journal article·2025-02Open access

Microstructure tailoring for crack mitigation in CM247LC manufactured by powder bed fusion – Laser beam

Ahmed Fardan, Andrea Fazi, Jakob Schröder, Tatiana Mishurova, Tobias Deckers, Giovanni Bruno, Mattias Thuvander, Andreas Markström, Håkan Brodin, Eduard Hryha

Abstract

Tailored microstructures in powder bed fusion – laser beam (PBF-LB) can aid in crack mitigation of non-weldable Ni-base superalloys such as CM247LC. This study explores the effect of a range of stripe widths from 5 mm down to 0.2 mm to control solidification cracking, microstructure, and residual stress in CM247LC manufactured by PBF-LB. The decrease in melt pool depth with the reduction in stripe width from 5 to 0.2 mm promoted the < 100 > crystallographic texture along the build direction. The crack density measurements indicated that there is an increase from 0.62 mm/mm 2 (5 mm) to 1.71 mm/mm 2 (1 mm) followed by a decrease to 0.33 mm/mm 2 (0.2 mm). Atom probe tomography investigations at high-angle grain boundaries revealed that there is higher Hf segregation in 0.2 mm stripe width when compared to 5 mm. This indicates that the cracking behavior is likely influenced by the grain boundary segregation which in turn is dependent on melt pool shape/size and mushy zone length indicated by accompanying simulations. Residual stress, measured by X-ray diffraction, decreased from 842 MPa (5 mm) to 690 MPa (1 mm), followed by an abnormal rise to 842 MPa (0.7 mm) and 875 MPa (0.5 mm). This residual stress behavior is likely associated with the cracks acting as a stress relief mechanism. However, the 0.2 mm stripe width exhibited the lowest stress of 647 MPa, suggesting a different mechanism for stress relief, possibly due to re-melting. These findings highlight the critical role of stripe width as a scan strategy in PBF-LB processing of crack-susceptible alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
2. Scanning strategy in selective laser melting (SLM): a review10.1007/s00170-021-06810-3 ↗
3. Laser powder bed fusion: a state-of-the-art review of the technology, materials, properties & defects, and numerical modelling10.1016/j.jmrt.2022.07.121 ↗
4. A comprehensive literature review on laser powder bed fusion of Inconel superalloys
5. Review of laser powder bed fusion of gamma-prime-strengthened nickel-based superalloys10.3390/met10080996 ↗
6. DuPont · 2009
7. Modelling of additive manufacturability of nickel-based superalloys for laser powder bed fusion10.1016/j.actamat.2022.118307 ↗
8. Processing a non-weldable nickel-base superalloy by Selective Laser Melting: role of the shape and size of the melt pools on solidification cracking10.1016/j.mtla.2020.100686 ↗
9. Atomic-scale grain boundary engineering to overcome hot-cracking in additively-manufactured superalloys10.1016/j.actamat.2019.07.041 ↗
10. On the role of boron, carbon and zirconium on hot cracking and creep resistance of an additively manufactured polycrystalline superalloy10.1016/j.mtla.2021.101193 ↗
11. On the role of Zr and B addition on solidification cracking of IN738LC produced by laser powder bed fusion10.1016/j.mtla.2022.101609 ↗
12. Crack inhibition to enhance strength-ductility of CM247LC alloy fabricated by laser powder bed fusion10.1016/j.msea.2023.145114 ↗
13. N.J. Balila, Influence of heat input on solidification cracking in additively manufactured CM247LC Ni-based Superalloy
14. Residual stress reduction of LPBF-processed CM247LC samples via multi laser beam strategies10.1007/s00170-021-07083-6 ↗
15. Cracking during thermal post-processing of laser powder bed fabricated CM247LC Ni-superalloy10.1016/j.matdes.2019.107793 ↗
16. Fine-tuning melt pools and microstructures: taming cracks in powder bed fusion – laser beam of a non-weldable Ni-base superalloy10.1016/j.mtla.2024.102059 ↗
17. Ghoussoub · 2020
18. A novel γ′-strengthened nickel-based superalloy for laser powder bed fusion10.3390/ma13214930 ↗
19. Scanning strategy induced cracking and anisotropic weakening in grain texture of additively manufactured superalloys
20. The effect of laser scanning strategies on the microstructure, texture and crystallography of grains exhibiting hot cracks in additively manufactured Hastelloy X10.1016/j.mechmat.2021.103816 ↗
