Electrochemical Sulfur Oxidation in Solid Oxide Fuel Cells Studied by Near Infrared Thermal Imaging and Chronocoulometry
Source abstract
Abstract
A newly adapted electrochemical technique, chronocoulometry, was used to characterize sulfur’s effect on the performance of porous Ni-YSZ anodes in electrolyte supported, solid oxide fuel cells (SOFCs) operating with dry H2 at 600 °C, 650 °C, 700 °C and 800 °C. Chronocoulometry data together with near-infrared thermal imaging show that H2S poisoning is more complex than sulfur simply blocking electrochemically active sites. Thermal imaging supports findings that SOFC susceptibility to sulfur poisoning depends strongly on temperature with higher performance and greater sulfur tolerance at higher temperatures. Chronocoulometry data are consistent with this description. Chronocoulometry results, however, are also more nuanced and show that sulfur adsorbed to the triple phase boundary (TPB) can be electrochemically oxidized, thereby limiting performance loss that would result simply from blocked or inaccessible electrochemically active sites. Furthermore, chronocoulometry results imply an increased TPB length at higher operating temperatures and suggest that the spatial extent of a SOFC electrode’s electrochemically active region plays a significant role in electrode surface chemistry. A simple model is developed to interpret the chronocoulometry results and determine the relative amount of sulfur adsorbed to the anode’s active triple phase boundary.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Trembly · J. Power Sources · 2007 · 169 · 34710.1016/j.jpowsour.2007.03.018 ↗
2. Rasi · Energy · 2007 · 32 · 137510.1016/j.energy.2006.10.018 ↗
3. Marina · J. Power Sources · 2010 · 195 · 703310.1016/j.jpowsour.2010.05.006 ↗
4. Reeping · J. Electrochem. Soc. · 2015 · 162 · F131010.1149/2.0191512jes ↗
5. Reeping · J. Power Sources · 2017 · 372 · 18810.1016/j.jpowsour.2017.10.071 ↗
6. Reeping · Sustain. Energ. Fuels · 2017 · 1 · 132010.1039/C7SE00156H ↗
7. Reeping · J. Phys. Chem. C · 2017 · 121 · 258810.1021/acs.jpcc.6b11548 ↗
8. Haga · J. Electrochem. Soc. · 2008 · 155 · B123310.1149/1.2980521 ↗
9. Gong · J. Power Sources · 2007 · 168 · 28910.1016/j.jpowsour.2007.03.026 ↗
10. Cheng · Solid State Ionics · 2007 · 178 · 92510.1016/j.ssi.2007.04.004 ↗
11. Cheng · Energy Environ. Sci. · 2011 · 4 · 438010.1039/c1ee01758f ↗
12. Sasaki · J. Power Sources · 2011 · 196 · 913010.1016/j.jpowsour.2010.09.122 ↗
13. Zeng · Phys. Chem. Chem. Phys. · 2013 · 15 · 676910.1039/c3cp51099a ↗
14. Gur · Prog. Energy Combust. Sci. · 2016 · 54 · 110.1016/j.pecs.2015.10.004 ↗
15. Mahato · Prog. Mater Sci. · 2015 · 72 · 14110.1016/j.pmatsci.2015.01.001 ↗
16. Niu · Electrochim. Acta · 2018 · 274 · 9110.1016/j.electacta.2018.04.066 ↗
17. Xue · Journal of Materials Chemistry A · 2019 · 7 · 2178310.1039/C9TA07027C ↗
18. Roushanafshar · Appl. Catal. B-Environ. · 2015 · 176 · 62710.1016/j.apcatb.2015.04.046 ↗
19. Boldrin · Chem. Rev. · 2016 · 116 · 1363310.1021/acs.chemrev.6b00284 ↗
20. Blinn · Energy & Environmental Science · 2012 · 5 · 791310.1039/c2ee21499g ↗
21. Hagen · J. Power Sources · 2011 · 196 · 727110.1016/j.jpowsour.2011.02.053 ↗
22. Yamada · J. Electrochem. Soc. · 2015 · 162 · F110710.1149/2.0061511jes ↗
23. Sasaki · J. Electrochem. Soc. · 2006 · 153 · A202310.1149/1.2336075 ↗
24. Sulfur Poisoning of SOFC Anodes: Effect of Overpotential on Long-Term Degradation10.1149/2.080406jes ↗
25. Matsuzaki · Solid State Ionics · 2000 · 132 · 26110.1016/S0167-2738(00)00653-6 ↗
26. Lohsoontorn · J. Power Sources · 2008 · 175 · 6010.1016/j.jpowsour.2007.09.065 ↗
27. Wang · J. Chem. Phys. · 2007 · 127 · 21470510.1063/1.2801985 ↗
28. Yap · Opt. Lett. · 1996 · 21 · 134810.1364/OL.21.001348 ↗
29. Dong · J. Power Sources · 2006 · 156 · 46110.1016/j.jpowsour.2005.06.016 ↗
30. Cheng · J. Phys. Chem. C · 2007 · 111 · 1799710.1021/jp0770209 ↗
31. Thi · Solid State Ionics · 2015 · 272 · 8410.1016/j.ssi.2015.01.007 ↗
32. Pomfret · Anal. Chem. · 2007 · 79 · 236710.1021/ac062189o ↗
33. Steinhurst · J. Power Sources · 2010 · 195 · 25710.1016/j.jpowsour.2009.06.072 ↗
34. Kirtley · Phys. Chem. Chem. Phys. · 2014 · 16 · 22710.1039/C3CP53278J ↗
35. Kirtley · J. Phys. Chem. C · 2015 · 119 · 1278110.1021/jp511304x ↗
36. Kirtley · J. Power Sources · 2016 · 336 · 5410.1016/j.jpowsour.2016.10.047 ↗
37. Rutman · Electrochim. Acta · 2007 · 52 · 607310.1016/j.electacta.2007.03.033 ↗
38. Offer · Electrochim. Acta · 2008 · 53 · 761410.1016/j.electacta.2008.04.001 ↗
39. Primdahl · J. Electrochem. Soc. · 1997 · 144 · 340910.1149/1.1838026 ↗
40. Eigenbrodt · J. Phys. Chem. C · 2011 · 115 · 289510.1021/jp109292r ↗
41. Kirtley · Anal. Chem. · 2012 · 84 · 974510.1021/ac301504g ↗
42. Kirtley · Solid Oxide Fuel Cells 15 (Sofc-Xv) · 2017 · 78 · 1261
43. Bard · 2001
44. Pomeroy · ECS Trans. · 2019 · 91 · 181510.1149/09101.1815ecst ↗
45. Welander · J. Electrochem. Soc. · 2018 · 165 · F15210.1149/2.0531803jes ↗
46. Rasmussen · J. Power Sources · 2009 · 191 · 53410.1016/j.jpowsour.2009.02.001 ↗
47. Stoltz · Anal. Chem. · 2005 · 77 · 179110.1021/ac048600u ↗
48. Rostrupnielsen · J. Catal. · 1968 · 11 · 22010.1016/0021-9517(68)90035-3 ↗
49. Prasad · J. Electrochem. Soc. · 2014 · 161 · F20810.1149/2.031403jes ↗
50. Burgess · 2000