Selective laser melting of CP-Ti to overcome the low cost and high performance trade-off
Source abstract
Abstract
Abstract In this study, commercially pure titanium (CP-Ti) parts were successfully fabricated by selective laser melting (SLM) using cost-effective hydride-dehydride (HDH) Ti powders for the first time modified by jet milling. Jet milling effectively improves the particle-shape sphericity, suppresses the impurity pick-up, and produces localized plastic deformation. The flowability of the jet-milled powders is tremendously improved to 29.7 s/50 g that satisfies the SLM processing well, while the oxygen content only increases by 0.02 wt.% (the raw oxygen level: 0.15 wt.%). The oxide layer in the powder surface is determined with the thickness of ∼8 nm and TiO being the predominant phase before and after jet milling. The SLM-made (SLMed) CP-Ti achieves dominant martensitic α’ phase with the fracture tensile strength up to 731.5 ± 5.7 MPa and elongation of 20.5 ± 1.1%, comparable with those using expensive atomized powders. Contrary to the conventional metallurgical mechanism for Ti which suffers the cost-performance dilemma, this work presents SLMed CP-Ti with excellent synergy of strength and ductility while using the cost-affordable HDH Ti powders.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Leyens · 2020
2. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
3. Lütjering · 2007
4. 24 - the additive manufacturing (AM) of titanium alloys
5. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
6. Peritectic titanium alloys for 3D printing10.1038/s41467-018-05819-9 ↗
7. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
8. Microstructural evolution of fusion zone in laser beam welds of pure titanium10.1016/j.matchar.2011.12.010 ↗
9. Microstructure evolution and density behavior of CP Ti parts elaborated by self-developed vacuum selective laser melting system10.1016/j.apsusc.2013.04.090 ↗
10. Simultaneous achievement of equiaxed grain structure and weak texture in pure titanium via selective laser melting and subsequent heat treatment10.1016/j.jallcom.2019.06.305 ↗
11. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
12. Thermal behavior during selective laser melting of commercially pure titanium powder: numerical simulation and experimental study
13. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
14. Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting10.1016/j.matchar.2018.03.003 ↗
15. Comparison of wear properties of commercially pure titanium prepared by selective laser melting and casting processes10.1016/j.matlet.2014.11.156 ↗
16. Comparative study of commercially pure titanium produced by laser engineered net shaping, selective laser melting and casting processes10.1016/j.msea.2017.08.103 ↗
17. Microstructure and mechanical properties investigation of CP titanium processed by selective laser melting (SLM)10.1016/j.jmatprotec.2016.10.022 ↗
18. 2 - conventional titanium powder production
19. A comparative study of Ti-6Al-4V powders for additive manufacturing by gas atomization, plasma rotating electrode process and plasma atomization10.1016/j.powtec.2018.04.013 ↗
20. Review of the methods for production of spherical Ti and Ti alloy powder10.1007/s11837-017-2513-5 ↗
21. 31 - a perspective on the future of titanium powder metallurgy
22. Ultra-low cost Ti powder for selective laser melting additive manufacturing and superior mechanical properties associated10.29026/oea.2019.180028 ↗
23. Fabrication of commercial pure Ti by selective laser melting using hydride-dehydride titanium powders treated by ball milling10.1016/j.jmst.2018.09.058 ↗
24. A novel method for production of spherical Ti-6Al-4V powder for additive manufacturing10.1016/j.powtec.2016.06.022 ↗
25. Microstructure and mechanical properties of Ti-6Al-4V fabricated by selective laser melting of powder produced by granulation-sintering-deoxygenation method10.1007/s11837-017-2584-3 ↗
26. On the texture, phase and tensile properties of commercially pure Ti produced via selective laser melting assisted by static magnetic field10.1016/j.msec.2016.09.011 ↗
27. Evaluation of the mechanical and wear properties of titanium produced by three different additive manufacturing methods for biomedical application10.1016/j.msea.2019.06.024 ↗
28. Porous structure uniformity investigation of tungsten matrix prepared by jet milled and annealed tungsten powder10.1016/j.powtec.2018.08.021 ↗
29. Microstructure and texture formation in commercially pure titanium prepared by cryogenic milling and spark plasma sintering10.1016/j.matchar.2019.02.035 ↗
30. Low-cost Ti powders for additive manufacturing treated by fluidized bed10.1016/j.powtec.2019.03.042 ↗
31. Fundamental understanding of the dissolution of oxide film on Ti powder and the unique scavenging feature by LaB610.1007/s11661-017-4366-5 ↗
32. Surface characterization of titanium hydride powder10.1016/j.vacuum.2011.07.054 ↗
33. Microstructure of adiabatic shear bands in Ti6Al4V10.1016/j.matchar.2012.10.009 ↗
34. Dynamic deformation and failure of ultrafine-grained titanium10.1016/j.actamat.2016.11.041 ↗
35. Chapter 4 - oxidation and oxides
36. Surface chemical state of Ti powders and its alloys: effect of storage conditions and alloy composition10.1016/j.apsusc.2016.01.046 ↗
37. Interstitial elements in titanium powder metallurgy: sources and control10.1179/174329011X13045076771759 ↗
38. Oxidation of commercial purity titanium10.1007/BF00659186 ↗
39. Thermal oxidation behaviour of bulk titanium with nanocrystalline surface layer10.1016/j.corsci.2012.03.005 ↗
40. Growth of titanium oxide overlayers by thermal oxidation of titanium10.1007/BF01115696 ↗
41. XPS study of the deoxidization behavior of hydrogen in TiH2 powders10.1016/j.powtec.2016.09.005 ↗
42. The hydrogen sorption and desorption behavior in spherical powder of pure titanium used for additive manufacturing10.1016/j.ijhydene.2017.04.248 ↗
43. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: a study from laser power perspective10.1016/j.matdes.2016.12.019 ↗
44. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
45. Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
46. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
47. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
48. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
49. Development and mechanical characterization of porous titanium bone substitutes10.1016/j.jmbbm.2012.01.008 ↗
50. Additive manufacturing of a novel alpha titanium alloy from commercially pure titanium with minor addition of Mo2C10.1016/j.mtla.2018.09.033 ↗
51. Microstructure and mechanical properties of Ti–Re alloys manufactured by selective laser melting10.1016/j.msea.2019.138290 ↗
52. Davis · 1989
53. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
54. Evolution of microstructure and shear-band formation in α-hcp titanium10.1016/0167-6636(94)90058-2 ↗
55. Farayibi · 2014
56. Numerical and experimental analysis of the effect of volumetric energy absorption in powder layer on thermal-fluidic transport in selective laser melting of Ti6Al4V10.1016/j.optlastec.2018.09.054 ↗
57. Numerical simulation in the absorption behavior of Ti6Al4V powder materials to laser energy during SLM10.1016/j.jmatprotec.2019.01.002 ↗
58. Continuous cooling β-to-α transformation behaviors of extra-pure and commercially pure Ti10.1007/s11661-004-0052-5 ↗
59. Abnormal grain growth in commercially pure titanium during additive manufacturing with electron beam melting10.1016/j.mtla.2019.100281 ↗
60. Kurz · 1989
61. Six decades of the Hall–petch effect – a survey of grain-size strengthening studies on pure metals10.1080/09506608.2016.1191808 ↗
62. Micromechanical behavior and thermal stability of a dual-phase α+α’ titanium alloy produced by additive manufacturing10.1016/j.actamat.2018.09.050 ↗