21. Predictive process diagram for parameters selection in laser powder bed fusion to achieve high-density and low-cracking built parts
22. Investigating the influence of process parameters on the structural integrity of an additively manufactured nickel-based superalloy10.3390/met9111191 ↗
23. Effects of stripe width on the porosity and mechanical performance of additively manufactured Ti-6Al-4V parts
24. Högman · 2021
25. Cracking behavior of rené 104 nickel-based superalloy prepared by selective laser melting using different scanning strategies10.3390/ma13092149 ↗
26. The effect of processing parameters and material properties on residual forces induced in Laser Powder Bed Fusion (L-PBF)
27. A.B. Freemelt, 2024, Electron beam powder bed fusion processing of pure tungsten, (2024). 〈https://freemelt.com/knowledge/electron-beam-powder-bed-fusion-processing-of-pure-tungsten/?lang=sv〉(Accessed March 24, 2024).
28. L. ZeyuElectron beam powder bed fusion of Nitinol: A development from production process window towards delicate structures, KTH, Production engineering, 2023.
29. Laser powder bed fabrication of nickel-base superalloys: Influence of parameters; characterisation, quantification and mitigation of cracking10.7449/2012/Superalloys_2012_577_586 ↗
30. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
31. Texture analysis with MTEX–free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
32. Theory and application of electron channelling contrast imaging under controlled diffraction conditions10.1016/j.actamat.2014.04.018 ↗
33. Trainable Weka Segmentation: a machine learning tool for microscopy pixel classification10.1093/bioinformatics/btx180 ↗
34. Coupling of electron channeling with EBSD: Toward the quantitative characterization of deformation structures in the sem10.1007/s11837-013-0678-0 ↗
35. In situ site-specific specimen preparation for atom probe tomography10.1016/j.ultramic.2006.06.008 ↗
36. EDDIDAT: a graphical user interface for the analysis of energy-dispersive diffraction data10.1107/S1600576720005506 ↗
37. ISODEC: software for calculating diffraction elastic constants10.1107/S0021889812014252 ↗
38. Microstress evolution during in situ loading of a superalloy containing high volume fraction of γ′ phase10.1016/S1359-6462(02)00504-3 ↗
39. Thermo-Calc Software AB, Additive Manufacturing (AM) Module User Guide, 2024. 〈https://thermocalc.com/wp-content/uploads/Documentation/Getting_Started/additive-manufacturing-module-getting-started-guide.pdf〉.
40. Texture-based residual stress analysis of laser powder bed fused Inconel 718 parts10.1107/S1600576723004855 ↗
41. Misorientation-dependent solute enrichment at interfaces and its contribution to defect formation mechanisms during laser additive manufacturing of superalloys
42. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
43. Additive manufacturing of Ni-based superalloys: residual stress, mechanisms of crack formation and strategies for crack inhibition10.1016/j.nanoms.2022.08.001 ↗
44. T.W. ClyneThe Influence of Composition on Solidification Cracking Susceptibility in Binary Alloy Systems, (1981).
45. Solidification cracking susceptibility associated with a teardrop-shaped weld pool10.1080/13621718.2021.1910179 ↗
46. Weld metal solidification I: grain structure10.1002/0471434027.ch7 ↗
47. Additive manufacturing of metallic components – Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
48. Unique crystallographic texture formation in Inconel 718 by laser powder bed fusion and its effect on mechanical anisotropy10.1016/j.actamat.2021.116876 ↗
49. Kou · 2003
50. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting10.1016/j.actamat.2017.09.047 ↗
51. Reducing cracking sensitivity of CM247LC processed via laser powder bed fusion through composition modification10.1016/j.jmrt.2024.02.082 ↗
52. Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy10.1016/j.actamat.2017.02.007 ↗
53. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment10.1016/j.matchar.2016.02.004 ↗
54. Directionally solidified DS CM 247 LC—optimized mechanical properties resulting from extensive γ′ solutioning
55. Electron beam based additive manufacturing of alloy 247 for turbine engine application: from research towards industrialization10.1007/s11661-022-06955-0 ↗