agents. The electrode potentials of Cu and Sn were investigated by open-circuit potential (OCP) to reveal the driving force of Sn deposition process in ChCl-H 2 O solution. Thiourea reversed the electrode potentials of Cu and Sn, causing the replacement reaction between Sn 2+ and Cu occurring. The replacement reaction is significantly influenced by the concentration of ChCl, SnCl 2 , and thiourea. The phenomenon of sustained Sn deposition was mainly facilitated by diffusing of Cu into the Sn coating and the reaction between Sn 2+ and Cu + . Furthermore, Sn coating got in ChCl-H 2 O solution had fairly good performance such as solderability.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Electronic Packaging and Soldering Technologies · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. 10.1149/1.235811910.1149/1.2358119 ↗
2. 10.1149/1.209663910.1149/1.2096639 ↗
3. 10.1016/j.jmatprotec.2005.04.11310.1016/j.jmatprotec.2005.04.113 ↗
4. 10.1016/S0257-8972(02)00412-710.1016/S0257-8972(02)00412-7 ↗
5. 10.1108/0305612991024451810.1108/03056129910244518 ↗
6. 10.1016/j.surfcoat.2007.06.00410.1016/j.surfcoat.2007.06.004 ↗
7. 10.1016/j.apsusc.2007.03.06910.1016/j.apsusc.2007.03.069 ↗
8. 10.1016/j.jallcom.2008.09.07410.1016/j.jallcom.2008.09.074 ↗
9. 10.1016/j.electacta.2010.01.06510.1016/j.electacta.2010.01.065 ↗
10. 10.1016/S0040-6090(02)01136-710.1016/S0040-6090(02)01136-7 ↗
11. 10.1016/j.fluid.2003.08.02010.1016/j.fluid.2003.08.020 ↗
12. 10.1039/B106357J10.1039/B106357J ↗
13. 10.1039/B210714G10.1039/B210714G ↗
14. 10.1021/ja048266j10.1021/ja048266j ↗
15. 10.1039/c0gc00395f10.1039/c0gc00395f ↗
16. 10.1016/j.electacta.2005.12.03010.1016/j.electacta.2005.12.030 ↗
17. 10.1039/b607763n10.1039/b607763n ↗
18. 10.1016/j.jelechem.2006.04.02410.1016/j.jelechem.2006.04.024 ↗
19. 10.1039/b703954a10.1039/b703954a ↗
20. 10.1016/j.surfcoat.2007.08.05510.1016/j.surfcoat.2007.08.055 ↗
21. 10.1149/2.012304jes10.1149/2.012304jes ↗
22. 10.1016/j.surfcoat.2007.05.05510.1016/j.surfcoat.2007.05.055 ↗
23. 10.4028/www.scientific.net/AMR.139-141.41010.4028/www.scientific.net/AMR.139-141.410 ↗
24. 10.1016/j.jmatprotec.2005.04.11310.1016/j.jmatprotec.2005.04.113 ↗
25. 10.2320/matertrans.M201132210.2320/matertrans.M2011322 ↗
26. 10.4028/www.scientific.net/AMR.154-155.105310.4028/www.scientific.net/AMR.154-155.1053 ↗
27. Zhang Y. C. Hu X. N. Xiang R. , in Plating Handbook, 3rd ed., p. 541, National Defense Industry Press, China (2007).