journal article·2019-10Open access

Shape retention and infiltration height in complex WC-Co parts made via binder jet of WC with subsequent Co melt infiltration

Corson L. Cramer, Natalie R. Wieber, Trevor G. Aguirre, Richard A. Lowden, Amy M. Elliott

Abstract

Abstract Additive manufacturing (AM) of complex tungsten carbide-cobalt (WC-Co) parts was achieved using binder jet additive manufacturing (BJAM) of WC powders followed by Co infiltration. The intent of the study is to explore the shape retention, infiltration height, and properties of parts made with this method. Using BJAM with infiltration of the metal phase can limit shrinkage and grain growth in ceramic-metal (cermet) composites compared to other additive manufacturing (AM) methods. Knowledge of previous infiltration studies was used to help process parts to imitate production of parts. The properties such as density, microstructure, grain size, and hardness of the parts are characterized along the infiltration height. Fracture toughness is measured where applicable. This approach has the potential to achieve highly dense WC-Co parts that are net-shaped with some ternary phase and z-direction distortion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Impact resistance of TiC-based cermets10.1016/j.ijimpeng.2013.06.008 ↗
2. Role of binder phase in cemented tungsten carbide-cobalt alloys
3. WC-Co enjoys proud history and bright future10.1016/S0026-0657(98)85097-2 ↗
5. Preparation and sintering of WC–Co composite powders for coarse grained WC–8Co hardmetals10.1016/j.ijrmhm.2014.04.004 ↗
6. Powder injection molding of WC–8%Co tungsten cemented carbide10.1016/S0263-4368(02)00015-X ↗
7. Scheithauer · 2019
8. Three-dimensional printing of tungsten carbide–10wt% cobalt using a cobalt oxide precursor10.1016/j.ijrmhm.2006.02.002 ↗
9. Obtaining crack-free WC-Co alloys by selective laser melting10.1016/j.phpro.2016.08.091 ↗
10. Direct selective laser sintering of hard metal powders: experimental study and simulation10.1007/s001700200024 ↗
11. Direct selective laser sintering of WC-Co cemented carbide by premixing of additives
12. Synthesis of nanostructured WC-Co hardmetal by selective laser melting10.1016/j.piutam.2017.06.011 ↗
13. Sintering of WC-12%Co processed by binder jet 3D printing (BJ3DP) technology10.1016/j.ijrmhm.2017.10.023 ↗
14. Wear properties of sintered WC-12%Co processed via Binder Jet 3D Printing (BJ3DP10.1016/j.ijrmhm.2018.10.003 ↗
15. Cramer · 2019
16. Structure and mechanical behavior of Big Area Additive Manufacturing (BAAM) materials10.1108/RPJ-12-2015-0183 ↗
17. Large-scale production of magnetic nanoparticles using bacterial fermentation10.1007/s10295-010-0749-y ↗
18. Tool wear simulation of complex shaped coated cutting tools10.1016/j.wear.2015.01.015 ↗
19. Grain size measurement by the intercept method10.1016/0026-0800(71)90005-X ↗
20. Influence of temperature, grain size and cobalt content on the hardness of WC–Co alloys10.1016/S0263-4368(98)00038-9 ↗
21. Effects of Co content and WC grain size on wear of WC cemented carbide10.1016/j.wear.2005.09.034 ↗
22. Microstructure, hardness and toughness of nanostructured and conventional WC-Co composites10.1016/S0965-9773(98)00123-8 ↗
23. Fracture toughness of two phase WC-Co cermets,” Acta Metall
24. Fracture toughness and fracture of WC-Co composites10.1007/BF00708272 ↗
25. Thermodynamic properties of the Co-W-C system10.1007/BF02651660 ↗