Preparation of weak-textured commercially pure titanium by electron beam melting
Source abstract
Abstract
Abstract This paper presents the first report on the development of weak-textured microstructures and resulting reduced in-plane anisotropy of mechanical properties in commercially pure titanium (CP-Ti) fabricated by electron beam melting (EBM). The as-built specimens exhibited fine grain structures with weakened crystallographic textures. The β → α′ martensitic transformation after solidification was responsible for the weak textures as well as the relatively high strength. The results suggest that it is possible to use EBM to produce isotropic CP-Ti components, which cannot be obtained by conventional processes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Characterization of titanium aluminide alloy components fabricated by additive manufacturing using electron beam melting10.1016/j.actamat.2009.11.032 ↗
2. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
3. Build direction dependence of microstructure and high-temperature tensile property of Co–Cr–Mo alloy fabricated by electron beam melting10.1016/j.actamat.2013.10.017 ↗
4. Microstructures and properties of solid and reticulated mesh components of pure iron fabricated by electron beam melting10.1016/j.jmrt.2013.10.002 ↗
5. Comparison of microstructures and mechanical properties for solid and mesh cobalt-base alloy prototypes fabricated by electron beam melting10.1007/s11661-010-0388-y ↗
6. Open-cellular copper structures fabricated by additive manufacturing using electron beam melting10.1016/j.msea.2011.03.053 ↗
7. Cellular Ti-6Al-4V structures with interconnected macro porosity for bone implants fabricated by selective electron beam melting10.1016/j.actbio.2008.03.013 ↗
8. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
9. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
10. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
11. Stress-state dependence of slip in Ti-6Al-4V and other H.C.P. metals10.1016/0001-6160(81)90049-3 ↗
12. A study of active deformation systems in titanium alloys: dependence on alloy composition and correlation with deformation texture10.1016/S0921-5093(02)00421-5 ↗
13. Orientation informed nanoindentation of α-titanium: indentation pileup in hexagonal metals deforming by prismatic slip10.1557/jmr.2011.334 ↗
14. Orientation dependence of slip and twinning in HCP metals10.1016/S1359-6462(97)00048-1 ↗
15. Improvement of stretch formability of pure titanium sheet by differential speed rolling10.1016/j.scriptamat.2010.05.005 ↗
16. Texture evolution during grain growth in recrystallized commercially pure titanium10.1016/j.msea.2005.02.049 ↗
17. In situ observation of texture evolution during α→β and β→α phase transformations in titanium alloys investigated by neutron diffraction10.1016/j.actamat.2007.06.017 ↗
18. Effect of deformation twinning on microstructure and texture evolution during cold rolling of CP-titanium10.1016/j.msea.2005.03.019 ↗
19. The importance of crystallographic texture in the use of titanium as an orthopedic biomaterial10.1039/C4RA05440G ↗
20. Microstructure and mechanical properties of pure Ti processed by high-ratio differential speed rolling at room temperature10.1016/j.scriptamat.2009.12.008 ↗
21. Characterization of grade 2 commercially pure trabecular titanium structures10.1016/j.msec.2013.02.034 ↗
22. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
23. Estimation of dislocation density in cold-rolled commercially pure titanium by using synchrotron diffraction10.1007/s11663-014-0066-3 ↗
24. The effect of grain size on yield stress and work hardening of polycrystalline titanium at 295K and 575K10.1016/0025-5416(78)90171-4 ↗
25. Strain hardening regimes and microstructure evolution during large strain compression of high purity titanium10.1016/S1359-6462(02)00005-2 ↗
26. Effect of oxygen and hydrogen on mechanical properties of commercial purity titanium10.1179/imr.1996.41.1.1 ↗
27. Effect of interstitial solutes on the strength and ductility of titanium10.1016/0079-6425(81)90001-3 ↗
28. Texture control during laser deposition of nickel-based superalloy10.1016/j.scriptamat.2012.06.014 ↗
29. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
30. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti–6Al–4V, Metall10.1007/s11661-010-0397-x ↗
31. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti-6Al-4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
32. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
33. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
34. Continuous cooling β-to-α transformation behaviors of extra-pure and commercially pure Ti10.1007/s11661-004-0052-5 ↗
35. Approximation of absolute surface temperature measurements of powder bed fusion additive manufacturing technology using in situ infrared thermography
36. Lütjering · 2007