Highly conductive and strong CuSn0.3 alloy processed via laser powder bed fusion starting from a tin-coated copper powder

Suraj Dinkar Jadhav, Dongmei Fu, Maxim Deprez, Kristof Ramharter, Denise Willems, Brecht Van Hooreweder, Kim Vanmeensel

Abstract

Abstract Despite the high demand, the successful fabrication of fully dense, highly conductive, and strong copper components via laser powder bed fusion (LPBF) is not readily evident. This is mainly due to the low optical absorption of copper, which inhibits the complete melting of copper powders when using commercially available fiber-laser-based LPBF machines. Accordingly, this article proposes a novel approach of using optically absorptive metal-coated copper powders for the fabrication of fully dense, highly conductive, and strong copper components via LPBF. To validate this approach, the surface of the copper powder is modified by applying a very thin (62 ± 14 nm) layer of metallic tin via an immersion plating technique. The application of only a 0.28 wt% of metallic tin coating significantly improved the room temperature powder optical absorption by ∼170 % at the fiber laser wavelength. Consequently, crack-free and fully dense copper parts combining high thermal conductivity of 334 ± 4 (W/(m·K)) and electrical conductivity of 80 ± 1 % international annealed copper standard (%IACS) with a good tensile strength of 256 ± 14 MPa, yield strength of 203 ± 4 MPa, and ductility of 21 ± 2 % have been fabricated using a fiber laser with an output laser power of 500 W. Furthermore, the article also describes the negative influence of the presence of a high amount of (0.091 wt%) sulfur, which originates from the organic additives during sub-optimal coating conditions, on the LPBF processing behavior of CuSn alloys. As such, high sulfur-containing tin-coated copper powders do not allow the fabrication of fully dense parts due to the occurrence of solidification cracks and the formation of pores. Subsequently, the optimum tin coating methodology, which limits the amount of sulfur below 0.0025 wt%, is described. The use of sulfur-free powder is recommended for the successful LPBF processing of fully dense parts made of copper and copper alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Davis · 2001
2. Laser 3D printing of complex copper structures
3. Additive manufacturing of shaped profile windings for minimal AC loss in electrical machines10.1109/TIA.2020.2975763 ↗
4. Copper: alloying
5. Modification of electrical and mechanical properties of selective laser‐melted CuCr0.3 alloy using carbon nanoparticles10.1002/adem.201900946 ↗
6. The utilization of selective laser melting technology on heat transfer devices for thermal energy conversion applications: a review10.1016/j.rser.2018.03.109 ↗
7. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
8. Design of 3D printed high performance windings for switched reluctance machines
9. 3D printing of highly pure copper10.3390/met9070756 ↗
10. Selective laser melting of copper10.4028/www.scientific.net/MSF.843.284 ↗
11. Selective laser melting of chemical pure copper powders
12. Electrical resistivity of pure copper processed by medium-powered laser powder bed fusion additive manufacturing for use in electromagnetic applications
13. Study on selective laser melting of copper
14. Hönl · 2018 · 1
15. Lang · 2017 · 1
16. Laser metal deposition of copper on diverse metals using green laser sources10.1007/s00170-020-05117-z ↗
17. Laser welding of copper using a high power disc laser at green wavelength10.1016/j.procir.2018.08.161 ↗
18. Laser metal deposition of pure copper on stainless steel with blue and IR diode lasers10.1016/j.optlastec.2018.06.012 ↗
19. In situ quality control of the selective laser melting process using a high-speed, real-time melt pool monitoring system10.1007/s00170-014-6214-8 ↗
20. Multiscale modeling of powder bed–based additive manufacturing10.1146/annurev-matsci-070115-032158 ↗
21. Influence of selective laser melting process parameters on texture evolution in pure copper10.1016/j.jmatprotec.2019.02.022 ↗
