In-situ hot rolling directed energy deposition-arc repair of shafts
Source abstract
Abstract
The shaft is a key component in mechanical systems and it needs to be repaired and replaced regularly due to long-term service in harsh conditions. However, using the directed energy deposition-arc (DED-arc) technology to repair the shaft results in columnar grains in the repair layer which affects the repair quality. In this study, the repair process of shafts by combining DED-arc and in-situ hot rolling was investigated, in which the material was rolled immediately after deposition, and plastic deformation occurred at high temperatures. A novel piece of equipment was developed, fabricated, and tested, and repair experiments were carried out on a 316 L stainless steel shaft. The effects of rolling on the tensile properties, hardness, and microstructure of the repaired parts were investigated, and electron backscatter diffraction (EBSD) characterization was performed on the deposited layers and interfaces to explore the hot deformation mechanism during the rolling process. The results showed that rolling led to dynamic recrystallization (DRX) nucleation and produced a large number of low angle grain boundaries (LAGBs) with high dislocation density, and static recrystallization occurred during subsequent deposition, thus refining the microstructure. Compared to the base metal, the hardness of the repaired layer increased by 20 %−30 %, and the yield strength and ultimate tensile strength increased from 220 MPa to 432 MPa and from 540 MPa to 595 MPa, respectively, with almost constant elongation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Repair of spline shaft by laser-cladding coarse TiC reinforced Ni-based coating: process, microstructure and properties10.1016/j.ceramint.2021.07.189 ↗
2. Torsional vibration and fatigue evaluation in repairing the worn shafting of the steam turbine10.1016/j.engfailanal.2012.06.001 ↗
3. Environmental life cycle assessment of remanufactured engines with advanced restoring technologies10.1016/j.rcim.2019.04.005 ↗
4. Application of directed energy deposition-based additive manufacturing in repair10.3390/app9163316 ↗
5. Microstructure and mechanical properties of electro-brush plated Fe/MWCNTs composite coatings10.1016/j.surfcoat.2018.05.034 ↗
6. A critical review on thermal spray based manufacturing technologies
7. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
8. Damage detection and reconstruction algorithm in repairing compressor blade by direct metal deposition10.1007/s00170-017-1413-8 ↗
9. Microstructure and nanoindentation creep behavior of IC10 directionally solidified superalloy repaired by laser metal deposition10.1016/j.msea.2021.140911 ↗
10. Damage reconstruction from tri-dexel data for laser-aided repairing of metallic components10.1007/s00170-018-1830-3 ↗
11. Invited review article: strategies and processes for high quality wire arc additive manufacturing
12. Current status and perspectives on wire and arc additive manufacturing (WAAM)10.3390/ma12071121 ↗
13. Repairing surface defects of metal parts by groove machining and wire plus arc based filling10.1016/j.jmatprotec.2019.116268 ↗
14. Life-cycle energy and carbon saving potential of wire arc additive manufacturing for the repair of mold inserts10.1016/j.cirpj.2021.10.007 ↗
15. Repair of damaged parts using wire arc additive manufacturing in machine tools10.1016/j.jmrt.2021.11.156 ↗
16. Micro-plasma transferred arc additive manufacturing for die and mold surface remanufacturing10.1007/s11837-016-1932-z ↗
17. Microstructure and mechanical properties of wire arc additive repairing Ti-6.5Al-2Sn-2Zr-4Mo-4Cr titanium alloy10.1080/02670836.2020.1822061 ↗
18. Effects of trace Sn and Cr addition on microstructure and mechanical properties of TC17 titanium alloy repaired by wire arc additive manufacturing10.1016/j.jallcom.2021.161473 ↗
19. Wire arc additive manufacturing for repairing aluminium structures in marine applications10.1016/j.matlet.2021.130112 ↗
20. Repairing casting part using laser assisted additive metal-layer deposition and its mechanical properties10.1016/j.optlastec.2018.04.007 ↗
21. Microstructure evolution and mechanical properties of a nickel-based superalloy repaired using wire and arc additive manufacturing10.1016/j.matchar.2022.112315 ↗
22. Hot forging wire and arc additive manufacturing (HF-WAAM)
23. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components10.1016/j.scriptamat.2016.10.031 ↗
24. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling10.1016/j.jmatprotec.2013.04.012 ↗
25. The effectiveness of combining rolling deformation With Wire-arc Additive Manufacture on beta-grain refinement and texture modification in Ti-6Al-4V10.1016/j.matchar.2016.02.001 ↗
26. Interpass rolling of Ti-6Al-4V wire + arc additively manufactured features for microstructural refinement
27. Control of residual stress and distortion in aluminium wire plus arc additive manufacture with rolling
28. Residual stress and texture control in Ti-6Al-4V wire + arc additively manufactured intersections by stress relief and rolling10.1016/j.matdes.2018.03.065 ↗
29. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
30. Micropore evolution in additively manufactured aluminum alloys under heat treatment and inter-layer rolling10.1016/j.matdes.2019.108288 ↗
31. Hybrid direct manufacturing method of metallic parts using deposition and micro continuous rolling10.1108/RPJ-01-2012-0006 ↗
32. HDMR technology for the aircraft metal part10.1108/RPJ-05-2015-0047 ↗
33. Investigation of mechanical properties for hybrid deposition and micro-rolling of bainite steel10.1016/j.jmatprotec.2017.07.023 ↗
34. Influence of in situ micro-rolling on the improved strength and ductility of hybrid additively manufactured metals10.1016/j.engfracmech.2021.107868 ↗
35. Defect-correlated fatigue resistance of additively manufactured Al-Mg4.5Mn alloy with in situ micro-rolling10.1016/j.jmatprotec.2020.117039 ↗
36. The study of hot deformation on laser cladding remanufactured 316L stainless steel10.1016/j.matdes.2021.110255 ↗
37. Effect of heat treatment temperature on microstructure and tensile properties of austenitic stainless 316L using wire and arc additive manufacturing10.1016/j.msea.2021.142446 ↗
38. Grain refinement by dynamic recrystallization during laser direct energy deposition of 316L stainless steel under thermal cycles10.1016/j.jmapro.2022.01.057 ↗
39. Microstructure evolution of wire-arc additively manufactured 2319 aluminum alloy with interlayer hammering10.1016/j.msea.2020.140168 ↗
40. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
41. The effect of repeated repair welding on mechanical and corrosion properties of stainless steel 316L10.1016/j.matdes.2013.08.052 ↗
42. Microstructural characterisation of thick-walled wire arc additively manufactured stainless steel10.1016/j.jmatprotec.2021.117373 ↗
43. Microstructure, hardness and petroleum corrosion evaluation of 316L/AWS E309MoL-16 weld metal10.1016/j.matchar.2008.09.017 ↗
44. Effect of in-situ layer-by-layer rolling on the microstructure, mechanical properties, and corrosion resistance of a directed energy deposited 316L stainless steel
45. Correlation between arc mode, microstructure, and mechanical properties during wire arc additive manufacturing of 316L stainless steel10.1016/j.msea.2019.02.078 ↗
46. Study on microstructure and tensile properties of 316L stainless steel fabricated by CMT wire and arc additive manufacturing10.1016/j.msea.2020.140006 ↗
47. Fabrication of 316L nuclear nozzles on the main pipeline with large curvature by CMT wire arc additive manufacturing and self-developed slicing algorithm10.1016/j.msea.2021.141539 ↗
48. Revealing relationships between heterogeneous microstructure and strengthening mechanism of austenitic stainless steels fabricated by directed energy deposition (DED)10.1016/j.jmrt.2021.08.036 ↗
49. Strengthening mechanisms in directed energy deposited austenitic stainless steel10.1016/j.actamat.2018.11.021 ↗
50. Tensile properties, strain rate sensitivity, and activation volume of additively manufactured 316L stainless steels10.1016/j.ijplas.2019.05.009 ↗
51. Tensile properties of a nanocrystalline 316L austenitic stainless steel10.1016/j.scriptamat.2005.01.023 ↗
52. Strengthening mechanisms in selective laser melted 316L stainless steel10.1016/j.msea.2021.142434 ↗
53. Orientation-dependent evolution of the dislocation density in grain populations with different crystallographic orientations relative to the tensile axis in a polycrystalline aggregate of stainless steel10.1016/j.actamat.2013.11.012 ↗
54. Enhancement of an additive-manufactured austenitic stainless steel by post- manufacture heat-treatment10.1016/j.msea.2019.04.111 ↗
55. Geometrically necessary dislocations distribution in face-centred cubic alloy with varied grain size10.1016/j.matchar.2020.110205 ↗