journal article·2019-10

An investigation into specimen property to part performance relationships for laser beam powder bed fusion additive manufacturing

Rakish Shrestha, Nima Shamsaei, Mohsen Seifi, Nam Phan

Publisher page

Abstract

Abstract The influence of part size and geometry on the melt pool size, microstructural features, and resulting mechanical properties of additive manufactured 17-4 precipitation hardening (PH) stainless steel (SS), fabricated using a laser beam powder bed fusion (LB-PBF) process is investigated. Three different types of geometries including a dog-bone part (i.e. representing the specimen or the witness coupon) and two square rods with different cross-sectional sizes (i.e. representing the parts) were designed and fabricated using the same set of process parameters. Mechanical properties were determined under quasi-static tensile and uniaxial strain-controlled fully-reversed fatigue loading conditions. Experimental results confirmed a minimal effect of part geometry on the tensile behavior of the LB-PBF 17-4 PH SS as the yield strength ranged from 1145 to 1198 MPa and ultimate tensile strength varied from 1171 to 1231 MPa. On the other hand, part geometry had a significant impact on the fatigue behavior in the high cycle regime. Specimens fabricated from the large square blocks contained the lowest amount of porosity, and consequently, exhibited the highest fatigue resistance. On the contrary, the highest amount of porosity was observed in the specimens fabricated from the dog-bone parts resulting in an inferior fatigue resistance as compared to other geometries. Microstructural analysis was performed to estimate the effect of part geometry on the thermal history experienced during manufacturing by measuring the melt pool dimensions. Some effects of geometry on the melt pool dimensions were observed as the melt pool depth was found to be shorter for dog-bone specimens and longer for large block specimens. The less elongated melt pools in dog-bone specimens can be attributed to higher cooling rate experienced by the specimens resulting in more entrapped gas pores.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. LCF behaviour and a comprehensive life prediction model for AlSi10Mg obtained by SLM10.1016/j.ijfatigue.2018.07.030 ↗
2. Fatigue assessment of Ti–6Al–4V circular notched specimens produced by selective laser melting10.3390/met7080291 ↗
3. An introduction to the fatigue and fracture behavior of additive manufactured parts10.1016/j.ijfatigue.2016.07.007 ↗
4. Fatigue behavior and failure mechanisms of direct laser deposited Ti–6Al–4V10.1016/j.msea.2015.12.026 ↗
5. Fatigue design with additive manufactured metals: issues to consider and perspective for future research10.1016/j.proeng.2018.02.002 ↗
6. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
7. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
8. Progress towards metal additive manufacturing standardization to support qualification and certification10.1007/s11837-017-2265-2 ↗
9. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
10. Defect distribution and microstructure heterogeneity effects on fracture resistance and fatigue behavior of EBM Ti–6Al–4V10.1016/j.ijfatigue.2016.06.001 ↗
11. Synchrotron-Based X-ray Microtomography Characterization of the Effect of Processing Variables on Porosity Formation in Laser Power-Bed Additive Manufacturing of Ti-6Al-4V10.1007/s11837-016-2234-1 ↗
12. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
13. Relating porosity to fatigue failure in additively manufactured alloy 71810.1016/j.msea.2018.04.075 ↗
14. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
15. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
16. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
17. Fatigue behavior of additive manufactured 316L stainless steel parts: effects of layer orientation and surface roughness
18. Fatigue behavior and modeling of additively manufactured Ti-6Al-4V including interlayer time interval effects10.1007/s11837-017-2625-y ↗
19. Effect of building direction on porosity and fatigue life of selective laser melted AlSi12Mg alloy10.1016/j.msea.2018.05.040 ↗
20. Fatigue behaviour of additive manufactured materials: an overview of some recent experimental studies on Ti-6Al-4V considering various processing and loading direction effects10.1111/ffe.13000 ↗
21. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
22. Mechanical properties and microstructural characterization of selective laser melted 17-4 PH stainless steel10.1108/RPJ-12-2015-0192 ↗
23. Porosity formation mechanisms and fatigue response in Al-Si-Mg alloys made by selective laser melting10.1016/j.msea.2017.11.078 ↗
24. Selection of steels suitable for additive layer manufacturing10.1179/0301923314Z.000000000269 ↗
25. Schade · 2010
26. Microstructure and mechanical properties of laser forming repaired 17-4PH stainless steel10.1016/j.msea.2012.05.095 ↗
27. ASTM E606-04 · 2004
28. Fatigue behavior of additively manufactured 17-4 PH stainless steel: synergistic effects of surface roughness and heat treatment10.1016/j.ijfatigue.2019.02.039 ↗
29. ASTM E8/8M-16a · 2016
30. ASTM E3-11 · 2017
31. Laser powder bed fusion of Ti-6Al-4V parts: thermal modeling and mechanical implications10.1016/j.ijmachtools.2017.04.007 ↗
32. Simultaneously enhanced strength and ductility for 3D-printed stainless steel 316L by selective laser melting10.1038/s41427-018-0018-5 ↗
33. Effects of design parameters on thermal history and mechanical behavior of additively manufactured 17-4 PH stainless steel
34. ASTM A693-16 · 2016
35. Fatigue performance of additive manufactured metallic parts10.1108/13552541311302932 ↗
36. An overview of Direct Laser Deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control
37. Transformation-induced plasticity and high strength in beta titanium alloy manufactured by selective laser melting10.1016/j.mtla.2019.100299 ↗
38. Stephens · 2000
39. In-process sensing in selective laser melting (SLM) additive manufacturing10.1186/s40192-016-0045-4 ↗
40. 2017
41. Common defects and contributing parameters in powder bed fusion AM process and their classification for online monitoring and control: a review10.1007/s00170-017-1172-6 ↗
42. Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting10.1016/j.actamat.2016.04.029 ↗