22. Selective laser melting of pure copper10.1007/s11837-017-2695-x ↗
23. Limits and solutions in processing pure Cu via selective laser melting using a high-power single-mode fiber laser10.1007/s00170-019-04015-3 ↗
24. Influence of powder particle size distribution on the printability of pure copper for selective laser melting
25. Additive manufacturing of copper alloys: influence of process parameters and alloying elements10.1080/02670836.2019.1600840 ↗
26. Microstructure and properties in QCr0.8 alloy produced by selective laser melting with different heat treatment10.1016/j.jallcom.2019.06.018 ↗
27. Microstructure and properties of high strength and high conductivity Cu-Cr alloy components fabricated by high power selective laser melting10.1016/j.matlet.2018.11.118 ↗
28. Effect of heat treatments on microstructure and properties of CuCrZr produced by laser-powder bed fusion10.1016/j.msea.2018.12.017 ↗
29. SLM process parameters development of Cu-alloy Cu7.2Ni1.8Si1Cr10.1108/RPJ-06-2017-0116 ↗
30. Selective Laser Melting of Cu 10Zn alloy powder using high laser power10.1016/j.powtec.2018.10.002 ↗
31. Mechanical and electrical properties of selective laser‐melted parts produced from surface‐oxidized copper powder
32. Surface modified copper alloy powder for reliable laser-based additive manufacturing
33. RF losses in selective laser melted GRCop-84 copper waveguide for an additively manufactured lower hybrid current drive launcher10.1016/j.fusengdes.2020.111762 ↗
34. Surface roughness and finishing techniques in selective laser melted GRCop-84 copper for an additive manufactured lower hybrid current drive launcher10.1016/j.fusengdes.2020.111801 ↗
35. Mechanical properties and microstructural characterization of Cu-4.3 pct Sn fabricated by selective laser melting10.1007/s11661-016-3779-x ↗
36. Manufacturing feasibility and forming properties of Cu-4Sn in selective laser melting10.3390/ma10040333 ↗
37. Additive manufacturing of Cu–10Sn bronze10.1016/j.matlet.2015.05.076 ↗
38. Processing optimisation, mechanical properties and microstructural evolution during selective laser melting of Cu-15Sn high-tin bronze10.1016/j.msea.2018.02.051 ↗
39. Vanmeensel, influence of carbon nanoparticle addition (and impurities) on selective laser melting of pure copper10.3390/ma12152469 ↗
40. Electroless tinning of copper powders10.1007/BF00792073 ↗
41. Buls · 2018
42. Thermal and electrical conductivity of 99.9% pure copper processed via selective electron beam melting10.1002/adem.201600078 ↗
43. Effect of applied interparticle force on the static and dynamic angles of repose of spherical granular material10.1103/PhysRevE.63.031302 ↗
44. Surface energy and wetting in island films
45. Grain boundary effect in surface tension measurement10.1007/BF03398958 ↗
46. Optical and electrical properties of tin
47. Lide · 2005
48. Bergström · 2008
49. Selective laser melting of typical metallic materials: an effective process prediction model developed by energy absorption and consumption analysis
50. Effects of sulfur concentration and Marangoni convection on melt-pool formation in transition mode of selective laser melting process10.1016/j.matdes.2019.107866 ↗
51. Powder bed fusion processes: an overview
52. Mechanism for minor element effect on gta fusion zone geometry
53. Effect of dissolved sulphur on the surface tension of liquid copper10.1007/BF03397527 ↗
54. Surface-active element transport and its effect on liquid metal flow in laser-assisted additive manufacturing10.1016/j.icheatmasstransfer.2017.06.007 ↗
55. In situ absorptivity measurements of metallic powders during laser powder-bed fusion additive manufacturing10.1016/j.apmt.2017.08.006 ↗
56. Energy coupling mechanisms and scaling behavior associated with laser powder bed fusion additive manufacturing10.1002/adem.201900185 ↗
57. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging10.1126/science.aav4687 ↗
58. Perry · 2011
59. Formation mechanism of 2D SnS 2 and SnS by chemical vapor deposition using SnCl 4 and H2S10.1039/C8TC01821A ↗